| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Charpy Impact, Notched |
2.50
J/cm² <br>@Thickness 102 mm,<br> Temperature 23.0 °C
|
11.9
ft-lb/in² <br>@Thickness 4.00 in,<br> Temperature 73.4 °F
|
ISO 179 |
|
Premix Thermoplastics PRE-ELEC® PE 1296 Conductive Thermoplastic Compound
PRE-ELEC® PE 1296 is a conductive thermoplastic masterbatch/compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. PRE-ELEC® PE 1296 has a high concentration o..
|
|||
| Charpy Impact, Notched |
2.50
J/cm² <br>@Thickness 102 mm,<br> Temperature 23.0 °C
|
11.9
ft-lb/in² <br>@Thickness 4.00 in,<br> Temperature 73.4 °F
|
ISO 179 |
|
Premix Thermoplastics PRE-ELEC® PS 1331 Carbon Black Filled Conductive Thermoplastic Compound
PRE-ELEC® PS 1331 is a carbon black filled conductive thermoplastic compound based on polystyrene. In addition to a low electrical resistivity PRE-ELEC® PS 1331 has excellent mechanical properties..
|
|||
| Charpy Impact, Notched |
2.50
J/cm² <br>@Temperature 23.0 °C
|
11.9
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179 |
|
Polykemi AB SCANTEC PC S85R Polycarbonate
Information provided by Polykemi AB
|
|||
| Charpy Impact, Notched |
2.50
J/cm² <br>@Temperature 23.0 °C
|
11.9
ft-lb/in² <br>@Temperature 73.4 °F
|
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® EXL4419 PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL4419 polycarbonate (PC) siloxane copolymer resin is a 9% Glass Fiber (GF) reinforced opaque injection molding (IM) grade. This medium flow resin offers much higher ductility, improved rele..
|
|||
| Charpy Impact, Notched |
2.50
J/cm² <br>@Temperature -20.0 °C
|
11.9
ft-lb/in² <br>@Temperature -4.00 °F
|
ISO 179 |
|
Polykemi AB POLYfill PP TOUCH 25325 Polypropylene, Glass Fiber Reinforced
Information provided by Polykemi AB
|
|||
| Charpy Impact, Notched |
2.50
J/cm² <br>@Temperature 23.0 °C
|
11.9
ft-lb/in² <br>@Temperature 73.4 °F
|
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Cycoloy® FXC810MA PC+ABS (Europe-Africa-Middle East)
CYCOLOY FXC810MA is a multi-purpose PC+ABS injection moulding grade, suitable for those applications that require marble colour effects. The colour package may effect performance.This data was suppl..
|
|||
| Charpy Impact, Notched |
2.50
J/cm² <br>@Temperature 23.0 °C
|
11.9
ft-lb/in² <br>@Temperature 73.4 °F
|
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Cycoloy® FXC810SK PC+ABS (Europe-Africa-Middle East)
CYCOLOY FXC810SK is a multi purpose PC+ABS injection moulding grade, providing a favourable balance of engineering properties. CYCOLOY FXC810SK is suitable for those applications that require sparkl..
|
|||
| Charpy Impact, Notched |
2.50
J/cm² <br>@Temperature 23.0 °C
|
11.9
ft-lb/in² <br>@Temperature 73.4 °F
|
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Cycoloy® FXC810SL PC+ABS (Europe-Africa-Middle East)
CYCOLOY FXC810SL is a multi-purpose PC+ABS injection moulding grade, suitable for those applications that require sparkle colour effects with lowered RFI inhibitor. Colour package may effect perform..
|
|||
| Charpy Impact, Notched |
2.50
J/cm² <br>@Temperature 23.0 °C
|
11.9
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eA |
|
DSM Akulon® K-FHG12 (Cond.) 60% Glass Reinforced Nylon 6 (North America)
(discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Charpy Impact, Notched |
2.50
J/cm² <br>@Temperature 23.0 °C
|
11.9
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eA |
|
DSM Akulon® K224-G3U (Cond.) 15% Glass Reinforced Nylon 6 (North America)
(discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Charpy Impact, Notched |
2.50
J/cm² <br>@Temperature 23.0 °C
|
11.9
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eA |
|
DSM Akulon® K224-TPG3 Impact Modified Nylon 6-15% Glass Reinforced (European Grade) (Dry)
(discontinued **)&l
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Charpy Impact, Notched |
2.50
J/cm² <br>@Temperature 23.0 °C
|
11.9
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eA |
|
DSM Akulon® Ultraflow™ K-FG12 Nylon 6-60% Glass Reinforced (European Grade) (Cond)
(discontinued **)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Charpy Impact, Notched |
2.50
J/cm² <br>@Temperature 23.0 °C
|
11.9
ft-lb/in² <br>@Temperature 73.4 °F
|
Conditioned; ISO 179/1eA |
|
Lanxess Durethan® BKV 130 GIT 900116 Copolyamide, 30% Glass Fiber
CoPA, injection molding grade, 30% glass fibers, elastomer-modified, suitable for GIT (gas assisted technology), good surface finishApplication Examples: Chain-saw handles, office chair armrests, of..
