Overview of materials for Phenolic; Unreinforced; Molded

Category Polymer , Thermoset , Phenolic , Phenolic; Unreinforced; Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Phenolic; Unreinforced; Molded.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic; Unreinforced; Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.35 - 2.13 g/cc
0.0488 - 0.0770 lb/in³
Average value: 1.49 g/cc Grade Count:15
Apparent Bulk Density 0.600 - 1.01 g/cc
0.0217 - 0.0365 lb/in³
Average value: 0.750 g/cc Grade Count:3
Water Absorption 0.0300 - 0.500 %
0.0300 - 0.500 %
Average value: 0.303 % Grade Count:15
Linear Mold Shrinkage 0.000400 - 0.0140 cm/cm
0.000400 - 0.0140 in/in
Average value: 0.00826 cm/cm Grade Count:15
Mechanical Properties Metric English Comments
Hardness, Rockwell E 86.0 - 91.0
86.0 - 91.0
Average value: 88.3 Grade Count:3
Tensile Strength, Ultimate 41.0 - 57.9 MPa
5950 - 8400 psi
Average value: 53.2 MPa Grade Count:15
Modulus of Elasticity 4.10 - 8.64 GPa
595 - 1250 ksi
Average value: 7.00 GPa Grade Count:5
Flexural Yield Strength 76.0 - 109 MPa
11000 - 15800 psi
Average value: 85.6 MPa Grade Count:15
Flexural Modulus 7.53 - 19.0 GPa
1090 - 2760 ksi
Average value: 11.5 GPa Grade Count:3
Compressive Yield Strength 183 - 226 MPa
26600 - 32800 psi
Average value: 206 MPa Grade Count:15
Izod Impact, Notched 0.210 - 0.320 J/cm
0.393 - 0.599 ft-lb/in
Average value: 0.270 J/cm Grade Count:14
Charpy Impact, Notched 0.190 - 0.390 J/cm²
0.904 - 1.86 ft-lb/in²
Average value: 0.305 J/cm² Grade Count:13
Thermal Properties Metric English Comments
Thermal Conductivity 0.940 - 0.940 W/m-K

@Temperature 100 - 100 °C
6.52 - 6.52 BTU-in/hr-ft²-°F

@Temperature 212 - 212 °F
Average value: 0.940 W/m-K Grade Count:1
Maximum Service Temperature, Air 150 - 219 °C
302 - 426 °F
Average value: 185 °C Grade Count:15
Deflection Temperature at 1.8 MPa (264 psi) 160 - 226 °C
320 - 439 °F
Average value: 176 °C Grade Count:15
Flammability, UL94 HB - V-0
HB - V-0
Grade Count:14
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+11 - 1.00e+13 ohm-cm
1.00e+11 - 1.00e+13 ohm-cm
Average value: 4.26e+12 ohm-cm Grade Count:15
Insulation Resistance 1.00e+8 - 1.00e+11 ohm
1.00e+8 - 1.00e+11 ohm
Average value: 2.78e+10 ohm Grade Count:10
Dielectric Constant 5.00 - 6.50
5.00 - 6.50
Average value: 5.64 Grade Count:5
Dielectric Strength 8.86 - 13.8 kV/mm
225 - 351 kV/in
Average value: 11.3 kV/mm Grade Count:15
Dissipation Factor 0.0190 - 0.0800
0.0190 - 0.0800
Average value: 0.0540 Grade Count:5
Arc Resistance 120 - 190 sec
120 - 190 sec
Average value: 145 sec Grade Count:8
Comparative Tracking Index 100 - 250 V
100 - 250 V
Average value: 160 V Grade Count:13