Material Notes:
LNP* LUBRICOMP* BG004 is a compound based on Styrene Acrylonitril resin containing Graphite. Added features include: Internally Lubricated.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ISO 1183
Water Absorption 0.19 %

@Time 86400 sec
0.19 %

@Time 24.0 hour
ISO 62-1
Linear Mold Shrinkage, Flow 0.0023 cm/cm
0.0023 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 64.0 MPa
9280 psi
5 mm/min; ISO 527
Elongation at Break 1.9 %
1.9 %
5 mm/min; ISO 527
Tensile Modulus 5.70 GPa
827 ksi
1 mm/min; ISO 527
Flexural Yield Strength 102 MPa
14800 psi
2 mm/min; ISO 178
Flexural Modulus 5.80 GPa
841 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 2.00 kJ/m²
0.952 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 12.0 kJ/m²
5.71 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 43.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
23.9 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 57.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
31.7 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 103 °C
217 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 96.0 °C
205 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af