Asahi Kasei Thermylene® F6-30FG-0100 30% Glass Fiber Reinforced, Chemically Coupled

Category Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Asahi Kasei
Trade Name Thermylene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Kasei Thermylene® F6-30FG-0100 30% Glass Fiber Reinforced, Chemically Coupled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Asahi Thermofil
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
ASTM D792
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Melt Flow 3.5 g/10 min
3.5 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 80
80
ASTM D785
Tensile Strength, Yield 72.4 MPa
10500 psi
ASTM D638
Elongation at Yield 4.0 %
4.0 %
ASTM D638
Flexural Strength 86.2 MPa
12500 psi
ASTM D790
Flexural Modulus 3.86 GPa
560 ksi
ASTM D790
Izod Impact, Notched 1.49 J/cm
2.80 ft-lb/in
ASTM D256
Izod Impact, Unnotched 7.47 J/cm
14.0 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
CTE, linear 46.8 µm/m-°C

@Temperature 20.0 °C
26.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 122 °C
251 °F
ASTM D648