Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lehmann & Voss LUVOCOM® 1105/XCF/30 PEEK, with carbon fiber

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Carbon Fiber Filled
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOCOM®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOCOM® 1105/XCF/30 PEEK, with carbon fiber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts, non flammable.Electrically conductive, suitable for continuous discharging of statically generated electricity.Bearings, sleeves, control disks, gear wheels, pump impellers, gear parts.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.41 g/cc
1.41 g/cc
ISO 1183
Water Absorption <= 0.10 %
<= 0.10 %
23°C/24h
Linear Mold Shrinkage 0.00050 - 0.0020 cm/cm
0.00050 - 0.0020 in/in
Mechanical Properties Metric English Comments
Tensile Stress 320 MPa
46400 psi
Elongation at Yield 1.8 %
1.8 %
2.1 %
2.1 %
flexural
Modulus of Elasticity 32.0 GPa
4640 ksi
Flexural Strength 445 MPa
64500 psi
Flexural Modulus 27.0 GPa
3920 ksi
Charpy Impact Unnotched 6.50 J/cm²
30.9 ft-lb/in²
edgewise; ISO 179 1eU
Charpy Impact, Notched 0.900 J/cm²
4.28 ft-lb/in²
ISO 179 1eA
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 250 °C
482 °F
300 °C
572 °F
short term
Deflection Temperature at 1.8 MPa (264 psi) 330 °C
626 °F
Electrical Properties Metric English Comments
Surface Resistance <= 1000 ohm
<= 1000 ohm
Insulation Resistance <= 1000 ohm
<= 1000 ohm
Processing Properties Metric English Comments
Processing Temperature 390 °C
734 °F
mass temp
Nozzle Temperature 360 - 380 °C
680 - 716 °F
Zone 1 360 - 370 °C
680 - 698 °F
Zone 2 380 - 390 °C
716 - 734 °F
Zone 3 390 - 400 °C
734 - 752 °F
Mold Temperature 170 - 200 °C
338 - 392 °F
Drying Temperature 120 °C

@Time 21600 - 28800 sec
248 °F

@Time 6.00 - 8.00 hour
or
150 °C

@Time 10800 - 21600 sec
302 °F

@Time 3.00 - 6.00 hour
Dehumidifying dryer
Descriptive Properties Value Comments
Color natural color (black)