Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Unnotched (ISO) = 11.4 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 24.0 kJ/m²

@Thickness 4.00 mm,
Temperature 23.0 °C
11.4 ft-lb/in²

@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180
Premix Thermoplastics PRE-ELEC® ESD 6300 Static Dissipative Thermoplastic Compound
PRE-ELEC® ESD 6300 is a static dissipative thermoplastic compound based on high impact polystyrene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD6300 has be..
Izod Impact, Unnotched (ISO) 24.0 - 33.0 kJ/m²
11.4 - 15.7 ft-lb/in²
Average value: 28.4 kJ/m² Grade Count:5
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar..
Izod Impact, Unnotched (ISO) 24.0 kJ/m²

@Temperature -30.0 °C
11.4 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics NORYL V03505 PPE+HIPS (Europe-Africa-Middle East)
Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
Izod Impact, Unnotched (ISO) 24.0 kJ/m²
11.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP IN001 PA6.12
LNP* LUBRICOMP* IN001 is a compound based on Nylon 6/12 resin containing 2% Moly. Added feature of this grade is: Wear Resistant.
Izod Impact, Unnotched (ISO) 24.0 kJ/m²
11.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP JFL36 PES
LNP LUBRICOMP* JFL36 is a compound based on Polyethersulfone resin containing 30% Glass Fiber, 15% PTFE. Added featurs of this material is: Wear Resistant.
Izod Impact, Unnotched (ISO) 24.0 kJ/m²
11.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP JFL36 PES (Asia Pacific)
LNP LUBRICOMP* JFL36 is a compound based on Polyethersulfone resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched (ISO) 24.0 kJ/m²
11.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP KFP032 Acetal Copolymer
LNP LUBRICOMP* KFP032 is a compound based on Acetal Copolymer resin containing 10% Glass Fiber, 15% PTFE/Silicone. Added feature of this material is: Wear Resistant.
Izod Impact, Unnotched (ISO) 24.0 kJ/m²

@Temperature 23.0 °C
11.4 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Lubricomp OFB32I PPS
LNP LUBRICOMP* OFB32I is a compound based on Polyphenylene Sulfide resin containing Carbon Fiber, PTFE. Added features of this material include: Electrically Conductive.This data was supplied by SA..
Izod Impact, Unnotched (ISO) 24.0 kJ/m²
11.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP OFL36 PPS - Linear
LNP* LUBRICOMP* OFL36 is a compound based on PPS - Linear resin containing 30% Glass Fiber, 15% PTFE. Added features of this grade include: Wear Resistant.
Izod Impact, Unnotched (ISO) 24.0 kJ/m²
11.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP OX97635 PPS
LNP LUBRICOMP* OX97635 is a compound based on Polyphenylene Sulfide resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Wear Resistant.
Izod Impact, Unnotched (ISO) 24.0 kJ/m²
11.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP RAP22 PA 66
LNP* LUBRICOMP* RAP22 is a compound based on Nylon 66 resin containing 10% Aramid, 10% PTFE/Silicone. Added feature of this grade includes: Wear Resistant.
Izod Impact, Unnotched (ISO) 24.0 kJ/m²
11.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP RFL449 PA 66
LNP* LUBRICOMP* RFL449 is a compound based on Nylon 66 resin containing 20% Glass Fiber, 20% PTFE. Added features of this grade include: Wear Resistant, Flame Retardant.
Izod Impact, Unnotched (ISO) 24.0 kJ/m²
11.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP ZFL31XXC PPE+PS
LNP* LUBRICOMP* ZFL31XXC is a compound based on PPE+PS resin containing 5% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant
Izod Impact, Unnotched (ISO) 24.0 kJ/m²
11.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-KON DE0069F PC
LNP* STAT-KON* DE0069F is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, Superior Molding.
Izod Impact, Unnotched (ISO) 24.0 kJ/m²
11.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-KON DEL13EXC PC
LNP STAT-KON* DEL13EXC is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 5% PTFE. Added features of this material include: Easy Molding, Electrically Conductive, Wear Resistan..
Izod Impact, Unnotched (ISO) 24.0 kJ/m²
11.4 ft-lb/in²
ISO 180
Solvay Specialty Polymers Ryton® BR111 Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® BR111 is a natural-colored glass fiber and mineral filled polyphenylene sulfide compound that provides enhanced mechanical strength with good electrical properties and outstanding chemical..
Izod Impact, Unnotched (ISO) 24.0 kJ/m²

