Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 6.50 J/cm² | 30.9 ft-lb/in² | DIN 53453 |
Nilit FRIANYL A63 HH-KV30 Nylon 6.6 for injection molding, 30% glass ball reinforced Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® HTN 52G45HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN52G45HSL BK083 is a 45% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds. It is also a PPA resin.Information provide.. |
|||
Charpy Impact Unnotched | 6.50 J/cm² | 30.9 ft-lb/in² | ISO 179-1eU |
Lanxess Pocan® B 3233 HR 000000 Polybutylene Terephthalate, 30% Glass Fibers PBT, 30% glass fibers, injection molding, improved flowability, hydrolysis stabilized |
|||
Charpy Impact Unnotched | 6.50 J/cm² | 30.9 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1-0889-4 Polyamide 66, with carbon fiber and glass fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically .. |
|||
Charpy Impact Unnotched | 6.50 J/cm² | 30.9 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1105/MS/15/TF/15 PEEK, with PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts,.. |
|||
Charpy Impact Unnotched | 6.50 J/cm² | 30.9 ft-lb/in² | |
LATI Latiohm 66-07 PD08 G/30 PA66, 30% Glass Fiber Reinforced Semiconductive/dissipative product based on Polyamide 66 (PA66). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |
|||
Charpy Impact Unnotched | 6.50 J/cm² | 30.9 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1105/XCF/30 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Charpy Impact Unnotched | 6.50 J/cm² | 30.9 ft-lb/in² | ISO 179-1 |
Unitika A3130HR-25 PA6, 25% Mineral Reinforced, Conditioned Information provided by Unitika Ltd. |
|||
Charpy Impact Unnotched | 6.50 J/cm² | 30.9 ft-lb/in² | ISO 179 |
Polyram Polytron P40N11 Polypropylene, 40% Long Glass Fibers A chemically coupled 40% long glass fiber reinforced natural polypropylene, heat stabilized, for injection molding applications.Information provided by Polyram. |
|||
Charpy Impact Unnotched | 6.50 J/cm² @Temperature 30.0 °C |
30.9 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® BG-35 PA6-GF35 Product description: Grilon BG-35 is a heat stabilized PA6 injection molding grade with 35% glass fibers. Grilon BG-35 has the following important properties: High stiffness Good surface finishEasy.. |
|||
Charpy Impact Unnotched | 6.50 J/cm² @Temperature 30.0 °C |
30.9 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® BG-40 HM PA6-GF40 Product description: Grilon BG-40 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 40% glass fibers. Grilon BG-40 HM has the following important prop.. |
|||
Charpy Impact Unnotched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6600 GV 25 DCHP 25% Glass Fiber Nylon 66, Special Heat Ageing Stabilization, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact Unnotched | 6.50 J/cm² @Temperature 30.0 °C |
30.9 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® LKN-5H PA12-GB50 Product description: Grilamid LKN-5H is a 50% glass bead reinforced, heat stabilized polyamide 12 injection molding grade with the following property profile: Very low moisture absorptionExtremely g.. |
|||
Charpy Impact Unnotched | 6.50 J/cm² @Temperature 30.0 °C |
30.9 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® TSG-30 PA666-GF30 Product description: Grilon TSG-30 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% glass fibers. Grilon TSG-30 has the following important properties: Excellent fl.. |
|||
Charpy Impact Unnotched | 6.50 J/cm² | 30.9 ft-lb/in² | ISO 179/1eU |
DuPont Performance Polymers Crastin® HR5330HF BK503 Polybutylene Terephthalate (PBT)
