Polymer Property : Charpy Impact, Notched = 11.9 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 2.50 J/cm²

@Temperature -20.0 °C
11.9 ft-lb/in²

@Temperature -4.00 °F
ISO 179
Polykemi AB POLYblend 85H PC/ABS-Blend
Information provided by Polykemi AB
Charpy Impact, Notched 2.50 J/cm²

@Temperature -20.0 °C
11.9 ft-lb/in²

@Temperature -4.00 °F
ISO 179
Polykemi AB POLYblend 85VB PC/ABS-Blend, Flame Retardant
Information provided by Polykemi AB
Charpy Impact, Notched 2.50 J/cm²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Cycoloy® FXC813SK PC+ABS (Europe-Africa-Middle East)
CYCOLOY FXC813SK is a multi purpose PC+ABS injection moulding grade, providing a favourable balance of engineering properties. CYCOLOY FXC813SK is suitable for those applications that require sparkl..
Charpy Impact, Notched 2.50 J/cm²

@Temperature -20.0 °C
11.9 ft-lb/in²

@Temperature -4.00 °F
ISO 179
Polykemi AB SCANMID 6 B52^ E Nylon 6, Modified
Information provided by Polykemi AB
Charpy Impact, Notched 2.50 J/cm²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® EXL4019 PC (Europe-Africa-Middle East)
Lexan* EXL4019 is an opaque 9% Glass Fiber (GF) reinforced polycarbonate (PC) siloxane copolymer resin for injection molding (IM) applications requiring improved stiffness. This resin also offers im..
Charpy Impact, Notched 2.50 J/cm²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
PolyOne Bergamid™ A700 TM-YF Polyamide 66 (Nylon 66)
Information provided by PolyOne
Charpy Impact, Notched 2.50 J/cm²

@Temperature -30.0 °C
11.9 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
DuPont Performance Polymers Hytrel® 6359FG NC010 TPC-ET  (Unverified Data**)
Hytrel® 6359FG is a medium modulus Hytrel® grade with nominal durometer hardness of 63D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing t..
Charpy Impact, Notched 2.50 J/cm²

@Temperature -20.0 °C
11.9 ft-lb/in²

@Temperature -4.00 °F
ISO 179
Polykemi AB POLYfill PP TOUCH 25325 Polypropylene, Glass Fiber Reinforced
Information provided by Polykemi AB
Charpy Impact, Notched 2.50 J/cm²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Cycoloy® FXC810MA PC+ABS (Europe-Africa-Middle East)
CYCOLOY FXC810MA is a multi-purpose PC+ABS injection moulding grade, suitable for those applications that require marble colour effects. The colour package may effect performance.This data was suppl..
Charpy Impact, Notched 2.50 J/cm²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Cycoloy® FXC810SL PC+ABS (Europe-Africa-Middle East)
CYCOLOY FXC810SL is a multi-purpose PC+ABS injection moulding grade, suitable for those applications that require sparkle colour effects with lowered RFI inhibitor. Colour package may effect perform..
Charpy Impact, Notched 2.50 J/cm²

@Temperature -30.0 °C
11.9 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
DSM Stapron® E EM 605 Polycarbonate/PET Blend (European Grade)  (discontinued **)
Information provided by DSM.
Charpy Impact, Notched 2.50 J/cm²

@Temperature -30.0 °C
11.9 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
DSM Akulon® S223-TP4 (Dry) Impact Modified Nylon 66 (North America)  (discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Charpy Impact, Notched 2.50 J/cm²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
DSM Akulon® Ultraflow™ K-FG0 Nylon 6-50% Glass Reinforced (European and Asian Grade) (Cond)  (discontinued **)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Charpy Impact, Notched 2.50 J/cm²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
50%RH; ISO 179/1eA
DuPont Performance Polymers Zytel® 73G30T BK261 Nylon 6  (Unverified Data**)
Zytel® 73G30T BK261 is a 30% glass fiber reinforced, toughened, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Charpy Impact, Notched 2.50 J/cm²

