Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYblend 85FS UV PC/ABS-Blend, UV stabilized Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 5.00 J/cm² @Thickness 102 mm, Temperature 23.0 °C |
23.8 ft-lb/in² @Thickness 4.00 in, Temperature 73.4 °F |
ISO 179 |
Premix Thermoplastics PRE-ELEC® PE 1297 Conductive Thermoplastic Compound PRE-ELEC® PE 1297 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PE.. |
|||
Charpy Impact, Notched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® C8080REC PC+ABS (Europe-Africa-Middle East) PC+ABS, Industrial quality resin with good flow, good temperature resistance and moderate ImpactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact, Notched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CE8510 PC+ABS (Asia Pacific) Extrusion grade PC/ABS. Low viscosity, high impact and ductility.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Charpy Impact, Notched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CP8930 PC+ABS (Europe-Africa-Middle East) High heat, PC/ABS for automotive electro plating applications, excellent balance in flow/impactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact, Notched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CY200FC PC+ABS (Europe-Africa-Middle East) High flow PC+ABS material designed for local Pacific Automotive applicationsThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact, Notched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® 4301 PPC+PC (Europe-Africa-Middle East) Lexan 4301 is a high heat resistant poly (ester) carbonate resin for injection moldingThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact, Notched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL4016 PC Copolymer (Europe-Africa-Middle East) 6% GF reinforced opaque polycarbonate-siloxane copolymer, for increased stiffness with good impact strength. Improved release properties. Available in limited colors only.This data was supplied by S.. |
|||
Charpy Impact, Notched | 5.00 J/cm² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FXD1433T PC Copolymer (Asia Pacific) Clear PC-siloxane copolymer with excellent processability in special light diffusion colors. Medium flow, UV stabilized. Improved toughness compared to standard PC in same color. Color package may .. |
|||
Charpy Impact, Notched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYfill PPC 20000 Polypropylene Copolymer Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® K230-HPV8 Impact Modified Nylon 6 (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 179/1eA |
Lanxess Durethan® B 31 F 000000 Nylon 6, Film Grade PA 6, film grade, low viscosity, easy flow, additive-freeApplication Examples: flat and blown film, monofilaments, coatings |
|||
Charpy Impact, Notched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
cond.; ISO 179-1eA |
Lanxess Durethan® B 35 F 000000 Nylon 6, Extrusion, Low Viscosity PA 6, non-reinforced, extrusion, low viscosity, no additivesInformation provided by LANXESS. |
|||
Charpy Impact, Notched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 179/1eA |
Lanxess Durethan® B 35 FKA 000000 Nylon 6, Film Grade PA 6 Film grade, medium viscosity, nucleated, with processing and slip additives, in compliance with FDA for food contactApplication Examples: flat and blown film, flat film coextrusion for PA/PE co.. |
|||
Charpy Impact, Notched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 179/1eA |
Lanxess Durethan® B 40 E 000000 Nylon 6 PA 6 extrusion grade, standard grade of high viscosity with processing aid/lubricant, not nucleated. |
|||
Charpy Impact, Notched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 179/1eA |
Lanxess Durethan® B 40 FA 000000 Nylon 6, Film Grade PA 6, film grade of high viscosity, lubricated, not nucleated, in compliance with FDA for food contact and acc. the German BgVV Recommendation XLIV, Section VI.A" Synthetic casings in polyamide"Appl.. |
|||
Charpy Impact, Notched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 179/1eA |
Lanxess Durethan® B 40 FAM 000000 Nylon 6, Film Grade PA 6 film grade of high viscosity with high slip agent and lubricant content, not nucleatedApplication Examples: flat and blown film with good surface slip and smoothness - including in the freshly .. |
|||
Charpy Impact, Notched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Lanxess Durethan® DP 2325 H3.0 000000 Nylon 66 PA 66, injection molding grade, non-reinforced, elastomer-modified, good heat-ageing resistance, extremely high notched impact strength even at dry state and at low temperatures |
|||
Charpy Impact, Notched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179/2C |
SABIC Innovative Plastics Xenoy® CL402U PBT+PC (Europe-Africa-Middle East) XENOY CL402U has been specially developed for extrusion blowmoulding applications, where higher melt strength is desired. XENOY CL402U is a high impact material combined with good UV resistance perf.. |
|||
Charpy Impact, Notched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179/2C |
SABIC Innovative Plastics Xenoy® XL1339U PC+PET (Europe-Africa-Middle East) XENOY XL1339U is an unreinforced amorphous PC+PET blend, offering excellent impact performance over a wide temperature range. It combines very good flow characteristics with high heat resistance. XL.. |
|||
Charpy Impact, Notched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xenoy® XL1562 PBT+PC (Europe-Africa-Middle East) XENOY XL1562 is an impact modified PBT+PC blend with outstanding chemical resistance, good UV stability and flow properties.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Charpy Impact, Notched | 5.00 J/cm² @Temperature -40.0 °C |
23.8 ft-lb/in² @Temperature -40.0 °F |
ISO 179 |
Styron PULSEâ„¢ 6000 BG PC/ABS Engineering Resin Overview: PULSE 6000 BG is a PC/ABS resin offering an interesting combination of heat ageing characteristics, low temperature impact performance and high melt strength. Its low MFR enables manufactu.. |
|||
Charpy Impact, Notched | 5.00 J/cm² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Styron PULSEâ„¢ GX50 PC/ABS Engineering Resin Overview: PULSE GX50 engineering resins give exceptional impact strength even at low temperature and have sufficient heat resistance for the majority of automotive interior components. This resin pr.. |
|||
Charpy Impact, Notched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Borealis BA390TF Polypropylene Copolymer BA390TF is a high molecular weight, low melt flow rate polypropylene block copolymer with very high impact strength. Applications: BA390TF is recommended for foam extrusion, or thermoforming.Inform.. |
|||
Charpy Impact, Notched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Unipetrol PP MONSTEN® MA 612 Polypropylene Impact Copolymer Made for injection molding applications. Antistatic stabilization. Impact copolymer.Information provided by Unipetrol RPA |
|||
Charpy Impact, Notched | >= 5.00 J/cm² @Temperature 23.0 °C |
>= 23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Total PPC 7810 Polypropylene, Heterophasic Copolymer, High Impact Polypropylene PPC 7810 is a very high impact heterophasic copolymer with a Melt Flow index of 15 g/10 min.Polypropylene PPC 7810 has been specially developed for high impact and heavy duty applicati.. |
|||
Charpy Impact, Notched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® K240-HP (Dry) Impact Modified Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
DIN EN ISO 179 |
BASF Elastollan 1154 D FHF TPUR Flame Retardant Halogen Free Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.Typical Applications: Cable sheathi.. |
|||
Charpy Impact, Notched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
DIN ISO 179 |
BASF Elastollan R 2000 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Charpy Impact, Notched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Valox® VX3608C PBT (Europe-Africa-Middle East) VALOX VX3608C is an impact modified, flame retardant PBT+PC injection moulding resin. Application: electrical enclosures. This grade is 3607U with reduced oxygen index.This data was supplied by SABI.. |