Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.210 J/cm | 0.393 ft-lb/in | ASTM D256 |
Plaskolite PL-24 Acrylic Resin For injection molding. An unlubricated version of PL-25 extrusion grade pellets. Highest molecular weight, maximum heat resistance.Information supplied by the manufacturer. |
|||
Izod Impact, Notched | 0.210 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.393 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Maxxam™ PP CS 75 Polypropylene, Unspecified (PP, Unspecified) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Izod Impact, Notched | 0.210 J/cm | 0.393 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycolac® INP576 ABS+SAN Can be used as compounding additives for polymer blends. Medium molecular weight SAN. Can be blended with high rubber graft modifier resins to produce customized ABS properties. Suitable for direc.. |
|||
Izod Impact, Notched | 0.210 - 0.400 J/cm | 0.393 - 0.749 ft-lb/in | ASTM D256-06 |
Proto3000 Objet Digital Materials™ DM_8430 Polypropylene-like Prototyping Polymer Primary material: VeroWhitePlusSecondary material: TangoPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide.. |
|||
Izod Impact, Notched | 0.210 J/cm @Thickness 3.17 mm |
0.393 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PTS SAN-80HF High Flow SAN Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 0.210 J/cm | 0.393 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP KONDUIT OX11314 PPS (Asia Pacific) Thermally conductive mineral filled PPS FR compound |
|||
Izod Impact, Notched | 0.210 - 0.320 J/cm | 0.393 - 0.599 ft-lb/in | Average value: 0.270 J/cm Grade Count:14 |
Overview of materials for Phenolic; Unreinforced; Molded This property data is a summary of similar materials in the MatWeb database for the category "Phenolic; Unreinforced; Molded". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Notched | 0.210 J/cm | 0.393 ft-lb/in | ASTM D256 |
Plenco 309 Black (INJ) Mineral/Fiber Filled Phenolic Molding Compound
(discontinued **) Plaslok 309 is a two-stage, mineral and fiber-filled phenolic molding compound having excellent impact strength; and as such, is considered a good candidate for replacing chopped-fiber filled compou.. |
|||
Izod Impact, Notched | 0.210 - 0.490 J/cm | 0.393 - 0.919 ft-lb/in | Average value: 0.399 J/cm Grade Count:4 |
Overview of materials for Nylon 66, 10% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Mineral Filled". Specific grades with primary filler content between 5% and 14% are includ.. |
|||
Izod Impact, Notched | 0.210 J/cm | 0.393 ft-lb/in | ASTM D256 |
Plaslok 309 Black (INJ) Mineral/Fiber Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 309 is a two-stage, mineral and fiber.. |
|||
Izod Impact, Notched | 0.210 J/cm | 0.393 ft-lb/in | ASTM D256/A |
Iran Petrochemical (PCC) 52528 High Density Polyethylene 52528 is a HDPE copolymer injection molding grade for thin walled applications requiring a good balance between high flowability and physical properties.Application: caps, thin walled, injection mol.. |
|||
Izod Impact, Notched | 0.210 J/cm @Temperature 23.0 °C |
0.393 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Lubricomp RL0049 PA 66 LNP* Lubricomp* RL0049 is a compound based on Nylon 66 resin containing PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Retardant.This data was supplied.. |
|||
Izod Impact, Notched | 0.210 J/cm @Temperature 23.0 °C |
0.393 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Lubricomp RP0049 PA 66 LNP LUBRICOMP* RP0049 is a compound based on Nylon 66 resin containing Flame Retardant, PTFE, Silicone. Added features of this material include: Flame Retardant.This data was supplied by SABIC-IP f.. |
|||
Izod Impact, Notched | 0.210 J/cm @Temperature 23.0 °C |
0.393 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Stat-kon AE0039 ABS (Asia Pacific) LNP* STAT-KON* AE0039 is a compound based on Acrylonitrile Butadiene Styrene resin containing Carbon Fiber, Flame Retardant. Added features of this material include: Electrically Conductive.This da.. |
|||
Izod Impact, Notched | 0.210 J/cm | 0.393 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP MB006S PP LNP THERMOCOMP* MB006S is a compound based on Polypropylene resin containing 30% Glass Bead. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Notched | 0.210 J/cm | 0.393 ft-lb/in | ASTM D256 |
