Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.94 J/cm | 5.51 ft-lb/in | ASTM D-256 |
PlastiComp Complet® LCF40 - PA66 Nylon 66, 40% Long Carbon Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 40% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Izod Impact, Notched | 2.94 J/cm | 5.51 ft-lb/in | ASTM D-256 |
PlastiComp Velocity® LGF50-PA6 High Flow Nylon 6, 50% Long Glass Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |
|||
Izod Impact, Notched | 2.94 J/cm | 5.51 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® MC5303 PC+ABS (Asia Pacific) |
|||
Izod Impact, Notched | 2.94 J/cm @Thickness 3.17 mm |
5.51 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PTS Trilac® ABS-MP1000 Metal Plating Grade ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 2.94 J/cm | 5.51 ft-lb/in | ASTM D-256 |
PlastiComp Complet® LCF40 - TPU Rigid Thermoplastic Polyurethane, 40% Long Carbon Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 40% carbon fiber reinforcementInformation provided by PlastiComp, In.. |
|||
Izod Impact, Notched | 2.94 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
5.51 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical HI121U ABS Feature: Injection Molding, Well Balanced Mechanical Properties, Good weatherabilityApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemic.. |
|||
Izod Impact, Notched | 2.94 J/cm | 5.51 ft-lb/in | ASTM D256 |
Global F-7000 High Density Polyethylene Description-high quality is suitable for blown film @wide range of size & thickness Applications-large & small rolled film, shopping bag, merchant bag, disposal waste bagInformation provided by Glob.. |
|||
Izod Impact, Notched | 2.94 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
5.51 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GN5001SF PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High FlowApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
Izod Impact, Notched | 2.94 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
5.51 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
ASTM D256 |
IRPC Polimaxx Porene SR101 Acrylonitrile Butadiene Styrene Applications:extrusion sheetrefrigerator door liners and inner box linerspicnic coolerssnow boatsluggage cases |
|||
Izod Impact, Notched | 2.94 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
5.51 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GN5009F PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High FlowApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
Izod Impact, Notched | 2.94 J/cm | 5.51 ft-lb/in | |
Shinil Chemical SHINFLAME PC/ABS Flame Retardant Polymer TV Housing SHINFLAME is a flame retardant (FR) compound which exhibits inherent flame retardant properties during fire. Shinil uses its patented dispersion blending technology with variety of polymers to prod.. |
|||
Izod Impact, Notched | 2.94 J/cm @Thickness 3.17 mm |
5.51 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® GC-0703 ABS/PET, Unreinforced Recycled Eco-friendly Post-Consumer recycled PET.Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 2.94 J/cm @Thickness 3.17 mm |
5.51 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® SR-7300 ABS/PET, Unreinforced Material with superior chemical resistance that can be used in the interior/exterior material of household appliances that require heat resistanceInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 2.94 J/cm @Thickness 3.17 mm |
5.51 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® GC-0703 ABS/PET, Unreinforced Recycled Eco-friendly Post-Consumer recycled PET.Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 2.94 J/cm @Thickness 3.17 mm |
5.51 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® SR-7300 ABS/PET, Unreinforced Material with superior chemical resistance that can be used in the interior/exterior material of household appliances that require heat resistanceInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 2.94 J/cm | 5.51 ft-lb/in | ASTM Data |
Styron Magnum™ 2620 ABS, Impact Grade MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Izod Impact, Notched | 2.94 J/cm | 5.51 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL INT2002 PPE+HIPS (Asia Pacific) PPE/HIPS unfilled for auto interior |
|||
Izod Impact, Notched | 2.94 J/cm | 5.51 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-LOY SLDM2005 PC (Asia Pacific) Antistatic Polycarbonate, Non Halogen FR V-2 grade, mineral 5% filled |
|||
Izod Impact, Notched | 2.94 J/cm @Temperature 23.0 °C |
5.51 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl EUN0240 PPE+HIPS (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 2.94 J/cm | 5.51 ft-lb/in | |
Zylog Hipolyene® 1532 MS Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Izod Impact, Notched | 2.94 J/cm | 5.51 ft-lb/in | ASTM D256A |
Dow 560.00 Developmental Performance Polypropylene Polymer OverviewConsistent processabilityExcellent gloss before and after thermoformingUV stabilized for increased weatherabilityD 560.00 Performance Polymer is designed as a co-extrusion cap layer for extr.. |
|||
Izod Impact, Notched | 2.94 J/cm | 5.51 ft-lb/in | ASTM D256A |
Dow 560.01 Developmental Performance Polypropylene Polymer OverviewConsistent processabilityHigh glossGood regrind stabilityContains U.V. stabilizers for increased weatherabilityD 560.01 Performance Polymer is intended for use in extrusion blow molding, she.. |
|||
Izod Impact, Notched | 2.94 J/cm | 5.51 ft-lb/in | ASTM Data |
Dow AIM® 4800 High Impact Styrenic Resin AIM® 4800 advanced styrenic resin is designed to offer the processability of high impact polystyrene and the gloss and practical toughness of high gloss ABS. It can be processed at lower temperatur.. |
|||
Izod Impact, Notched | 2.94 J/cm | 5.51 ft-lb/in | ASTM Data |
Dow AIM® 4810 High Impact Styrenic Resin AIM® 4810 advanced styrenic resin is designed to offer the processability of high impact polystyrene and the gloss and practical toughness of high gloss ABS. It can be processed at lower temperatur.. |
|||
Izod Impact, Notched | 2.94 J/cm | 5.51 ft-lb/in | ASTM D256 |
E-Polymers TEKAMID® H24M10 MF 10% Heat resistance Dimensional stability PA/ABS Alloy Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.H-series: PA6/ABS, PA66/AB.. |
|||
Izod Impact, Notched | 2.94 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
5.51 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
Asahi Kasei Xyron® X0715 Modified Polyphenylene Ether AutomotiveInformation provided by Asahi Kasei |
|||
Izod Impact, Notched | 2.94 J/cm | 5.51 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate CA700 , Unreinforced, 37% Plasticizer
(discontinued **) Amorphous Cellulose Acetate (CA)Characteristics: Chemical Resistance, Toughness, Strength, Hardness, Gloss, Clarity and "Feel"Applications: Tool Handles, Optical Products, Toys and Sheet ProductsPro.. |
|||
Izod Impact, Notched | 2.94 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
5.51 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
ASTM D256 |
IRPC Polimaxx Porene KU900 Acrylonitrile Butadiene Styrene Applications:extrusion sheetrefrigerator door liners and inner box linerspicnic coolerssnow boatsluggage cases |
|||
Izod Impact, Notched | 2.94 J/cm | 5.51 ft-lb/in | ASTM Data |
Styron Magnum™ 9020 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM AB.. |
|||
Izod Impact, Notched | 2.94 J/cm | 5.51 ft-lb/in | ASTM Data |
Styron Magnum™ 9025 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM AB.. |