Material Notes:
Flame retardant ABS for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
DIN 53479
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
Melt Flow 5.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
5.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 45.0 MPa
6530 psi
ASTM-D638
Elongation at Break 10 %
10 %
ASTM-D638
Tensile Modulus 2.30 GPa
334 ksi
ASTM-D790
Flexural Strength 70.0 MPa
10200 psi
ASTM-D790
Flexural Modulus 2.10 GPa
305 ksi
ASTM-D790
Izod Impact, Notched 2.50 J/cm

@Temperature 23.0 °C
4.68 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C
174 °F
DIN 53461
Vicat Softening Point 86.0 °C
187 °F
ASTM-D1525
Flammability, UL94 V-0