Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.500 J/cm | 0.937 ft-lb/in | ASTM D256 |
Nylene® PA6 Glass/Mineral Filled 7115 HS Nylon 6 15% Glass; 25% Mineral; Dry as molded.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Izod Impact, Notched | 0.500 - 6.99 J/cm | 0.937 - 13.1 ft-lb/in | Average value: 1.28 J/cm Grade Count:25 |
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35.. |
|||
Izod Impact, Notched | 0.500 - 0.600 J/cm | 0.937 - 1.12 ft-lb/in | Average value: 0.567 J/cm Grade Count:3 |
Overview of materials for Polyphthalamide (PPA), Stainless Fiber, EMI This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum va.. |
|||
Izod Impact, Notched | 0.500 J/cm @Temperature -40.0 °C |
0.937 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Shell Carilon® D26FX100 Polyketone, General-Purpose Extrusion Grade
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer D26FX100 is a general-purpose extrusion grade with mechanical properties that classify it as an eng.. |
|||
Izod Impact, Notched | 0.500 J/cm @Temperature -40.0 °C |
0.937 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
BASF Capron® 8200 NL Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Izod Impact, Notched | 0.500 J/cm @Temperature -29.0 °C |
0.937 ft-lb/in @Temperature -20.2 °F |
ASTM D256 |
Global POM-90 General Purpose Acetal Information provided by Global Polymers Corporation. |
|||
Izod Impact, Notched | 0.500 - 0.550 J/cm | 0.937 - 1.03 ft-lb/in | ASTM D256 |
Loxim 230 01V0 Polybutylene Terephthalate Information provided by Loxim Industries |
|||
Izod Impact, Notched | 0.500 J/cm | 0.937 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL V01525 PPE+HIPS (Asia Pacific) Noryl* V01525 is a 15% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Izod Impact, Notched | 0.500 J/cm @Temperature -30.0 °C |
0.937 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL V03550 PPE+HIPS (Europe-Africa-Middle East) Noryl* V03550 is a 35% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Izod Impact, Notched | 0.500 J/cm | 0.937 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM ATX3562R PEI+PCE (Europe-Africa-Middle East) 50% Glass fiber and mineral filled, high flow Polyetherimide blend with internal mold release and enhanced dimensional stability. RoHS compliant. |
|||
Izod Impact, Notched | 0.500 J/cm | 0.937 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® ENH4530 PBT (Europe-Africa-Middle East) 15% GF PBT, Non-Brominated & Non-Chlorinated Flame retardant |
|||
Izod Impact, Notched | 0.500 J/cm @Temperature -30.0 °C |
0.937 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® HX3091HP PBT PBT for compounding/fibers only. Not intended for injection molding. Biocompatible. Melt viscosity at 250C and 21.6kgf is 3500-4500 poise. Available in Natural color (1001) only. |
|||
Izod Impact, Notched | 0.500 - 0.700 J/cm | 0.937 - 1.31 ft-lb/in | ASTM D256 |
Shuman 811 Black Polystyrene Medium Impact Injection molding and extrusion grades, easy processability, good gloss, good surface appearance.Data provided by the manufacturer. |
|||
Izod Impact, Notched | 0.500 J/cm | 0.937 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® IQ325HP PBT (Europe-Africa-Middle East) FDA compliant PBT resin, using chemically recycled post consumer PET Bottles. Fit to food contact applications. |
|||
Izod Impact, Notched | 0.500 J/cm @Temperature -30.0 °C |
0.937 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® SHF4930 PBT (Europe-Africa-Middle East) Super high flow FR PBT grade with 15% Glass reinforced |
|||
Izod Impact, Notched | 0.500 J/cm @Thickness 3.17 mm |
0.937 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Washington Penn PPH2CF2 Polypropylene, 20% Calcium Carbonate Reinforced Homopolymer. FDA for food contact, anti-stat package included.Applications: Toys, appliances, housewares, and automotive components.Data provided by Washington Penn Plastic Co., Inc. |
|||
Izod Impact, Notched | 0.500 J/cm | 0.937 ft-lb/in | ISO 180 |
Wellman Wellamid® MR340 42H-N 34% Mineral Reinforced Nylon 6, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Izod Impact, Notched | 0.500 J/cm | 0.937 ft-lb/in | ISO 180 |
Wellman Wellamid® MRGF25/15 22H-N 25% Mineral/15% Glass Fiber Reinforced Nylon 66, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Izod Impact, Notched | 0.500 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
0.937 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epinyl PA 6 Polyamide 6 Characteristics: medium viscosity, good mechanical properties |
|||
Izod Impact, Notched | 0.500 J/cm | 0.937 ft-lb/in | ASTM D256 |
E-Polymers TEKAMID® TA250FR , Flame Retardant Un-Reinforced PA66, DAM Flame retardantInformation provided by E-Polymers Co. Ltd. |
|||
Izod Impact, Notched | 0.500 J/cm | 0.937 ft-lb/in | ASTM D256 |
E-Polymers TEKAMID® TA250GM , GF/MF Reinforced PA66, DAM GF/MF reinforced, Good surface, Low warpageInformation provided by E-Polymers Co. Ltd. |
|||
Izod Impact, Notched | 0.500 J/cm | 0.937 ft-lb/in | ASTM D256 |
Adell AS-10 Nylon 66, General Purpose Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Notched | 0.500 J/cm | 0.937 ft-lb/in | ASTM D256 |
Adell BH-38 Nylon 6, 40% Mineral Filled Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Notched | 0.500 - 0.700 J/cm @Thickness 6.35 mm |
0.937 - 1.31 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Chang Chun Plastic PBT4815 Fire Retardant & 15% Glass Fiber Enforced Grade PBT Information provided by Dowell Trading Company Ltd. |
|||
Izod Impact, Notched | 0.500 J/cm @Thickness 3.20 mm |
0.937 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Beijing Chemical Industry KAIFA® HN301-G0 PA6 Resin High flame retardant, Good flowInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Izod Impact, Notched | 0.500 J/cm | 0.937 ft-lb/in | ASTM D256 |
Gharda Chemicals GATONE™ 5600PF Polyetheretherketone (PEEK)
(discontinued **) Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric.. |
|||
Izod Impact, Notched | 0.500 J/cm | 0.937 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Ixef® 2530/X9027 Polyarylamide, 55% Mineral + Glass Fiber, at Equilibrium (65% RH)
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Izod Impact, Notched | 0.500 J/cm @Temperature 23.0 °C |
0.937 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamSter PF701 PBT, UV Stabilized UV stabilized high viscosity PBT for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.500 J/cm @Temperature -30.0 °C |
0.937 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® VX4510 PBT (Europe-Africa-Middle East) VALOX VX4510 is a flame retarded, 10% glassfiber reinforced injection moulding PBT resin. |