Shuman 811 Black Polystyrene Medium Impact

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer Shuman
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shuman 811 Black Polystyrene Medium Impact.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Injection molding and extrusion grades, easy processability, good gloss, good surface appearance.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D792
Melt Flow 4.0 - 6.9 g/10 min
4.0 - 6.9 g/10 min
ASTM D1238
7.0 - 9.9 g/10 min
7.0 - 9.9 g/10 min
10 - 12.9 g/10 min
10 - 12.9 g/10 min
13 - 15.9 g/10 min
13 - 15.9 g/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Yield 36.0 MPa
5220 psi
ASTM D638
Izod Impact, Notched 0.500 - 0.700 J/cm
0.937 - 1.31 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 88.0 °C
190 °F
ASTM D648
Vicat Softening Point 99.0 °C
210 °F
ASTM D1525
Processing Properties Metric English Comments
Processing Temperature 204 - 227 °C
399 - 441 °F