| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Charpy Impact, Notched |
5.00
J/cm² <br>@Temperature 23.0 °C
|
23.8
ft-lb/in² <br>@Temperature 73.4 °F
|
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Cycoloy® C1200 PC+ABS (Europe-Africa-Middle East)
CYCOLOY C1200 is a PC+ABS blend developed to serve extremely demanding applications in a variety of markets while maintaining good processing properties. The combination of superior heat resistance ..
|
|||
| Charpy Impact, Notched |
5.00
J/cm² <br>@Temperature 23.0 °C
|
23.8
ft-lb/in² <br>@Temperature 73.4 °F
|
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Cycoloy® C1204HF PC+ABS (Asia Pacific)
High heat PC/ABS blend offering good flow and excellent impact. Food compliant according to FDA and European directive 2002/72/EC. Available in limited colors. Effective January 15th, 2008 this gra..
|
|||
| Charpy Impact, Notched |
5.00
J/cm² <br>@Temperature 23.0 °C
|
23.8
ft-lb/in² <br>@Temperature 73.4 °F
|
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Cycoloy® C3650 PC+ABS (Europe-Africa-Middle East)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according ..
|
|||
| Charpy Impact, Notched |
5.00
J/cm² <br>@Temperature 23.0 °C
|
23.8
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179 |
|
Polykemi AB POLYblend 85H PC/ABS-Blend
Information provided by Polykemi AB
|
|||
| Charpy Impact, Notched |
5.00
J/cm² <br>@Temperature 23.0 °C
|
23.8
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179 |
|
Polykemi AB POLYblend 90VB PC/ABS-Blend, Flame Retardant
Information provided by Polykemi AB
|
|||
| Charpy Impact, Notched |
5.00
J/cm² <br>@Temperature 23.0 °C
|
23.8
ft-lb/in² <br>@Temperature 73.4 °F
|
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Cycoloy® CE8510 PC+ABS (Europe-Africa-Middle East)
Extrusion grade PC/ABS. Low viscosity, high impact and ductility.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Charpy Impact, Notched |
5.00
J/cm² <br>@Temperature -30.0 °C
|
23.8
ft-lb/in² <br>@Temperature -22.0 °F
|
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® EXL1463T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1463T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with medium flow ch..
|
|||
| Charpy Impact, Notched |
5.00
J/cm² <br>@Temperature 23.0 °C
|
23.8
ft-lb/in² <br>@Temperature 73.4 °F
|
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® EXL4016 PC Copolymer (Asia Pacific)
6% GF reinforced opaque polycarbonate-siloxane copolymer, for increased stiffness with good impact strength. Improved release properties. Available in limited colors only.This data was supplied by S..
|
|||
| Charpy Impact, Notched |
5.00
J/cm² <br>@Temperature 23.0 °C
|
23.8
ft-lb/in² <br>@Temperature 73.4 °F
|
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Cycoloy® C1100HF PC+ABS (Europe-Africa-Middle East)
CYCOLOY C1100HF is the improved flow version of CYCOLOY C1100 and has been developed to better fill long and complex parts while maintaining still excellent mechanical properties. Its superior flow ..
|
|||
| Charpy Impact, Notched |
5.00
J/cm² <br>@Temperature 23.0 °C
|
23.8
ft-lb/in² <br>@Temperature 73.4 °F
|
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® 4301 PPC+PC
Lexan 4301 is a high heat resistant poly (ester) carbonate resin for injection moldingThis data was supplied by SABIC-IP for the Americas region.
|
|||
| Charpy Impact, Notched |
5.00
J/cm² <br>@Temperature 23.0 °C
|
23.8
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eA |
|
DSM Akulon® K230-HPV8 Impact Modified Nylon 6 (European Grade) (Dry)
(discontinued **)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Charpy Impact, Notched |
5.00
J/cm² <br>@Temperature 23.0 °C
|
23.8
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179 |
|
LG Chemical RS-800 ABS, Extrusion, High Impact, HCFC Resistant
Information Provided by LG Chem
|
|||
| Charpy Impact, Notched |
5.00
J/cm² <br>@Temperature 23.0 °C
|
23.8
ft-lb/in² <br>@Temperature 73.4 °F
|
cond.; ISO 179-1eA |
|
Lanxess Durethan® B 35 F 000000 Nylon 6, Extrusion, Low Viscosity
PA 6, non-reinforced, extrusion, low viscosity, no additivesInformation provided by LANXESS.
|
|||
| Charpy Impact, Notched |
5.00
J/cm² <br>@Temperature 23.0 °C
|
23.8
ft-lb/in² <br>@Temperature 73.4 °F
|
Conditioned; ISO 179/1eA |
|
Lanxess Durethan® B 35 FA 000000 Nylon 6, Film Grade
PA 6, film , medium viscosity, lubricated, not nucleated, in compliance with FDA for food contact and acc. the German BgVV Recommendation XLIV, Section VI.A" Synthetic casings in polyamide"Applicati..
|
|||
| Charpy Impact, Notched |
5.00
J/cm² <br>@Temperature 23.0 °C
|
23.8
ft-lb/in² <br>@Temperature 73.4 °F
|
Conditioned; ISO 179/1eA |
|
Lanxess Durethan® B 38 FKA 000000 Nylon 6, Film Grade
PA 6 film-grade, medium to higher viscosity, with processing aid and slip agent, nucleated, in compliance with FDA for food contactApplication Examples: flat and blown film, flat film coextrusion fo..
