Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 80.0 - 100 kJ/m²

@Temperature -30.0 - -30.0 °C
38.1 - 47.6 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 95.7 kJ/m² Grade Count:7
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is ..
Izod Impact, Unnotched (ISO) 80.0 - 100 kJ/m²
38.1 - 47.6 ft-lb/in²
Average value: 85.0 kJ/m² Grade Count:4
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m..
Izod Impact, Unnotched (ISO) 30.0 - 100 kJ/m²
14.3 - 47.6 ft-lb/in²
Average value: 68.2 kJ/m² Grade Count:13
Overview of materials for Nylon 66, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr..
Izod Impact, Unnotched (ISO) 35.0 - 100 kJ/m²
16.7 - 47.6 ft-lb/in²
Average value: 58.9 kJ/m² Grade Count:12
Overview of materials for Nylon 66, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..
Izod Impact, Unnotched (ISO) 18.0 - 100 kJ/m²

@Temperature -30.0 - -30.0 °C
8.57 - 47.6 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 67.0 kJ/m² Grade Count:4
Overview of materials for Nylon 66, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu..
Izod Impact, Unnotched (ISO) 100 - 100 kJ/m²

@Temperature -30.0 - -30.0 °C
47.6 - 47.6 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 100 kJ/m² Grade Count:1
Overview of materials for Nylon 6, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v..
Izod Impact, Unnotched (ISO) 30.0 - 100 kJ/m²

@Temperature -30.0 - -30.0 °C
14.3 - 47.6 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 57.0 kJ/m² Grade Count:12
Overview of materials for Nylon 6, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro..
Copyright © lookpolymers.com All Rights Reserved