Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.350 J/cm² @Temperature -20.0 °C |
1.67 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom PLASTALEN® PQ 82 N Polypropylene with improved impact strength PP impact modified. General application in all industry branches. Delivered in natural mode and in the full RAL color scale. For injection molding.Information Provided by Plastcom spol. s r.o. |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature -20.0 °C |
1.67 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVAMID® 6 GF 25 E LS PA6 reinforced with glass fiber, UV stabilized PA 6 grade for extrusion, reinforced with 25% glass fiber, determined for extrusion of window profile systems. Delivered in natural as well as full RAL scale color.Information Provided by Plastcom s.. |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature -20.0 °C |
1.67 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PP CIP6020F Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature -20.0 °C |
1.67 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB SCANMID 6 B60 Nylon 6, Modified Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.350 - 0.500 J/cm² @Temperature 23.0 °C |
1.67 - 2.38 ft-lb/in² @Temperature 73.4 °F |
Injection; ISO 179/ 1eA |
Raschig Group 2567 AMC Glass fiber-reinforced and inorganically filled polyester molding compound (UP) in various colors. Outstanding mechanical strength similar to BMC/SMC, very good electrical isolation properties and .. |
|||
Charpy Impact, Notched | 0.350 - 0.600 J/cm² @Temperature 23.0 °C |
1.67 - 2.86 ft-lb/in² @Temperature 73.4 °F |
Compression; ISO 179/ 1eA |
Raschig Group 5553 DAP Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona.. |
|||
Charpy Impact, Notched | 0.350 - 0.500 J/cm² @Temperature 23.0 °C |
1.67 - 2.38 ft-lb/in² @Temperature 73.4 °F |
Injection; ISO 179/ 1eA |
Raschig Group RALUPOL® 4806 UP Glass-fiber reinforced polyester molding compound. Very low mold shrinkage and post-shrinkage, very good mechanical strength, very good electrical values, better performance values compared to UP 80.. |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature 23.0 °C |
1.67 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
PolyOne Bergamid™ B65 G/Mi20 UF grey LS Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature 23.0 °C |
1.67 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYfill PP HIP8040 VT2 Polypropylene, Mineral Reinforced, Heat Resistant Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature 23.0 °C |
1.67 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYfill PP HIP8040F VT2 Polypropylene, Mineral Reinforced, Heat Resistant Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.350 - 0.500 J/cm² @Temperature 23.0 °C |
1.67 - 2.38 ft-lb/in² @Temperature 73.4 °F |
Injection; ISO 179/ 1eA |
Raschig Group SURAPLAST 54 UPA Glass fiber reinforced polyester molding compound. Minimal mold shrinkage and post-shrinkage, very good arc resistance, very good mechanical strength. This product meets the allowed upper limits for.. |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature 23.0 °C |
1.67 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Minlon® 10B140 BK061 Nylon 66
(Unverified Data**) Minlon® 10B140 BK061 is a 40% mineral reinforced, black polyamide 66 resin for injection molding. It has very low warpage.Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature 23.0 °C |
1.67 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® 151 NC010 Nylon 612
(Unverified Data**) Zytel® 151 NC010 is a PA 612 resin.Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature 23.0 °C |
1.67 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 1-5140 BLH 40% Talc-Filled Polypropylene Homopolymer INNOPOL® CS 1-5140 BLH is a 40% talc-filled polypropylene homopolymer compound /PP-H TD40 (ISO 1043)/.INNOPOL® CS 1-5140 BLH is recommended especially for producing products, where high stiffn.. |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature 23.0 °C |
1.67 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 2-2130 30% Talc Filled Polypropylene Copolymer INNOPOL® CS 2-2130 is a 30 % talc-filled polypropylene compound /PP-B TD30 (ISO 1043)/. This grade is available in natural and custom colored form.INNOPOL® CS 2-2130 is recommended for produci.. |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature 23.0 °C |
1.67 ft-lb/in² @Temperature 73.4 °F |
|
LATI Kelon® B FR H2 CEG/500-V0CT3 PA 6, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Low thermal expansion co.. |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature -20.0 °C |
1.67 ft-lb/in² @Temperature -4.00 °F |
|
LATI Kelon® B FR H2 CEG/500-V0CT3 PA 6, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Low thermal expansion co.. |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature 23.0 °C |
1.67 ft-lb/in² @Temperature 73.4 °F |
|
LATI Lasulf G/15 PSU, 15% Glass Fiber Reinforced Polysulfone (PSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stabilityAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; Nort.. |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature -20.0 °C |
1.67 ft-lb/in² @Temperature -4.00 °F |
|
LATI Lasulf G/15 PSU, 15% Glass Fiber Reinforced Polysulfone (PSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stabilityAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; Nort.. |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature 23.0 °C |
1.67 ft-lb/in² @Temperature 73.4 °F |
|
LATI Latamid 66 B G/20-V PA 66, 20% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. High fluidity. Glass fibers. Flame retardant, non classifiable, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific;.. |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature 23.0 °C |
1.67 ft-lb/in² @Temperature 73.4 °F |
|
LATI Latigray 53/22-01 CX/25 PP Homopolymer, Impact Modified Radiopaque compound based on Polypropylene homopolymer (PPh), impact modified. Special mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformatio.. |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature 23.0 °C |
1.67 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Borealis Borcom™ WG140AI Polypropylene Borcom™ WG140AI is a polypropylene microcomposite intended for injection molding. This material has an excellent balance between impact strength and stiffness, high melt flow rate and gives a good.. |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature -20.0 °C |
1.67 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis Daplen™ KB4436 Polypropylene TPO Compound Daplen™ KB4436 is a 30% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and gi.. |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature 0.000 °C |
1.67 ft-lb/in² @Temperature 32.0 °F |
ISO 179/1eA |
Borealis RA130E-1498 Polypropylene Random Copolymer RA130E-1498 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is white colored. Applications: RA130E-1498 is recommended for the production of PP-R p.. |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature 0.000 °C |
1.67 ft-lb/in² @Temperature 32.0 °F |
ISO 179/1eA |
Borealis RA130E-6034 Polypropylene Random Copolymer RA130E-6034 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is green colored. Applications: domestic water, heating, relining, plumbing, and indust.. |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature 23.0 °C |
1.67 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DuPont Performance Polymers Delrin® FG570 NC000 Acetal Homopolymer Delrin® FG570 NC000 is a medium viscosity acetal homopolymer containing 20% glass fiber for injection molding. It has high stiffness and low warpage. It has been developed for consideration in appl.. |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature -30.0 °C |
1.67 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
BASF Ultraform® N2720 M210 POM Description: Is a POM, product with increased stiffness and strength as well as good wear characteristics, used, for instance, for sliding chains and conveyor systems.Information provided by BASF |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature 23.0 °C |
1.67 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
BASF Ultraform® N2720 M63 30% Mineral Filled POM Description: Is a POM, 30 % mineral-reinforced material for low-warpage moldings with high stiffness, strength and hardness.Information provided by BASF |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature 23.0 °C |
1.67 ft-lb/in² @Temperature 73.4 °F |
|
LATI Laticonther 62 CEG/500-V0HF1 PA 6, Glass/Mineral Reinforced, Flame Retardant High thermal conductivity product based on Polyamide 6 (PA6). Glass fibers / Mineral filler. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Mid.. |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature -30.0 °C |
1.67 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® SC315 NC010 Nylon 612
(Unverified Data**) Zytel® SC315 NC010 is an unreinforced, lubricated 612 polyamide suitable for injection molding. It has been developed for applications such as parts for the healthcare industry.Information provided.. |