| Category | Polymer , Thermoplastic , Nylon , Nylon 612 |
| Manufacturer | |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | DuPont Performance Polymers Zytel® 151 NC010 Nylon 612
(Unverified Data**).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.06 g/cc | 0.0383 lb/in³ | DAM; ISO 1183 |
| Water Absorption | 1.3 % @Temperature 23.0 °C |
1.3 % @Temperature 73.4 °F |
Equilibrium 50%RH; DAM; ISO 62, Similar to |
| 3.0 % @Temperature 23.0 °C |
3.0 % @Temperature 73.4 °F |
Saturation, immersed; DAM; ISO 62, Similar to | |
| Linear Mold Shrinkage | 0.011 cm/cm @Thickness 3.20 mm |
0.011 in/in @Thickness 0.126 in |
Flow; DAM |
| 0.011 cm/cm @Thickness 3.20 mm |
0.011 in/in @Thickness 0.126 in |
Transverse; DAM | |
| Linear Mold Shrinkage, Flow | 0.013 cm/cm @Thickness 2.00 mm |
0.013 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
| Linear Mold Shrinkage, Transverse | 0.014 cm/cm @Thickness 2.00 mm |
0.014 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 114 | 114 | DAM; ISO 2039/2 |
| Tensile Strength, Yield | 54.0 MPa @Temperature 23.0 °C |
7830 psi @Temperature 73.4 °F |
50%RH; ISO 527 |
| 62.0 MPa @Temperature 23.0 °C |
8990 psi @Temperature 73.4 °F |
DAM; ISO 527 | |
| Elongation at Break | 17 % @Temperature 23.0 °C |
17 % @Temperature 73.4 °F |
DAM; nominal; ISO 527 |
| >= 50 % @Temperature 23.0 °C |
>= 50 % @Temperature 73.4 °F |
50%RH; nominal; ISO 527 | |
| Elongation at Yield | 4.5 % @Temperature 23.0 °C |
4.5 % @Temperature 73.4 °F |
DAM; ISO 527 |
| 18 % @Temperature 23.0 °C |
18 % @Temperature 73.4 °F |
50%RH; ISO 527 | |
| Tensile Modulus | 1.70 GPa @Temperature 23.0 °C |
247 ksi @Temperature 73.4 °F |
50%RH; ISO 527 |
| 2.40 GPa @Temperature 23.0 °C |
348 ksi @Temperature 73.4 °F |
DAM; ISO 527 | |
| Flexural Modulus | 1.44 GPa @Temperature 23.0 °C |
209 ksi @Temperature 73.4 °F |
50%RH; ISO 178 |
| 2.10 GPa @Temperature 23.0 °C |
305 ksi @Temperature 73.4 °F |
DAM; ISO 178 | |
| Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 180/1A |
| 4.00 kJ/m² @Temperature 23.0 °C |
1.90 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 180/1A | |
| 4.50 kJ/m² @Temperature -30.0 °C |
2.14 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 180/1A | |
| 4.50 kJ/m² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 180/1A | |
| Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eU |
| NB @Temperature -30.0 °C |
NB @Temperature -22.0 °F |
DAM; ISO 179/1eU | |
| NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
50%RH; ISO 179/1eU | |
| NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
DAM; ISO 179/1eU | |
| Charpy Impact, Notched | 0.300 J/cm² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eA |
| 0.350 J/cm² @Temperature -30.0 °C |
1.67 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eA | |
| 0.350 J/cm² @Temperature 23.0 °C |
1.67 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eA | |
| 0.400 J/cm² @Temperature 23.0 °C |
1.90 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 500 µm/m-°C @Temperature -40.0 - 23.0 °C |
278 µin/in-°F @Temperature -40.0 - 73.4 °F |
DAM; ISO 11359-1/-2 |
| 500 µm/m-°C @Temperature 23.0 - 55.0 °C |
278 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 | |
