Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 6.41 J/cm | 12.0 ft-lb/in | ASTM D256 |
Nylene® Naxel™ PC10 Polycarbonate Description: Naxel™ PC10 is a 9 melt, general purpose polycarbonate. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources C.. |
|||
Izod Impact, Notched | 6.41 J/cm @Temperature 22.8 °C |
12.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC/ABS-FR1 Flame Retardant PC/ABS Alloy PC/ABS Alloy, Flame Retardant, Standard FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided.. |
|||
Izod Impact, Notched | 6.41 J/cm @Temperature 22.8 °C |
12.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC-FD4-[color]-1 Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig.. |
|||
Izod Impact, Notched | 6.41 J/cm @Temperature 22.8 °C |
12.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC-FR1A-D Polycarbonate, Flame Retardant, Low Flow Polycarbonate, Flame Retardant, Low FlowFeatures: • High Impact Resistance • High Viscosity • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing co.. |
|||
Izod Impact, Notched | 6.41 J/cm @Temperature 22.8 °C |
12.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC-FR2-D-[color]-3 Polycarbonate, Improved Flame Retardant, Medium Flow, UV-stabilized Polycarbonate, Improved Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Izod Impact, Notched | 6.41 J/cm @Temperature 22.8 °C |
12.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC-GP4-[color]-3 Polycarbonate, UV-stabilized, Easy Flow Polycarbonate, UV-stabilized, Easy FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P.. |
|||
Izod Impact, Notched | 6.41 J/cm @Temperature 22.8 °C |
12.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC-GP4-[color]-6 Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samp.. |
|||
Izod Impact, Notched | 6.41 J/cm | 12.0 ft-lb/in | 73°F, 0.125 in; ASTM D256 |
Ravago Manufacturing Americas Hybrid B6720U Polycarbonate + PBT Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Izod Impact, Notched | 6.41 J/cm @Temperature 22.8 °C |
12.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC/ABS-FR1-[color]-UV Flame Retardant PC/ABS Alloy, UV-stabilized PC/ABS Alloy, Flame Retardant, Standard Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Izod Impact, Notched | 6.41 J/cm | 12.0 ft-lb/in | Lengthwise; ASTM D256 |
G-11 Fiberglass Epoxy Laminate Sheet This glass-epoxy laminate is specified for its extremely high strength and high dimensional stability over temperature. G-11 is used for terminal boards, high humidity applications, electrical and e.. |
|||
Izod Impact, Notched | 6.41 J/cm | 12.0 ft-lb/in | ASTM D256 |
Global GPC-105-S Enhanced Modulus, Structural Grade Polycarbonate Information provided by Global Polymers Corporation. |
|||
Izod Impact, Notched | 6.41 J/cm @Thickness 3.17 mm |
12.0 ft-lb/in @Thickness 0.125 in |
|
Mitsubishi Iupilon® H3000R 30 MFI Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 6.41 J/cm @Thickness 3.17 mm |
12.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Lucent Polymers PC/PBT-1212 Polycarbonate+PBT, General Purpose, Injection Grade Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Izod Impact, Notched | 6.41 J/cm @Thickness 3.17 mm |
12.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Lucent Polymers PC/PBT-1230 Polycarbonate+PBT, General Purpose, Injection Grade Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Izod Impact, Notched | 6.41 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
12.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Lucent Polymers PC-1428FD Polycarbonate, FDA Compliant, Injection Grade High FlowAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Izod Impact, Notched | 6.41 J/cm | 12.0 ft-lb/in | 73°F, 0.125 in.; ASTM D256 |
Star Plastics PC1212FRUV Molding Grade PC FR Information provided by Star Plastics, Inc. |
|||
Izod Impact, Notched | 6.41 J/cm | 12.0 ft-lb/in | 73°F, 0.125 in.; ASTM D256 |
Star Plastics PC1510R Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Izod Impact, Notched | 6.41 J/cm | 12.0 ft-lb/in | 73°F, 0.125 in.; ASTM D256 |
Star Plastics PC1510R Molding Grade PC with Release Information provided by Star Plastics, Inc. |
|||
Izod Impact, Notched | 6.41 J/cm | 12.0 ft-lb/in | ASTM Data |
Styron Pulse® 930 ABS + Polycarbonate PULSE® 930 Engineering resin has been designed to provide excellent processability, high heat resistance, and high impact strength at room temperature. PULSE 930 Engineering resin has been used i.. |
|||
Izod Impact, Notched | 6.41 J/cm @Thickness 3.17 mm |
12.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill FR® PC FR UG X GY158 Availability: North AmericaForms: PelletsAdditive: Mold ReleaseFeatures: Flame Retardant and Good Mold ReleaseAppearance: GreyInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 6.41 J/cm | 12.0 ft-lb/in | 73°F, 0.125 in.; ASTM D256 |
Star Plastics PC1212R Molding Grade PC with Release Information provided by Star Plastics, Inc. |
|||
Izod Impact, Notched | 6.41 J/cm | 12.0 ft-lb/in | ASTM Data |
Styron CALIBRE™ IM 401 18 Polycarbonate, Impact Modified CALIBRE® IM401 series resins are impact modified, UL listed polycarbonate resins which contain mold release. CALIBRE IM 401 polycarbonate resins exhibit an excellent balance of impact strength an.. |
|||
Izod Impact, Notched | 6.41 J/cm | 12.0 ft-lb/in | ASTM Data |
Styron Pulse® EXT 100 ABS + Polycarbonate PULSE® EXT 100 Engineering resin has been designed to provide excellent processability, high heat resistance, and high impact strength at both room and low temperatures. PULSE EXT100 Engineering .. |
|||
Izod Impact, Notched | 6.41 J/cm | 12.0 ft-lb/in | ASTM D256 |
Entec Hylex® P1025L1 HB Polycarbonate Available in North America Features: General Purpose Agency Ratings: FDA 21 CFR 177.1580 RoHS Compliant Form: Pellets Information provided by Entec |
|||
Izod Impact, Notched | 6.41 J/cm | 12.0 ft-lb/in | ASTM D256 |
Entec Hylex® P1325L1 HB Polycarbonate UV Stabilized, High Flow, Mold Release, Water ClearInformation provided by Entec. |
|||
Izod Impact, Notched | 6.41 J/cm | 12.0 ft-lb/in | ASTM D256 |
Chase Plastics CP Pryme® PPC100NB-10M Polypropylene Copolymer Information provided by Chase Plastics. |