Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 2.00 kJ/m² @Temperature 23.0 °C |
0.952 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Konduit MT00EL PP LNP* Konduit* MT00EL is a Polypropylene base resin with thermal fillers. Characteristics of this grade are Thermal Conductivity and it is Low Extraactible.This data was supplied by SABIC-IP for th.. |
|||
Izod Impact, Notched (ISO) | 2.00 kJ/m² | 0.952 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP KONDUIT OX11314 PPS (Europe-Africa-Middle East) Thermally conductive mineral and glass fiber filled PPS Eco-FR compound |
|||
Izod Impact, Notched (ISO) | 2.00 - 10.0 kJ/m² @Temperature -30.0 - -30.0 °C |
0.952 - 4.76 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 5.50 kJ/m² Grade Count:4 |
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an.. |
|||
Izod Impact, Notched (ISO) | 2.00 - 62.0 kJ/m² | 0.952 - 29.5 ft-lb/in² | Average value: 11.4 kJ/m² Grade Count:8 |
Overview of materials for PET + PBT Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "PET + PBT Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Izod Impact, Notched (ISO) | 2.00 - 18.0 kJ/m² @Temperature -30.0 - -30.0 °C |
0.952 - 8.57 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 6.43 kJ/m² Grade Count:7 |
Overview of materials for PET + PBT Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "PET + PBT Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Izod Impact, Notched (ISO) | 2.00 - 20.0 kJ/m² | 0.952 - 9.52 ft-lb/in² | Average value: 8.39 kJ/m² Grade Count:45 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Izod Impact, Notched (ISO) | 2.00 kJ/m² | 0.952 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP BG004 SAN (Europe-Africa-Middle East) LNP* LUBRICOMP* BG004 is a compound based on Styrene Acrylonitril resin containing Graphite. Added features include: Internally Lubricated. |
|||
Izod Impact, Notched (ISO) | 2.00 kJ/m² | 0.952 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP CG006 PS (Europe-Africa-Middle East) LNP* Lubricomp* CG006 is a compound based on Polystyrene resin containing Graphite. |
|||
Izod Impact, Notched (ISO) | 2.00 - 4.00 kJ/m² @Temperature -40.0 - -20.0 °C |
0.952 - 1.90 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 3.00 kJ/m² Grade Count:4 |
Overview of materials for Nylon 6, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ.. |
|||
Izod Impact, Notched (ISO) | 2.00 - 7.00 kJ/m² @Temperature -40.0 - -20.0 °C |
0.952 - 3.33 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 3.71 kJ/m² Grade Count:5 |
Overview of materials for Nylon 66, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Izod Impact, Notched (ISO) | 2.00 kJ/m² | 0.952 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP IBP34 PA6.12 LNP* LUBRICOMP* IBP34 is a compound based on Nylon 6/12 containing 20% Glass Bead, 15% PTFE/Silicone. Added features include: Wear Resistant. |
|||
Izod Impact, Notched (ISO) | 2.00 kJ/m² | 0.952 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP OL003A PPS - Branched LNP* LUBRICOMP* OL003A is a compound based on PPS - Branched resin containing 15% PTFE. Added features of this grade are: Wear Resistant. |
|||
Izod Impact, Notched (ISO) | 2.00 kJ/m² | 0.952 ft-lb/in² | 80*10*4mm, Cut; ISO 180/1A |
SABIC Innovative Plastics SABIC PPCOMPOUND 19T1040 PP SABIC® PPcompound 19T1040 is a general purpose, talc filled, heat stabilized homopolymer polypropylene compound. This compound exhibits high flow and is suitable for injection molding application.. |
|||
Izod Impact, Notched (ISO) | 2.00 kJ/m² | 0.952 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP RN001S PA 66 (Asia Pacific) LNP* Lubricomp* RN001S is a compound based on Nylon 66 resin containing MOS2. Added features of this material include: Internally Lubricated, Heat Stabilized. |
|||
