Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 80.0 kJ/m²
38.1 ft-lb/in²
80*10*3; ISO 180/1U
SABIC Innovative Plastics Lexan® BFL2015 PC
Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only
Izod Impact, Unnotched (ISO) 80.0 kJ/m²

@Temperature -30.0 °C
38.1 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1U
SABIC Innovative Plastics Lexan® BFL2015 PC
Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only
Izod Impact, Unnotched (ISO) 80.0 kJ/m²

@Temperature -30.0 °C
38.1 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1U
SABIC Innovative Plastics Lexan® BFL2015 PC (Asia Pacific)
Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only
Izod Impact, Unnotched (ISO) 80.0 kJ/m²
38.1 ft-lb/in²
80*10*3; ISO 180/1U
SABIC Innovative Plastics Lexan® BFL2015 PC (Europe-Africa-Middle East)
Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only
Izod Impact, Unnotched (ISO) 80.0 kJ/m²
38.1 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP FARADEX MS003 PP (Asia Pacific)
LNP* Faradex* MS003 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Izod Impact, Unnotched (ISO) 80.0 kJ/m²
38.1 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP FARADEX MS003 PP (Europe-Africa-Middle East)
LNP* Faradex* MS003 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Izod Impact, Unnotched (ISO) 80.0 kJ/m²
38.1 ft-lb/in²
ASTM D256
PTS PBT-101G0 PBT Resin
Typical Applications: Appliance partsInformation provided by PTS LLC.
Izod Impact, Unnotched (ISO) 80.0 kJ/m²
38.1 ft-lb/in²
DIN 53453
Ineos Nova S-3401 Medium Impact Compact Polystyrene  (discontinued **)
Impact polystyrene with good flow characteristics and a high elongation. Generally used for applications where a tough material is required. The material is provided with external lubricate to imp..
Izod Impact, Unnotched (ISO) 80.0 - 100 kJ/m²

@Temperature -30.0 - -30.0 °C
38.1 - 47.6 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 95.7 kJ/m² Grade Count:7
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is ..
Izod Impact, Unnotched (ISO) 80.0 kJ/m²
38.1 ft-lb/in²
d.a.m.; ISO 180-1U
Lanxess Durethan® BKV 35 H3.0 000000 Nylon 6, Glass Fiber Reinforced
PA 6, 35% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS.
Izod Impact, Unnotched (ISO) 80.0 kJ/m²
38.1 ft-lb/in²
ISO 180/1eU
Solvay TECHNYLSTARâ„¢ S 216 V35 PA6, 35% glass filled, Conditioned
Description: TECHNYLSTAR polyamide, reinforced with 35% of glass fiber, for injection molding. Characterized by a high fluidity of the melt.Available in: Europe and North AmericaProduct Applications..
Izod Impact, Unnotched (ISO) 80.0 kJ/m²
38.1 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP RFL36S PA 66 (Europe-Africa-Middle East)
LNP* Lubricomp* RFL36S is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Heat Stabilized.
Izod Impact, Unnotched (ISO) 80.0 kJ/m²
38.1 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP RFL36SXS PA 66 (Europe-Africa-Middle East)
LNP* LUBRICOMP* RFL36SXS is a compound based on PA 66 resin containing Glass Fiber, PTFE. Added features include Internally Lubricated, Heat Stabilized.
Izod Impact, Unnotched (ISO) 80.0 kJ/m²
38.1 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP RFN18 PA 66 (Europe-Africa-Middle East)
LNP* Lubricomp* RFN18 is a compound based on Nylon 66 resin containing Glass Fiber, MOS2.
Izod Impact, Unnotched (ISO) 80.0 kJ/m²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Thermocomp RF006EU PA 66 (Europe-Africa-Middle East)
LNP* THERMOCOMP* RF006EU is a compound based on PA 66 resin containing Glass Fiber. Added features include: Easy Molding, UV-StabilizedThis data was supplied by SABIC-IP for the Europe-Africa-Middle..
Izod Impact, Unnotched (ISO) 80.0 kJ/m²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Thermocomp RF00ASXP PA6.6 (Europe-Africa-Middle East)
LNP* THERMOCOMP* RF00ASXP is a compound based on PA 66 resin containing Glass Fiber. Added features include: Heat Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regi..
Izod Impact, Unnotched (ISO) 80.0 kJ/m²
38.1 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP RF00ASXS PA6.6 (Europe-Africa-Middle East)
LNP* Thermocomp* RF00ASXS is a compound based on PA 66 resin containing Glass Fiber. Added features include: Heat Stabilized.
Izod Impact, Unnotched (ISO) 80.0 kJ/m²
38.1 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP YF006A Polyester Elastomer (Europe-Africa-Middle East)
LNP* THERMOCOMP* YF006A is a compound based on Polyester Elastomer containing Glass Fiber.
Izod Impact, Unnotched (ISO) 80.0 kJ/m²
38.1 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-KON DX05305C PC
LNP* STAT-KON* DX05305C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Clean Compounding System.
Izod Impact, Unnotched (ISO) 80.0 kJ/m²

