Addiplast Addinyl B2H G15 Flame Retardant Nylon 6, 15% Glass Bead

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass Bead Filled , Nylon 6, Glass Fiber Filled, Flame Retardant
Manufacturer Addiplast
Trade Name Addinyl
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Addiplast Addinyl B2H G15 Flame Retardant Nylon 6, 15% Glass Bead.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Flame retardant, 15% glass bead filled, with halogensInformation provided by Addiplast.
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Hardness, Shore D 86
86
Conditioned; ISO 868
88
88
ISO 868
Tensile Strength at Break 32.0 MPa
4640 psi
Conditioned; ISO R 527
62.0 MPa
8990 psi
ISO R 527
Elongation at Break 4.0 %
4.0 %
ISO R 527
25 %
25 %
Conditioned; ISO R 527
Modulus of Elasticity 1.60 GPa
232 ksi
Conditioned; ISO 178
3.60 GPa
522 ksi
ISO 178
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
Conditioned; ISO 180/1A
3.50 kJ/m²
1.67 ft-lb/in²
ISO 180/1A
Charpy Impact Unnotched 2.50 J/cm²
11.9 ft-lb/in²
ISO 179/IeU
6.50 J/cm²
30.9 ft-lb/in²
Conditioned; ISO 179/IeU
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
ISO 179/IeA
0.300 J/cm²
1.43 ft-lb/in²
Conditioned; ISO 179/IeA
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ISO 3146/C2
Deflection Temperature at 1.8 MPa (264 psi) 98.0 °C
208 °F
ISO 75-2/AF
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
Oxygen Index 30 %
30 %
ISO 4589
Glow Wire Test 960 °C
1760 °F
CEI 60695/2/1
Electrical Properties Metric English Comments
Comparative Tracking Index 250 V
250 V
CEI 60112/Solution A