Polymer Property : Izod Impact, Notched (ISO) = 18.0 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 2.00 - 18.0 kJ/m²

@Temperature -30.0 - -30.0 °C
0.952 - 8.57 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 6.43 kJ/m² Grade Count:7
Overview of materials for PET + PBT Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "PET + PBT Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Izod Impact, Notched (ISO) 18.0 - 18.0 kJ/m²

@Temperature -30.0 - -30.0 °C
8.57 - 8.57 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 18.0 kJ/m² Grade Count:1
Overview of materials for Polyphthalamide (PPA), High Impact
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, High Impact". Each property range of values reported is minimum and maximum values of a..
Izod Impact, Notched (ISO) 8.00 - 18.0 kJ/m²

@Temperature -30.0 - -20.0 °C
3.81 - 8.57 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 12.3 kJ/m² Grade Count:22
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is ..
Izod Impact, Notched (ISO) 7.00 - 18.0 kJ/m²

@Temperature -40.0 - -20.0 °C
3.33 - 8.57 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 11.0 kJ/m² Grade Count:18
Overview of materials for Nylon 6, Glass Filled, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu..
Izod Impact, Notched (ISO) 3.00 - 18.0 kJ/m²
1.43 - 8.57 ft-lb/in²
Average value: 8.38 kJ/m² Grade Count:42
Overview of materials for Nylon 66, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..
Izod Impact, Notched (ISO) 7.00 - 18.0 kJ/m²
3.33 - 8.57 ft-lb/in²
Average value: 9.87 kJ/m² Grade Count:22
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% ..
Izod Impact, Notched (ISO) 3.50 - 18.0 kJ/m²
1.67 - 8.57 ft-lb/in²
Average value: 8.53 kJ/m² Grade Count:3
Overview of materials for Polypropylene with 10% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be..
Izod Impact, Notched (ISO) 4.50 - 18.0 kJ/m²
2.14 - 8.57 ft-lb/in²
Average value: 6.57 kJ/m² Grade Count:7
Overview of materials for Polytrimethylene Terephthalate (PTT)
This property data is a summary of similar materials in the MatWeb database for the category "Polytrimethylene Terephthalate (PTT)". Each property range of values reported is minimum and maximum val..