@Temperature -30.0 °C
38.1 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Xenoy® X5630 PC+PET (Asia Pacific)
Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applications
Izod Impact, Unnotched (ISO) 80.0 kJ/m²

@Temperature -30.0 °C
38.1 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Xenoy® X5630Q PC+PET (Europe-Africa-Middle East)
Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applications
Izod Impact, Unnotched (ISO) 80.0 kJ/m²
38.1 ft-lb/in²
50%RH; ISO 180/1U
DuPont Performance Polymers Zytel® 80G33L NC010 Nylon 66  (Unverified Data**)
33% Glass Reinforced Toughened Polyamide 66 Zytel 80G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Inf..
Izod Impact, Unnotched (ISO) 80.0 kJ/m²

@Temperature -30.0 °C
38.1 ft-lb/in²

@Temperature -22.0 °F
DAM; ISO 180/1U
DuPont Performance Polymers Zytel® 80G33L NC010 Nylon 66  (Unverified Data**)
33% Glass Reinforced Toughened Polyamide 66 Zytel 80G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Inf..
Izod Impact, Unnotched (ISO) 80.0 kJ/m²
38.1 ft-lb/in²
80x10x4; ISO 180/1U
Eurostar Starflam MX06089 PP, Flame Retardant, Injection Molding
Starflam MX06089 is an Unfilled Flame Retardant Polypropylene Injection Molding ResinInformation provided by Eurostar.
Izod Impact, Unnotched (ISO) 80.0 kJ/m²
38.1 ft-lb/in²
ISO 180/1C
Chi Mei Polylac® PA-756H ABS - High Flow
Super high flow
Izod Impact, Unnotched (ISO) 80.0 kJ/m²
38.1 ft-lb/in²
80x10x4; ISO 180/1U
Eurostar Star L PA66 30V D51 PA66, Glass Fiber Filled, Injection Molded
Star L PA66 30V D51 is a PTFE lubricated, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
Izod Impact, Unnotched (ISO) 80.0 kJ/m²
38.1 ft-lb/in²
ASTM D256
BLUESTAR 101G0 PBT
Typical Applications: Appliance, partsInformation provided by Polymer Technology and Services, LLC (PTS).
Izod Impact, Unnotched (ISO) 80.0 kJ/m²
38.1 ft-lb/in²
ASTM D256
Beijing Ranger Chem PBT 403 M-G50 Heat Resistant and Environmental Protection Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Izod Impact, Unnotched (ISO) 80.0 kJ/m²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
80x10x4mm; ISO 180/1U
SYNTHOS Krasten® 552M High Impact Polystyrene
High impact grade with a wide range of Applications. Processed mainly by injection moulding. Production of consumer goods and technical parts subjected to increased mechanical stress. Good results i..
Izod Impact, Unnotched (ISO) 80.0 kJ/m²

@Temperature -30.0 °C
38.1 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Xenoy® X5630 PC+PET (Europe-Africa-Middle East)
Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applications