| 500 µm/m-°C @Temperature 55.0 - 160 °C |
278 µin/in-°F @Temperature 131 - 320 °F |
DAM; ISO 11359-1/-2 | |
| CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
50.0 µin/in-°F @Temperature -40.0 - 73.4 °F |
DAM; ISO 11359-1/-2 |
| 120 µm/m-°C @Temperature 23.0 - 55.0 °C |
66.7 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 | |
| 180 µm/m-°C @Temperature 55.0 - 160 °C |
100 µin/in-°F @Temperature 131 - 320 °F |
DAM; ISO 11359-1/-2 | |
| Melting Point | 218 °C | 424 °F | 10°C/min; DAM; ISO 11357-1/-3 |
| Deflection Temperature at 0.46 MPa (66 psi) | 135 °C | 275 °F | DAM; ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | DAM; ISO 75-1/-2 |
| UL RTI, Electrical | 105 °C @Thickness 0.860 mm |
221 °F @Thickness 0.0339 in |
DAM; UL 746B |
| 105 °C @Thickness 1.50 mm |
221 °F @Thickness 0.0591 in |
DAM; UL 746B | |
| 105 °C @Thickness 3.00 mm |
221 °F @Thickness 0.118 in |
DAM; UL 746B | |
| UL RTI, Mechanical with Impact | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
DAM; UL 746B |
| 65.0 °C @Thickness 0.860 mm |
149 °F @Thickness 0.0339 in |
DAM; UL 746B | |
| 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0591 in |
DAM; UL 746B | |
| UL RTI, Mechanical without Impact | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
DAM; UL 746B |
| 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0591 in |
DAM; UL 746B | |
| 65.0 °C @Thickness 0.860 mm |
149 °F @Thickness 0.0339 in |
DAM; UL 746B | |
| Flammability, UL94 | V-2 @Thickness 0.860 mm |
V-2 @Thickness 0.0339 in |
DAM; IEC 60695-11-10 |
| V-2 @Thickness 1.50 mm |
V-2 @Thickness 0.0591 in |
DAM; IEC 60695-11-10 | |
| V-2 @Thickness 3.00 mm |
V-2 @Thickness 0.118 in |
DAM; IEC 60695-11-10 | |
| V-2 @Thickness 0.860 mm |
V-2 @Thickness 0.0339 in |
DAM; UL94 | |
| V-2 @Thickness 1.50 mm |
V-2 @Thickness 0.0591 in |
DAM; UL94 | |
| V-2 @Thickness 3.00 mm |
V-2 @Thickness 0.118 in |
DAM; UL94 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Comparative Tracking Index | 600 V @Temperature 23.0 °C |
600 V @Temperature 73.4 °F |
DAM; IEC 60112 |
| >= 600 V @Temperature 23.0 °C |
>= 600 V @Temperature 73.4 °F |
DAM; ASTM D3638 | |
| >= 600 V @Temperature 23.0 °C |
>= 600 V @Temperature 73.4 °F |
DAM; UL 746A |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 250 °C | 482 °F | DAM; Optimum |
| 230 - 290 °C | 446 - 554 °F | DAM | |
| Mold Temperature | 70.0 °C | 158 °F | DAM; optimum |
| 50.0 - 90.0 °C | 122 - 194 °F | DAM | |
| Drying Temperature | 80.0 °C | 176 °F | DAM |
| Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | DAM |
| Moisture Content | <= 0.15 % | <= 0.15 % | DAM |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | Natural Color | DAM |
| Drying Recommended | Yes, if moisture content of resin exceeds recommended level | DAM |
| Forms | Pellets | DAM |
| Generic | Nylon 612 | DAM |
| Material Status | Current | DAM |
| Part Marking Code | >PA612< | ISO 11469; DAM |
| Processing Method | Injection Molding | DAM |
| Product Category | Unreinforced Resins | DAM |
| Region Available - Global | Yes | DAM |
| Resin Identification | PA612 | ISO 1043; DAM |
| RoHS Compliance | Contact Manufacturer | DAM |