@Temperature -30.0 °C
11.9 ft-lb/in²

@Temperature -22.0 °F
ISO 179
LG Chemical RS-800 ABS, Extrusion, High Impact, HCFC Resistant
Information Provided by LG Chem
Charpy Impact, Notched 2.50 J/cm²

@Temperature -40.0 °C
11.9 ft-lb/in²

@Temperature -40.0 °F
ISO 179/1eA
Kuraray Genestarâ„¢ N1006D-H31 Nylon
Standard unreinforced extrusion grade. Main Features:Chemical resistanceLong term heat resistanceExample of applications:Tube applications
Charpy Impact, Notched 2.50 J/cm²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
Conditioned; ISO 179/1eA
Lanxess Durethan® B 31 SK 000000 Nylon 6
PA 6, injection molding grade, non-reinforced, easy flow, easy-release, rapid solidification, crystallizes somewhat more finely and uniformly than B 30 S
Charpy Impact, Notched 2.50 J/cm²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
Conditioned; ISO 179-1eA
Lanxess Durethan® BKV 50 H3.0 000000 Nylon 6, 50% Glass Fibers
PA 6, 50% glass fibers, injection molding, heat-ageing stabilized
Charpy Impact, Notched 2.50 J/cm²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Solvay TECHNYL® eXten D 437P PA6.10
Description: TECHNYL® eXten D 437P is a high viscosity, unfilled, plasticized, UV and heat stabilized PA6.10 for extrusion applications. Technyl® eXten D 437P is a partially biosourced materia..
Charpy Impact, Notched 2.50 J/cm²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Sax Polymers SAXLAC 310A Acrylonitrile Butadiene Styrene
Saxalac 310A is a medium viscosity, impact resistant ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.Information provid..
Charpy Impact, Notched 2.50 J/cm²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
cond; ISO 179/1eA
DSM Akulon® K224-G6-FC 99.99.99 PA6-GF30
30% Glass Reinforced, Food Contact Grade
Charpy Impact, Notched 2.50 J/cm²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
DSM Akulon® Ultraflow™ K-FHG12 Nylon 6-60% Glass Reinforced (European and Asian Grade) (Cond)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Charpy Impact, Notched 2.50 J/cm²

@Temperature -30.0 °C
11.9 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
DSM Arnitel® EM550 55 Shore D, Extrusion Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Charpy Impact, Notched 2.50 J/cm²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
cond; ISO 179/1eA
DSM EcoPaXX® Q-X07209 PA410-I-GF40
% Glass Reinforced, Impact Modified
Charpy Impact, Notched 2.50 J/cm²

@Temperature -30.0 °C
11.9 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
DSM Arnitel® EL550 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Charpy Impact, Notched 2.50 J/cm²

@Temperature -30.0 °C
11.9 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Ascend Performance Materials Vydyne® 41H NT Nylon 66, Impact Modified, Conditioned
Vydyne® 41H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyn..
Charpy Impact, Notched 2.50 J/cm²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Ascend Performance Materials Vydyne® 66J Nylon 66, General Purpose, high viscosity, Conditioned
Vydyne® 66J is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66J resin offers high strength, ..
Charpy Impact, Notched 2.50 J/cm²

@Temperature -30.0 °C
11.9 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
DSM Akulon® K223-TP4 (Cond.) Impact Modified Nylon 6 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Charpy Impact, Notched 2.50 J/cm²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Ascend Performance Materials Vydyne® R633 Nylon 66 Copolymer, 33% Glass Filled, Conditioned (2.5% Moisture)
Vydyne® R633 is 33% glass-fiber reinforced, PA66/6 copolymer resin for superior surface appearance. Available in natural, this injection-molding grade resin is lubricated for machine feed and mold ..
Charpy Impact, Notched 2.50 J/cm²

@Temperature -30.0 °C
11.9 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Polyram RamSter PF801 PBT, High Impact Modified
High impact modified PBT for injection molding applications.Information provided by Polyram.