Izod Impact, Notched (ISO) | 2.00 kJ/m² | 0.952 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP ZX05506 PPE+PS (Asia Pacific) LNP LUBRICOMP* ZX05506 is a compound based on PPE+PS Blend resin containing Graphite Powder, PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched (ISO) | 2.00 kJ/m² @Temperature -30.0 °C |
0.952 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics ULTEM EXUM0167 PEI Blend Improved ductility, transparent, standard flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming. |
|||
Izod Impact, Notched (ISO) | 2.00 kJ/m² @Temperature -30.0 °C |
0.952 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics ULTEM EXUM0169 PEI Blend Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming. |
|||
Izod Impact, Notched (ISO) | 2.00 kJ/m² | 0.952 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Valox® 176 PBT Unreinforced, neat PBT resin for fibers. Natural Color Only, Not intended for injection molding. |
|||
Izod Impact, Notched (ISO) | 2.00 kJ/m² @Temperature -30.0 °C |
0.952 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Valox® EH7020HF PBT+PET (Asia Pacific) Valox EH7020HF is a mineral filled PBT/PET that offers good surface appearance, high flow and good heat performance. EH7020HF was developped for automotiove bezel application that require basecoat +.. |
|||
Izod Impact, Notched (ISO) | 2.00 kJ/m² @Temperature 0.000 °C |
0.952 ft-lb/in² @Temperature 32.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Valox® VX3101N PBT (Europe-Africa-Middle East) VALOX VX3101N is an unreinforced PBT injection moulding resin, with excellent flow properties, good hydrolitical stability and chemical resistance. |
|||
Izod Impact, Notched (ISO) | 2.00 kJ/m² @Temperature -30.0 °C |
0.952 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Valox® VX3101N PBT (Europe-Africa-Middle East) VALOX VX3101N is an unreinforced PBT injection moulding resin, with excellent flow properties, good hydrolitical stability and chemical resistance. |
|||
Izod Impact, Notched (ISO) | 2.00 kJ/m² @Temperature -30.0 °C |
0.952 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Valox® IQ325HP PBT (Europe-Africa-Middle East) FDA compliant PBT resin, using chemically recycled post consumer PET Bottles. Fit to food contact applications. |
|||
Izod Impact, Notched (ISO) | 2.00 kJ/m² | 0.952 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP MB008S PP LNP* THERMOCOMP* MB008S is a compound based on Polypropylene resin containing 40% Glass Bead. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Notched (ISO) | 2.00 kJ/m² @Temperature 23.0 °C |
0.952 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Thermocomp MB008S PP (Asia Pacific) LNP* Thermocomp* MB008S is a compound based on Polypropylene resin containing Glass Bead. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia Pa.. |
|||
Izod Impact, Notched (ISO) | 2.00 kJ/m² | 0.952 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOTUF CF007IXP PS LNP* Thermotuf* CF007IXP is a compound based on Polystyrene containing glass fiber. Characteristics of this grade are: High Impact. |
|||
Izod Impact, Notched (ISO) | 2.00 kJ/m² | 0.952 ft-lb/in² | ISO 180/1A |
Chi Mei Polyrex® PG-80 Polystyrene High strength |
|||
Izod Impact, Notched (ISO) | 2.00 kJ/m² @Temperature 0.000 °C |
0.952 ft-lb/in² @Temperature 32.0 °F |
80*10*4mm, Cut; ISO 180/1A |
SABIC Innovative Plastics SABIC PPCOMPOUND 15T1020 PP SABIC® PPcompound 15T1020. This grade is a general purpose, talc filled, heat stabilized polypropylene resin suitable for injection molded applications. The IMDS ID is 16486973. |
|||
Izod Impact, Notched (ISO) | 2.00 - 8.10 kJ/m² | 0.952 - 3.85 ft-lb/in² | Average value: 4.73 kJ/m² Grade Count:10 |
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m.. |
|||
Izod Impact, Notched (ISO) | 2.00 kJ/m² | 0.952 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP CX94108 PS (Europe-Africa-Middle East) LNP* LUBRICOMP* CX94108 is a compound based on Polystyrene resin containing Proprietary Lubricant. Added features include: Internally Lubricated. |