Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.50 J/cm | 4.68 ft-lb/in | ASTM D256 |
Nylene® 406 Nylon 6, 50% RH Injection molding grade. Nylene 406 is a general purpose, fast cycling molding resin. Crystallization initiators provide fast molding cycles through rapid melt set-up. Parts molded from 406 have bet.. |
|||
Izod Impact, Notched | 2.50 J/cm | 4.68 ft-lb/in | ASTM D256 |
Nylene® 409 Nylon 6, 50% RH Injection molding grade. Nylene 409 is a heat stabilized version of 406 which is a general purpose, fast cycling molding resin. Crystallization initiators provide fast molding cycles through rapid m.. |
|||
Izod Impact, Notched | 2.50 J/cm | 4.68 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycolac® MG37EPX ABS ABS plating grade optimized for a broad processing window for both painted and plated applications. NSF standard 61 compliant (80 sq in/L) |
|||
Izod Impact, Notched | 2.50 J/cm @Temperature -30.0 °C |
4.68 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of properties |
|||
Izod Impact, Notched | 2.50 J/cm | 4.68 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® CM8622 PC+ABS (Europe-Africa-Middle East) CYCOLOY* CM8622 is a high heat PC/ABS blend offering high modulus, low CTE and good |
|||
Izod Impact, Notched | 2.50 J/cm @Temperature -40.0 °C |
4.68 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Covestro Bayblend® 2153 Polycarbonate + ABS Blend, General Purpose
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Izod Impact, Notched | 2.50 J/cm @Temperature -40.0 °C |
4.68 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Covestro Bayblend® 2753 Polycarbonate + ABS Blend, Automotive
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Izod Impact, Notched | 2.50 J/cm @Temperature 23.0 °C |
4.68 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Reliance Industries Repol D120MA Polypropylene REPOL Polypropylene D120MA is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly.. |
|||
Izod Impact, Notched | 2.50 J/cm | 4.68 ft-lb/in | ASTM D256 |
Ineos Nova Styrosun® 6600 Weather Resistant High Impact Styrenic Polymer Features: Outdoor weatherablePhysical property retention after UV exposurePaintable and printableExcellent toughness Can be injection molded or co-extruded Easy to process, no drying required Appli.. |
|||
Izod Impact, Notched | 2.50 J/cm @Thickness 3.17 mm |
4.68 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Hannam Chemical Hanalac 780 ABS, High Flow FDA Approved. High flow grade suitable for intricate or thin structures and low processing cycle time. Applications include TVs, radios, calculators, appliances, toys. |
|||
Izod Impact, Notched | 2.50 J/cm @Temperature -20.0 °C |
4.68 ft-lb/in @Temperature -4.00 °F |
BS 2782.306A |
Micropol Isoplas P651 Crosslinkable Polyethylene Information provided by Micropol Limited |
|||
Izod Impact, Notched | 2.50 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
4.68 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM D256 |
Ineos ABS Triax® 1220 S ABS + Polyamide Blend, Extrusion, Dry as Extruded Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with |
|||
Izod Impact, Notched | 2.50 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
4.68 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM D256 |
Ineos ABS TRIAX® 1220 S ABS/Nylon Blend, Dry as Molded Extrusion and injection molding grade with good stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical dampi.. |
|||
Izod Impact, Notched | 2.50 J/cm @Temperature -20.0 °C |
4.68 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL STN15HF PPE+PS Automotive interiors. Improved flow characteristics/overall processing economy. 240F DTUL. High impact/good property retention after heat ageing. |
|||
Izod Impact, Notched | 2.50 J/cm @Temperature -20.0 °C |
4.68 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL STN15HF PPE+PS (Asia Pacific) Automotive interiors. Improved flow characteristics/overall processing economy. 240F DTUL. High impact/good property retention after heat ageing. |
|||
Izod Impact, Notched | 2.50 J/cm | 4.68 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® IQ4840 PBT+PC Xenoy iQ4840 (PBT+PC) resin is an environmental responsible, sustainable, and low carbon footprint resin. It is a 10% mineral filled resin with high modulus and ductile (HMD) characteristics. Xen.. |
|||
Izod Impact, Notched | 2.50 J/cm | 4.68 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® IQ4840 PBT+PC (Asia Pacific) Xenoy iQ4840 (PBT+PC) resin is an environmental responsible, sustainable, and low carbon footprint resin. It is a 10% mineral filled resin with high modulus and ductile (HMD) characteristics. Xen.. |
|||
Izod Impact, Notched | 2.50 J/cm | 4.68 ft-lb/in | ASTM D256 |
Styrolution Luran® S 778 Q42 Colored ASA Description: Injection molding grade with enhanced toughness and resistance to heat distortion. Especially suitable for exterior automotive components (e.g. radiator grills, rear end appliqué pan.. |
|||
Izod Impact, Notched | 2.50 J/cm | 4.68 ft-lb/in | ASTM D256 |
Styrolution Luran® S 778 UV Colored ASA Description: Injection molding grade with enhanced toughness and resistance to heat distortion. Especially suitable for exterior automotive components (e.g. radiator grills, rear end appliqué pan.. |
|||
Izod Impact, Notched | 2.50 J/cm | 4.68 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PVX0800 PPE NORYL* PVX0800 resin is a high flow, V0 = 1.5 mm grade, suitable for a variety of electronics applications. |
|||
Izod Impact, Notched | 2.50 J/cm | 4.68 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PX1278 PPE+PS Primarily EXTRUSION material. Automotive. Passes FMVSS 302. Heat resistance of 130 C (266 F). |
|||
Izod Impact, Notched | 2.50 J/cm @Temperature -30.0 °C |
4.68 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL EM6100 PPE+PS PPE+PS blend. Unfilled. Good balance of flow/heat/impact. Dimensional stability. Paint adhesion. Suitable for the automotive interior market: HVAC housings, radio components. MS-DB424, WSB-M4D844-A9.. |
|||
Izod Impact, Notched | 2.50 J/cm @Temperature 23.0 °C |
4.68 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram Polytron P50B11 Homopolymer Polypropylene, Chemically Coupled 50% LGF A chemically coupled 50% LGF reinforced black PP, heat stabilized for injection molding applications.Information provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 2.50 J/cm @Temperature 23.0 °C |
4.68 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram Polytron P50N01 Homopolymer Polypropylene, Chemically Coupled 50% Long Glass Fiber A CHEMICALLY COUPLED 50% LONG GLASS FIBER REINFORCED NATURAL POLYPROPYLENE HEAT STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 2.50 J/cm @Temperature 23.0 °C |
4.68 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamShine PV507 ABS, Flame Retardant Flame retardant ABS for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 2.50 J/cm @Temperature 23.0 °C |
4.68 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamTough PZ500 Polycarbonate, Flame Retardant Flame retardant polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 2.50 J/cm | 4.68 ft-lb/in | |
Bapolan® ABS8430 ABS Polymer, Extrusion/Injection Grade Applications: Electronic Instruments, appliances.Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers |
|||
Izod Impact, Notched | 2.50 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
4.68 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
Asahi Kasei Xyron® A0210 PPE/PA AutomotiveInformation provided by Asahi Kasei |
|||
Izod Impact, Notched | 2.50 J/cm | 4.68 ft-lb/in | ASTM D256 |
UBE UBESTA® 3035JX47 Plasticized Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: conductiveInformation provided by UBE. |
|||
Izod Impact, Notched | 2.50 J/cm @Temperature -30.0 °C |
4.68 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS (Asia Pacific) CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of properties |