Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics NORYL PX1278 PPE+PS

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL PX1278 PPE+PS.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Primarily EXTRUSION material. Automotive. Passes FMVSS 302. Heat resistance of 130 C (266 F).
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
Water Absorption 0.060 %

@Time 86400 sec
0.060 %

@Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 121
121
ASTM D785
Tensile Strength, Yield 59.0 MPa
8560 psi
Type I, 50 mm/min; ASTM D638
Elongation at Break 29 %
29 %
Type I, 50 mm/min; ASTM D638
Flexural Yield Strength 93.0 MPa
13500 psi
2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 2.37 GPa
344 ksi
2.6 mm/min, 100 mm span; ASTM D790
Izod Impact, Notched 2.50 J/cm
4.68 ft-lb/in
ASTM D256
1.22 J/cm

@Temperature -30.0 °C
2.29 ft-lb/in

@Temperature -22.0 °F
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 54.0 µm/m-°C

@Temperature -40.0 - 95.0 °C
30.0 µin/in-°F

@Temperature -40.0 - 203 °F
ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi) 140 °C

@Thickness 6.40 mm
284 °F

@Thickness 0.252 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 132 °C

@Thickness 6.40 mm
270 °F

@Thickness 0.252 in
unannealed; ASTM D648
Descriptive Properties Value Comments
Specific Volume 0.93cm^3/g
ASTM D792