Styrolution Styrolux® 656 C SBC Description: Styrolux® 656 C is a clear styrene-butadiene copolymer (SBC) with enhanced flow properties. It is used almost exclusively for injection molding of rigid, tough parts requiring highes.. |
|||
Izod Impact, Notched | 0.210 J/cm | 0.393 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® 7062HP PBT (Asia Pacific) ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Izod Impact, Notched | 0.210 J/cm | 0.393 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP MB006HS PP LNP* THERMOCOMP* MB006HS is a compound based on Polypropylene resin containing 30% Glass Bead. Added features of this material include: Heat Stabilized, Healthcare. |
|||
Izod Impact, Notched | 0.210 J/cm | 0.393 ft-lb/in | ASTM D256 |
Sumitomo Bakelite Durez® 29502 Phenolic, Compression Grade Durez 29502 Brown Phenolic is a two stage, asbestos free, glass filled, special purpose molding material. It is formulated for close tolerance applications such as transmission valve bodies, and di.. |
|||
Izod Impact, Notched | 0.210 J/cm | 0.393 ft-lb/in | ASTM Data |
Dow Tyril® 990 SAN TYRIL® 990 SAN copolymer grade provides colorless glass-like clarity and excellent overall optical properties. It provides a profile of very good strength with stiffness, chemical resistance, heat .. |
|||
Izod Impact, Notched | 0.210 J/cm @Temperature 23.0 °C |
0.393 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Braskem H 502HC Thermoforming Polypropylene Homopolymer Disposable cupware and dishware; High-stiffness parts; Hot packaging.Information provided by Braskem. |
|||
Izod Impact, Notched | 0.210 J/cm @Temperature -40.0 °C |
0.393 ft-lb/in @Temperature -40.0 °F |
ASTM Test |
BASF Ultramid® 8202CQ PA6 (Conditioned) Ultramid 8202CQ is a low viscosity, PA6 injection molding homopolymer, possessing a modified crystalline structure or increased property performance and faster cycles. It is also available in pigme.. |
|||
Izod Impact, Notched | 0.210 J/cm | 0.393 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 152 Polypropylene, Mineral Reinforced Data provided by the manufacturer, ComAlloy International Company.20% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 0.210 J/cm @Temperature -40.0 °C |
0.393 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Ashley Polymers Ashlene® 831 Nylon 6 General purpose extrusion grade for wire jacketing, tubing, rods, slabs and centrifugal casting. ASHLENE 831 meets FDA requirements and is therefore also suitable for film extrusion and co-extrusio.. |
|||
Izod Impact, Notched | 0.210 - 0.500 J/cm @Temperature -40.0 - -40.0 °C |
0.393 - 0.937 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 0.374 J/cm Grade Count:11 |
Overview of materials for Nylon 6, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v.. |
|||
Izod Impact, Notched | 0.210 J/cm | 0.393 ft-lb/in | 63.5*12.7*3.2mm, Cut; ASTM D256 |
SABIC Innovative Plastics SABIC PPCOMPOUND 15T1020 PP SABIC® PPcompound 15T1020. This grade is a general purpose, talc filled, heat stabilized polypropylene resin suitable for injection molded applications. The IMDS ID is 16486973. |
|||
Izod Impact, Notched | 0.210 - 0.64068 J/cm @Temperature 0.000 - 0.000 °C |
0.393 - 1.2003 ft-lb/in @Temperature 32.0 - 32.0 °F |
Average value: 0.330 J/cm Grade Count:10 |
Overview of materials for Acrylic, Impact Modified, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Izod Impact, Notched | 0.210 J/cm @Diameter 3.17 mm |
0.393 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
BP Amoco Accpro® 9433 Enhanced Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: High stiffness, Surface hardness, Stain resistance, Antistatic, NucleatedComplies with FDA specification, Title 21, CFR 177.1520.Typical app.. |
|||
Izod Impact, Notched | 0.210 - 1.90 J/cm | 0.393 - 3.56 ft-lb/in | Average value: 0.606 J/cm Grade Count:16 |
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and.. |
|||
Izod Impact, Notched | 0.210 J/cm | 0.393 ft-lb/in | ASTM D256 |
Plaslok 308 Black (INJ) Mineral/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 308 is a two-stage, mineral and flock.. |