|
|||
| Charpy Impact, Notched |
5.00
J/cm² <br>@Temperature 23.0 °C
|
23.8
ft-lb/in² <br>@Temperature 73.4 °F
|
Conditioned; ISO 179/1eA |
|
Lanxess Durethan® B 40 F 000000 Nylon 6, Film Grade
PA 6, Film grade, high viscosity, without additives or processing aids, in compliance with FDA for food contact and acc. the German BgVV Recommendation XLIV, Section VI.A" Synthetic casings in polya..
|
|||
| Charpy Impact, Notched |
5.00
J/cm² <br>@Temperature 23.0 °C
|
23.8
ft-lb/in² <br>@Temperature 73.4 °F
|
Conditioned; ISO 179/1eA |
|
Lanxess Durethan® BC 30 000000 Nylon 6
PA 6, injection molding grade, non-reinforced, rapid processing, higher notched impact strength than B 30 S / B 31 SK in dry and conditioned state, impact-modified
|
|||
| Charpy Impact, Notched |
5.00
J/cm² <br>@Temperature 23.0 °C
|
23.8
ft-lb/in² <br>@Temperature 73.4 °F
|
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Xenoy® CL402 PBT+PC (Asia Pacific)
XENOY CL402 is a high viscosity, unfilled, elastomer modified PC/PBT blend for extrusion/blowmolding applications. ISO1043-label: PC+PBT-I.This data was supplied by SABIC-IP for the Asia Pacific reg..
|
|||
| Charpy Impact, Notched |
5.00
J/cm² <br>@Temperature 23.0 °C
|
23.8
ft-lb/in² <br>@Temperature 73.4 °F
|
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Xenoy® CL402 PBT+PC (Europe-Africa-Middle East)
XENOY CL402 is a high viscosity, unfilled, elastomer modified PC/PBT blend for extrusion/blowmolding applications. ISO1043-label: PC+PBT-I.This data was supplied by SABIC-IP for the Europe-Africa-Mi..
|
|||
| Charpy Impact, Notched |
5.00
J/cm² <br>@Temperature 23.0 °C
|
23.8
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/2C |
|
SABIC Innovative Plastics Xenoy® CL402U PBT+PC (Europe-Africa-Middle East)
XENOY CL402U has been specially developed for extrusion blowmoulding applications, where higher melt strength is desired. XENOY CL402U is a high impact material combined with good UV resistance perf..
|
|||
| Charpy Impact, Notched |
5.00
J/cm² <br>@Temperature -40.0 °C
|
23.8
ft-lb/in² <br>@Temperature -40.0 °F
|
ISO 179 |
|
Styron PULSEâ„¢ 6000 BG PC/ABS Engineering Resin
Overview: PULSE 6000 BG is a PC/ABS resin offering an interesting combination of heat ageing characteristics, low temperature impact performance and high melt strength. Its low MFR enables manufactu..
|
|||
| Charpy Impact, Notched |
5.00
J/cm² <br>@Temperature 23.0 °C
|
23.8
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eA |
|
Borealis BA390TF Polypropylene Copolymer
BA390TF is a high molecular weight, low melt flow rate polypropylene block copolymer with very high impact strength. Applications: BA390TF is recommended for foam extrusion, or thermoforming.Inform..
|
|||
| Charpy Impact, Notched |
5.00
J/cm² <br>@Temperature 23.0 °C
|
23.8
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eA |
|
Borealis Daplen™ ED117AE Polypropylene TPO Compound
Daplen™ ED117AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and gives a good surfac..
|
|||
| Charpy Impact, Notched |
5.00
J/cm² <br>@Temperature 23.0 °C
|
23.8
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179 |
|
Unipetrol PP MONSTEN® MA 612 Polypropylene Impact Copolymer
Made for injection molding applications. Antistatic stabilization. Impact copolymer.Information provided by Unipetrol RPA
|
|||
| Charpy Impact, Notched |
>=
5.00
J/cm² <br>@Temperature 23.0 °C
|
>=
23.8
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179 |
|
Total PPC 3650 Polypropylene, Heterophasic Copolymer, Injection Molding
Polypropylene PPC 3650 is a heterophasic copolymer with a Melt Flow index of 2 g/10 min.Polypropylene PPC 3650 provides an excellent balance between toughness and flow, being particularly suitable i..
|
|||
| Charpy Impact, Notched |
5.00
J/cm² <br>@Temperature 23.0 °C
|
23.8
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eA |
|
DSM Akulon® K240-HP Impact Modified Nylon 6 (European Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Charpy Impact, Notched |
5.00
J/cm² <br>@Thickness 3.00 mm,<br> Temperature 23.0 °C
|
23.8
ft-lb/in² <br>@Thickness 0.118 in,<br> Temperature 73.4 °F
|
partial break; ISO 7391/b.o. ISO 179-1eA |
|
Covestro Makrolon® FS 2000 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Low viscosityAs of 1 S..
|
|||
| Charpy Impact, Notched |
5.00
J/cm² <br>@Temperature 23.0 °C
|
23.8
ft-lb/in² <br>@Temperature 73.4 °F
|
DIN EN ISO 179 |
|
BASF Elastollan 1154 D FHF TPUR Flame Retardant Halogen Free
Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.Typical Applications: Cable sheathi..
|
|||
| Charpy Impact, Notched |
5.00
J/cm² <br>@Temperature 23.0 °C
|
23.8
ft-lb/in² <br>@Temperature 73.4 °F
|
DIN ISO 179 |
|
BASF Elastollan R 2001 20% Glass Filled TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan..
|
|||
| Charpy Impact, Notched |
5.00
J/cm² <br>@Temperature 23.0 °C
|
23.8
ft-lb/in² <br>@Temperature 73.4 °F
|
DIN ISO 179 |
|
BASF Elastollan R 2000 20% Glass Filled TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan..
|
|||