(Unverified Data**)& 30% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5330HF is a 30% glass reinforced PBT with high flow (HF) moderately toughened hydrolysis resistant (HR) resin. Excellen.. |
|||
Charpy Impact Unnotched | 6.50 J/cm² | 30.9 ft-lb/in² | ISO 179/1eU |
DuPont Performance Polymers Crastin® HR5330HFS BK591 Polybutylene Terephthalate (PBT)
(Unverified Data**) 30% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5330HFS is a 30% glass fiber reinforced moderately toughened hydrolysis resistant polybutylene terephthalate for inject.. |
|||
Charpy Impact Unnotched | 6.50 J/cm² | 30.9 ft-lb/in² | ISO 179/1eU |
DuPont Performance Polymers Crastin® SK605 BK851 Polybutylene Terephthalate (PBT)
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Crastin SK605 BK851 is a 30% glass fiber reinforced lubricated black polybutylene terephthalate resin for injection molding.Information provided by Du.. |
|||
Charpy Impact Unnotched | 6.50 J/cm² | 30.9 ft-lb/in² | DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® HTN FE350038 BK083 Polyphthalamide (PPA) 33% Glass Reinforced PPA High Performance Polyamide Zytel HTNFE350038 BK083 is a 33% glass reinforced heat stabilized lubricated hydrolysis resistant high performance polyamide resin developed for i.. |
|||
Charpy Impact Unnotched | 6.50 J/cm² | 30.9 ft-lb/in² | Edgew 80x10x4; ISO 179/1eU |
Eurostar Staramide AG4 PA66, 20% Glass Filled, Injection Molded AG4 is a 20% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Charpy Impact Unnotched | 6.50 J/cm² | 30.9 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® XE 4216 black 9233 PA6T/66-GF30 Product description: Grivory XE 4216 black 9233 is a high heat stabilized, 30% glass fiber reinforced, semicrystalline, thermoplastic engineering material for injection molding. Polymer designation .. |
|||
Charpy Impact Unnotched | 6.50 J/cm² | 30.9 ft-lb/in² | |
BASF Procom® GC20S 400 Polypropylene Uses: electrical appliance housings (e.g. drills), components requiring high impact and temperature resistance, furniture frames.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 6.50 J/cm² | 30.9 ft-lb/in² | Conditioned; ISO 179/IeU |
Addiplast Addinyl A2 ZV30 Nylon 66, 30% Glass Filled Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast. |
|||
Charpy Impact Unnotched | 6.50 J/cm² @Temperature -30.0 °C |
30.9 ft-lb/in² @Temperature -22.0 °F |
|
Polimeri Europa EDISTIR PD RK6223N High Impact Polystyrene (HIPS)
(discontinued **) Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,M,083-12-07-23 Halogen and Antimony free, medium impact polystyrene. This grade complies at 2 mm with IEC 65-20-2 and BSI.. |
|||
Charpy Impact Unnotched | 6.50 J/cm² | 30.9 ft-lb/in² | ISO 179/IeU |
Addiplast Addinyl B2 V30 Nylon 6, 30% Glass Filled Glass fiber reinforced, high strengthInformation provided by Addiplast. |
|||
Charpy Impact Unnotched | 6.50 J/cm² | 30.9 ft-lb/in² | ISO 179/IeU |
Addiplast Addinyl B2 V40 Nylon 6, 40% Glass Filled Glass fiber reinforced, high strengthInformation provided by Addiplast. |
|||
Charpy Impact Unnotched | 6.50 J/cm² | 30.9 ft-lb/in² | ISO 179/IeU |
Addiplast Addinyl B2 ZV30 Nylon 6, 30% Glass Filled Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast. |
|||
Charpy Impact Unnotched | 6.50 J/cm² | 30.9 ft-lb/in² | Conditioned; ISO 179/IeU |
Addiplast Addinyl B2H G15 Flame Retardant Nylon 6, 15% Glass Bead Flame retardant, 15% glass bead filled, with halogensInformation provided by Addiplast. |
|||
Charpy Impact Unnotched | 6.50 J/cm² | 30.9 ft-lb/in² | ISO 179/IeU |
Addiplast Addinyl C2 ZV40 Nylon 66/6, 40% Glass Filled Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast. |