|
|||
| Charpy Impact, Notched |
2.50
J/cm² <br>@Temperature -30.0 °C
|
11.9
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179/1eA |
|
Lanxess Pocan® S 1506 000000 PBT
PBT, non-reinforced, injection molding extrusion, impact modified
|
|||
| Charpy Impact, Notched |
2.50
J/cm² <br>@Temperature -30.0 °C
|
11.9
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179/1eA |
|
Lanxess Pocan® S 1506 901510 PBT
PBT, injection molding grade, non-reinforced, elastomer-modified, high impact strength, even at low temperatures
|
|||
| Charpy Impact, Notched |
2.50
J/cm² <br>@Temperature -30.0 °C
|
11.9
ft-lb/in² <br>@Temperature -22.0 °F
|
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Xenoy® CL402 PBT+PC (Europe-Africa-Middle East)
XENOY CL402 is a high viscosity, unfilled, elastomer modified PC/PBT blend for extrusion/blowmolding applications. ISO1043-label: PC+PBT-I.This data was supplied by SABIC-IP for the Europe-Africa-Mi..
|
|||
| Charpy Impact, Notched |
2.50
J/cm² <br>@Temperature 12.0 °C
|
11.9
ft-lb/in² <br>@Temperature 53.6 °F
|
ISO 179/1eA |
|
Styron CALIBREâ„¢ 303-15 Polycarbonate Resin
Overview: CALIBREâ„¢ 300-115 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity. The CALIBREâ„¢ 300-10 series products are available in 4 ..
|
|||
| Charpy Impact, Notched |
2.50
J/cm² <br>@Temperature 23.0 °C
|
11.9
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eA |
|
Borealis Daplen™ EE168AI Polypropylene TPO Compound
Daplen™ EE168AI is a 10% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process. ..
|
|||
| Charpy Impact, Notched |
2.50
J/cm² <br>@Temperature -30.0 °C
|
11.9
ft-lb/in² <br>@Temperature -22.0 °F
|
cond; ISO 179/1eA |
|
DSM Akulon® Fuel Lock FL-LP PA6
Low fuel permeation PA6 suitable for use in injection molding/welding of small engine fuel tanks, UV stabilized
|
|||
| Charpy Impact, Notched |
2.50
J/cm² <br>@Temperature 23.0 °C
|
11.9
ft-lb/in² <br>@Temperature 73.4 °F
|
cond; ISO 179/1eA |
|
DSM Akulon® K224-G6-FC BK00001 PA6-GF30
30% Glass Reinforced, Food Contact Grade
|
|||
| Charpy Impact, Notched |
2.50
J/cm² <br>@Temperature 23.0 °C
|
11.9
ft-lb/in² <br>@Temperature 73.4 °F
|
cond; ISO 179/1eA |
|
DSM Akulon® K224-LG6 /E PA6-GF30
30% Glass Reinforced, Injection Molding, Improved UV-stability
|
|||
| Charpy Impact, Notched |
2.50
J/cm² <br>@Temperature 23.0 °C
|
11.9
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eA |
|
DSM Akulon® K224-PG6 Impact Modified Nylon 6-30% Glass Reinforced (European and Asian Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Charpy Impact, Notched |
2.50
J/cm² <br>@Temperature 23.0 °C
|
11.9
ft-lb/in² <br>@Temperature 73.4 °F
|
cond; ISO 179/1eA |
|
DSM EcoPaXX® Q-PG6 PA410-I-GF30
% Glass Reinforced, Impact Modified
|
|||
| Charpy Impact, Notched |
2.50
J/cm² <br>@Temperature 23.0 °C
|
11.9
ft-lb/in² <br>@Temperature 73.4 °F
|
cond; ISO 179/1eA |
|
DSM EcoPaXX® Q-X07209 PA410-I-GF40
% Glass Reinforced, Impact Modified
|
|||
| Charpy Impact, Notched |
2.50
J/cm² <br>@Temperature -30.0 °C
|
11.9
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179/eA |
|
Eurotec® Tecomid® NB40 NL IH PA 6 impact modified
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
|
|||
| Charpy Impact, Notched |
2.50
J/cm² <br>@Temperature -30.0 °C
|
11.9
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179/1eA |
|
DSM Arnitel® EL550 55 Shore D, Injection Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
|
|||
| Charpy Impact, Notched |
2.50
J/cm² <br>@Temperature -30.0 °C
|
11.9
ft-lb/in² <br>@Temperature -22.0 °F
|
DIN EN ISO 179 |
|
BASF Elastollan C 98 A TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c..
|
|||
| Charpy Impact, Notched |
2.50
J/cm² <br>@Temperature -30.0 °C
|
11.9
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179/1eA |
|
DSM Akulon® K223-TP4 (Cond.) Impact Modified Nylon 6 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Charpy Impact, Notched |
2.50
J/cm² <br>@Temperature -40.0 °C
|
11.9
ft-lb/in² <br>@Temperature -40.0 °F
|
ISO 179 |
|
Ascend Performance Materials Vydyne® 41 NT Nylon 66, Impact Modified, Conditioned
Vydyne® 41 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im..
|
|||