Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 3.50 - 6.50 kJ/m²

@Temperature -30.0 - -30.0 °C
1.67 - 3.09 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 5.75 kJ/m² Grade Count:7
Overview of materials for Polystyrene, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a..
Izod Impact, Notched (ISO) 3.50 - 6.50 kJ/m²

@Thickness 4.00 - 4.00 mm
1.67 - 3.09 ft-lb/in²

@Thickness 0.157 - 0.157 in
Average value: 5.75 kJ/m² Grade Count:7
Overview of materials for Polystyrene, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a..
Izod Impact, Notched (ISO) 4.00 - 6.50 kJ/m²
1.90 - 3.09 ft-lb/in²
Average value: 5.22 kJ/m² Grade Count:9
Overview of materials for Acetal Copolymer, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va..
Izod Impact, Notched (ISO) 3.00 - 6.50 kJ/m²
1.43 - 3.09 ft-lb/in²
Average value: 4.44 kJ/m² Grade Count:8
Overview of materials for Polypropylene, Fiber Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Fiber Grade". Each property range of values reported is minimum and maximum values of app..
Izod Impact, Notched (ISO) 6.00 - 6.50 kJ/m²
2.86 - 3.09 ft-lb/in²
Average value: 6.33 kJ/m² Grade Count:3
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m..
Izod Impact, Notched (ISO) 6.50 - 6.50 kJ/m²

@Temperature -30.0 - -30.0 °C
3.09 - 3.09 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 6.50 kJ/m² Grade Count:1
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m..
Izod Impact, Notched (ISO) 4.00 - 6.50 kJ/m²
1.90 - 3.09 ft-lb/in²
Average value: 5.15 kJ/m² Grade Count:13