Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Braskem H 502HC Thermoforming Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Sheet/Thermoforming Grade
Manufacturer Braskem
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem H 502HC Thermoforming Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Disposable cupware and dishware; High-stiffness parts; Hot packaging.Information provided by Braskem.
Physical Properties Metric English Comments
Specific Gravity 0.905 g/cc
0.905 g/cc
ASTM D792
Melt Flow 3.3 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.3 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D785
Tensile Strength, Yield 39.0 MPa
5660 psi
ASTM D638
Elongation at Yield 7.0 %
7.0 %
ASTM D638
Flexural Modulus, 1% Secant 2300 MPa
334000 psi
ASTM D790A
Izod Impact, Notched 0.210 J/cm

@Temperature 23.0 °C
0.393 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 130 °C
266 °F
ASTM D648
Optical Properties Metric English Comments
Haze 46 %

@Thickness 1.00 mm
46 %

@Thickness 0.0394 in
ASTM D1003
Users viewing this material also viewed the following: