Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 6.00 kJ/m² @Temperature -40.0 °C |
2.86 ft-lb/in² @Temperature -40.0 °F |
ISO 180 |
Solvay Engineered Polymers SEQUEL® 2325 Engineered Polyolefin
(discontinued **) Description: SEQUEL® 2325 engineered polyolefin is designed for mold-in-color automotive interior applications. This material exhibits excellent low-gloss surface appearance and processability. Ap.. |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer (Europe-Africa-Middle East) Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior .. |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² @Temperature 23.0 °C |
2.86 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® E53 NC010 Nylon 66
(Unverified Data**) Zytel® E53 NC010 is a very high viscosity polyamide 66 resin for extrusion.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP GL003 PSU LNP* Lubricomp* GL003 is a compound based on Polysulfone resin containing 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics ULTEM 1000RV PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRILOY D20001 PC (Asia Pacific) LNP LUBRILOY* D20001 is a compound based on Polycarbonate resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Flame Retardant. |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRILOY K2000 Acetal (Asia Pacific) LNP LUBRILOY* K2000 is a compound based on Acetal resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP STAT-KON AE004 ABS LNP STAT-KON* AE004 is a compound based on ABS resin containing 20% Carbon Fiber. Added feature of this material is: Electrically Conductive. |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics ULTEM HU1000 PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | Notch A; ISO 180 |
Solvay Specialty Polymers Ryton® R-7-121BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-121NA and R-7-121BL glass fiber and mineral filled polyphenylene sulfide compounds provide good mechanical strength with good flow and low maintenance molding using conventional moldin.. |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Valox® ENH4560 PBT (Asia Pacific) Valox* ENH4560 resin is a non-brominated/non-chlorinated flame retardant product based on Valox* iQ PBT resin. |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP DC006H PC (Asia Pacific) LNP* Thermocomp* DC006H is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP EC006E PEI LNP THERMOCOMP* EC006E is a compound based on Polyetherimide resin containing 30% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP GF004 PSU LNP* Thermocomp* GF004 is a compound based on Polysulfone resin containing 20% Glass Fiber. |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP JF006LXZ PES LNP* THERMOCOMP* JF006LXZ is a compound based on Polyethersulfone resin containing 30% Glass Fiber. Added features of this material include: Low Extractible. |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP LF004E PEEK (Europe-Africa-Middle East) LNP* THERMOCOMP* LF004E is a compound based on Polyetheretherketone resin containing Glass Fiber. Added features include: Easy Molding. |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP STAT-KON EX07311P PEI (Asia Pacific) LNP Stat-kon* EX07311P is an easy flowing ESD-safe compound based on Polyetherimide resin. This compound is developed for good dimensional stability for use in ESD Tray for Backend Semicon and HDD t.. |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP RF006EUC PA 66 LNP* THERMOCOMP* RF006EUC is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include Easy Molding, UV Stabilized. |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | ASTM D256 |
Tipco Tipcofil® AG 200 - 10% Glass Fiber Reinforced Nylon-6 Compound, with High Heat Stability 10% Glass Reinforced Nylon-6 CompoundApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | ISO 180 |
Tisan TISLAMID® 6 30% Mineral Reinforced Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² @Temperature -20.0 °C |
2.86 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Total PPC 2660 Polypropylene, Heterophasic Copolymer ATOFINA Polypropylene PPC 2660 is a heterophasic copolymer. PPC 2660 is characterized by a low fluidity hence good melt strength to provide ease of processing and good manufactured article properti.. |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | ISO 180-A |
Ecomass® 4301TU74 Tungsten Filled Polyphthalamide Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsTungsten Powder Filled Polyphthalamide (PPA)Very Good ToughnessInformation provided by Technical Polymers |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² @Thickness 3.20 mm |
2.86 ft-lb/in² @Thickness 0.126 in |
ISO 180-A |
Ecomass® 705BI79 BaSO4 Filled ABS Nontoxic alternative to traditional materials, radiation shielding applications.Moderate Specific GravityBaSO4 Powder Filled ABSInformation provided by Technical Polymers |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | 50%RH; ISO 180/1A |
DuPont Performance Polymers Zytel® 158L NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
ISO 180/A |
BASF Ultrason S 2010 PSU Ultrason S 2010 is an unreinforced, medium viscosity standard injection molding PSU grade. It flows readily and offers outstanding heat resistance and dimensional stability. It conforms to FDA req.. |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | ISO 180/1A |
Addiplast Addilene H 210 Polypropylene Homopolymer UnreinforcedInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 6.00 - 6.50 kJ/m² | 2.86 - 3.09 ft-lb/in² | Average value: 6.33 kJ/m² Grade Count:3 |
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Izod Impact, Notched (ISO) | 6.00 - 13.0 kJ/m² @Thickness 4.00 - 4.00 mm |
2.86 - 6.19 ft-lb/in² @Thickness 0.157 - 0.157 in |
Average value: 8.77 kJ/m² Grade Count:3 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma.. |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® X5630 PC+PET (Europe-Africa-Middle East) Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applications |