Download PDF Techmer ES HiFill® PP GF/M50 CC BK 50% Glass/Mineral Filled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 50% Filler by WeightFeatures: Chemically CoupledAppearance: BlackInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
ASTM D792
Water Absorption 0.060 %

@Time 86400 sec
0.060 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0030 cm/cm

@Thickness 3.17 mm
0.0030 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 95
95
ASTM D785
Tensile Strength, Yield 72.4 MPa
10500 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Yield Strength 96.5 MPa
14000 psi
ASTM D790
Flexural Modulus 5.52 GPa
800 ksi
ASTM D790
Izod Impact, Notched 0.694 J/cm

@Thickness 3.17 mm
1.30 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 7.47 J/cm

@Thickness 3.17 mm
14.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 21.6 µm/m-°C
12.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 152 °C
305 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 143 °C
290 °F
Unannealed; ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+16 ohm-cm
2.00e+16 ohm-cm
ASTM D257
Dielectric Strength 20.1 kV/mm
510 kV/in
Method A (Short-Time); ASTM D149