Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 13.0 MPa | 1890 psi | ASTM D412 |
Precision Polymer Engineering Perlast® G60H Perfluoroelastomer Special, pure white compound with excellent high temperature properties and wide chemical resistance. Extremely low outgassing properties.Applications: For use in applications which require exposur.. |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | ASTM D412 |
Precision Polymer Engineering V71C Fluoroelastomer Compound Fluoroelastomer Rubber, 66-75 °IRHD. Terpolymer of vinylidene difluoride and hexafluoropropylene tetrafluoroethylene. Compounded to have extremely low temperature capability, Glass transition tem.. |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | 20 in/min, injection molded, type 1 specimen; ASTM D638 |
Phillips Sumika Marlex® CHP-035 Thermoplastic Polyolefin
(discontinued **) Applications: Painted air-bag coversSoft interior trimSoft touch overmoldingInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | ASTM D638 |
NOVA Chemicals Novapol® PI-3526-A LLDPE Masterbatch Resin
(discontinued **) Molded Plaque Properties. Features: high flow.Applications: general purpose, housewares.Data provided by the manufacturer. |
|||
Tensile Strength, Yield | 13.0 - 90.0 MPa | 1890 - 13100 psi | Average value: 66.5 MPa Grade Count:109 |
Overview of materials for Acetal Homopolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values .. |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | ASTM D638 |
Ineos ABS Lustran® 456 Extrusion, Matte-Gloss
(discontinued **) Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with |
|||
Tensile Strength, Yield | 13.0 - 31.0 MPa | 1890 - 4500 psi | Average value: 22.3 MPa Grade Count:52 |
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be.. |
|||
Tensile Strength, Yield | 13.0 - 79.0 MPa @Temperature -40.0 - 80.0 °C |
1890 - 11500 psi @Temperature -40.0 - 176 °F |
Average value: 45.9 MPa Grade Count:5 |
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m.. |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | |
LyondellBasell Lupolen® 3010 K LDPE, Injection Molding Grade Injection moldingsData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | |
LyondellBasell Lupolen® 3024 H LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | |
LyondellBasell Lupolen® 3026 F LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | Dry |
Kraton® NEXAR™ MD9150 Polymer Barrier Membrane NEXAR™ sulfonated block copolymer membranes are designed for water transport, filtration and separation. They have a high moisture vapor transportation rate, allowing usage in humidification a.. |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | ISO 527-1, -2 |
LyondellBasell Hifaxâ„¢ CB272 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CB272 high melt flow, 900 MPa flexural modulus, low CLTE, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good balance of rigidity and dime.. |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | ASTM D 638 |
SABIC Innovative Plastics LNP Lubricomp YP003 TPEE LNP LUBRICOMP* YP003 is a compound based on TPEE resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Americas .. |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | BP 13B/1 |
SIDPEC EGYPTENE® LL 0550 AA LLDPE Injection Molding Applications:House waresVery thin-walled food containersLidsInformation provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (SIDPEC) Products |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | ISO 527 |
SABIC Innovative Plastics LNP Thermocomp MH0500A PP (Asia Pacific) LNP THERMOCOMP* MH0500A is a compound based on Polypropylene resin. Added features of this material include: High Specific Gravity.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP TH0300A PUR LNP THERMOCOMP* TH0300A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP 9H1100C LNP* Thermocomp* 9H1100C is a High Specific Gravity compound containing proprietary fillers. |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | ASTM D412 |
Teknor Apex APEX® 94-A0098A-70 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-General Purpose Uses-General PurposeAppearance-Natural Color, OpaqueForms-PelletsProcessing Method-I.. |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | 9.8 in/min; ASTM D638 |
Teknor Apex Sinvicomp SIM 5039 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: High Strength Uses: Electrical/Electronic Applications < Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | |
Trelleborg B747 Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | |
Trelleborg R570 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | ASTM D638 |
Trelleborg Horda Cable E8400 Easy Strippable Semiconductive Shielding E8400 is a vulcanizable, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8400 meets the requirements as be.. |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | ASTM D638 |
Eastman Eastman AP007 Copolyester Applications:Automotive componentsBreathable filmsElectronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsOffice furniturePackagingPolymer modificationProfilesRubber an.. |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | ASTM D638 |
Eastman Neostar FN007 Elastomer Neostar FN007 elastomer is the third in Eastman’s series of tough, clear, durable copolyester ethers. Though originally designed for use in the profile and automotive markets, this innovative copol.. |
|||
Tensile Strength, Yield | 13.0 MPa @Strain 300 % |
1890 psi @Strain 300 % |
ASTM D412 |
Dow Buna® SB 1723 Cold polymerized Emulsion Styrene Butadiene Rubber (E-SBR) Buna® SB 1723 - Schkopau is manufactured by cold polymerization using mixed rosin acid / fatty acid soaps. It is plasticized with 37.5 parts of a TDAE oil in relation to solid rubber. A discolori.. |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0437C40L Calcium Reinforced |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | ISO 527 |
Azoty Tarnow™ TARFLEN SM-G20 PTFE Reinforced with 20% graphite for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | ISO 527 |
A.D. Compound Adene NCZAG Copolymer 70% CaCO3 Filled Polypropylene Information provided by A.D. Compound |
|||
Tensile Strength, Yield | 13.0 - 70.0 MPa | 1890 - 10200 psi | Average value: 24.7 MPa Grade Count:45 |
Overview of materials for Polypropylene with 30% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini.. |