Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 4.00 - 6.90 J/cm² @Temperature -30.0 - 30.0 °C |
19.0 - 32.8 ft-lb/in² @Temperature -22.0 - 86.0 °F |
Average value: 5.95 J/cm² Grade Count:13 |
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DuPont Performance Polymers Rynite® FR530L BK507 PET
(Unverified Data**) Rynite® FR530L BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 4.00 J/cm² | 19.0 ft-lb/in² | DIN 53453 |
Nilit FRIANYL C73 GV40 Nylon 6.6/6 for injection molding, 40% glass fiber reinforced Nylon 6.6/6 for injection molding, medium viscosity.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 4.00 - 6.50 J/cm² | 19.0 - 30.9 ft-lb/in² | Average value: 5.23 J/cm² Grade Count:10 |
Overview of materials for Nylon 66, Glass/Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² | 19.0 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1105-7938/GY PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² | 19.0 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1106-7622 Polyether imide, with carbon fiber Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.High dimensionally stable precision parts.Electrical.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Lehmann & Voss LUVOCOM® 1-RG 2 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² | 19.0 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 3-8266 Polyamide 6, unreinforced Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² | 19.0 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 50-7110 Polycarbonate, with carbon fiber, low-warpage, easy flowing Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Electrically conductive, suitable for continuous discharging o.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² | 19.0 ft-lb/in² | |
LATI Latan 13 S/20 POM, 20% Glass Bead Reinforced Polyoxymethylene (POM) based compound. Glass beads. Medium viscosity. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Lehmann & Voss LUVOCOM® 1105-0918/BL PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics NORYL V01525 PPE+HIPS (Europe-Africa-Middle East) Noryl* V01525 is a 15% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² | 19.0 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics ULTEM 2300R PEI (Europe-Africa-Middle East) 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Charpy Impact Unnotched | 4.00 J/cm² | 19.0 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics ULTEM 2310F PEI (Europe-Africa-Middle East) 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 listing. US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics ULTEM 2410R PEI (Europe-Africa-Middle East) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Valox® 4012 PBT (Europe-Africa-Middle East) VALOX 4012 is a 10% high strength glass fibre reinforced PBT injection moulding resin with improved mechanical properties. Applications: connectors. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Valox® 8032UX PBT+PET VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics NORYL GTX GTX830 PPE+PA (Europe-Africa-Middle East) NORYL GTX830 a 30% glass reinforced grade which offers an excellent combination of chemical/heat resistance in combination with stiffness. |
|||
Charpy Impact Unnotched | 4.00 J/cm² | 19.0 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics NORYL GTX GTX975 PPE+PA NORYL GTX975 is a 18% mineral filled material especially designed for in- or on-line painted exterior automotive trim part, e.g. tankflaps and corner panels. This material combines high stiffness an.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² | 19.0 ft-lb/in² | ISO 179-1 |
Unitika RUN35-C25 PA6, Conditioned High modulus and low warpage nylonInformation provided by Unitika Ltd. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6600 MR 309 HWCP 30% Mineral Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature 30.0 °C |
19.0 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® HT2V-3H PA6T/66-GF30 Product description: Grivory HT2V-3H is a 30 % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamde. Polymer designation acc. to ISO: .. |
|||
Charpy Impact Unnotched | 4.00 J/cm² | 19.0 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® XE 4164 black 9225 PA*-GF30 Product description: Grivory XE 4164 black 9225 is a 30% glass fiber reinforced engineering thermoplastic material based on a semicrystalline, partially aromatic copolyamide. ISO polymer designation.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature 30.0 °C |
19.0 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® BG-50 HM PA6-GF50 Product description: Grilon BG-50 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 50% glass fibers. Grilon BG-50 HM has the following important prop.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6000 GVS 10/20 HWCP 10% Glass Fiber and 20% Glass Sphere Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact Unnotched | 4.00 J/cm² | 19.0 ft-lb/in² | ISO 179/1eU |
DuPont Performance Polymers Crastin® SO653 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 20% Glass Bead Filled Polybutylene Terephthalate with Low Warpage CharacteristicsCrastin SO653 NC010 is a 20% glass bead filled polybutylene terephthalate resin for injection molding. It has isotrop.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² | 19.0 ft-lb/in² | ISO 179-1eU |
Barlog Plastics KEBATRON L1040G3 PPS, linear, 40% glass fiber reinforced PPS-GF40Information provided by BARLOG plastics GmbH. |
|||
Charpy Impact Unnotched | 4.00 J/cm² | 19.0 ft-lb/in² | ISO 179 |
Teijin Panlite® GV-3410R High Flame Retardancy, Glass Fiber Reinforced Polycarbonate Resin GF 10% reinforced, improved flame retardance and mold release grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need mechanical property e.g., stiffnessPrecis.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² | 19.0 ft-lb/in² | ISO179 |
Beijing Chemical Industry KAIFA® MN301-G0 Nylon 66 Resin High flame retardant, Good flowInformation provided by Beijing Chemical Industry Research Institute (Group) |