@Temperature 23.0 °C
11.4 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Stat-kon DEL369E PC
LNP* Stat-Kon* DEL369E is a compound based on Polycarbonate containing Carbon Fiber and PTFE. Characteristics of this grade are Flame Retardant and Statically Conductive.This data was supplied by S..
Izod Impact, Unnotched (ISO) 24.0 kJ/m²

@Temperature 23.0 °C
11.4 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Stat-kon DEP32XXC PC
LNP STAT-KON* DEP32XXC is a compound based on Polycarbonate resin containing Carbon Fiber, Silicone, PTFE. Added features of this material include: Electrically Conductive.This data was supplied by..
Izod Impact, Unnotched (ISO) 24.0 kJ/m²

@Temperature 23.0 °C
11.4 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Stat-kon DEP32XXC PC (Asia Pacific)
LNP* STAT-KON* DEP32XXC is a compound based on Polycarbonate resin containing PTFE, Silicone, Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied b..
Izod Impact, Unnotched (ISO) 24.0 kJ/m²
11.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP AF002 ABS
LNP THERMOCOMP* AF002 is a compound based on ABS resin containing 10% Glass Fiber.
Izod Impact, Unnotched (ISO) 24.0 kJ/m²

@Temperature 23.0 °C
11.4 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Thermocomp EB004 PEI
LNP* Thermocomp* EB004 is a compound based on Polyetherimide resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched (ISO) 24.0 kJ/m²
11.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP EC005 PEI
LNP THERMOCOMP* EC005 is a compound based on Polyetherimide resin containing 25% Carbon Fiber. Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched (ISO) 24.0 kJ/m²

@Temperature 23.0 °C
11.4 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Thermocomp RW008XXZ PA 66
LNP* Thermocomp* RW008XXZ is a compound based on Nylon 6/6 resin containing Wollastonite.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched (ISO) 24.0 kJ/m²
11.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics NORYL NH7112 PPE+HIPS (Asia Pacific)
Noryl* NH7112 resin is a 10% glass reinforced, modified PPE-PS blend. The material offers an exceptional balance of strength and dimensional stability while using non-halogenated flame retardants to..
Izod Impact, Unnotched (ISO) 24.0 kJ/m²
11.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics NORYL NH7112 PPE+HIPS (Europe-Africa-Middle East)
Noryl* NH7112 resin is a 10% glass reinforced, modified PPE-PS blend. The material offers an exceptional balance of strength and dimensional stability while using non-halogenated flame retardants to..
Izod Impact, Unnotched (ISO) 24.0 kJ/m²
11.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-KON RE002 PA 66
LNP* STAT-KON* RE002 is a compound based on Nylon 66 resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched (ISO) 24.0 kJ/m²
11.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-KON RE002 PA 66 (Asia Pacific)
LNP* Stat-kon* RE002 is a compound based on Nylon 66 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched (ISO) 24.0 kJ/m²
11.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-KON RE0029 PA 66
LNP* STAT-KON* RE0029 is a compound based on Nylon 66 resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant.
Izod Impact, Unnotched (ISO) 24.0 kJ/m²
11.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP AF002XXC ABS
LNP THERMOCOMP* AF002XXC is a compound based on ABS resin containing 10% Glass Fiber.
Izod Impact, Unnotched (ISO) 24.0 kJ/m²
11.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP MF002AS PP
LNP THERMOCOMP* MF002AS is a compound based on Polypropylene resin containing 10% Glass Fiber. Added features of this material include: Heat Stabilized.