Proto3000 Objet Digital Materials™ DM_8430 Polypropylene-like Prototyping Polymer

Category Polymer , Rapid Prototyping Polymer
Manufacturer Proto3000
Trade Name Objet Digital Materials™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Proto3000 Objet Digital Materials™ DM_8430 Polypropylene-like Prototyping Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Primary material: VeroWhitePlusSecondary material: TangoPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide the desired mechanical properties and to resemble the product’s target materials.Information provided by Proto3000 for their protoyping engineering services.
Mechanical Properties Metric English Comments
Tensile Strength at Break 29.0 - 38.0 MPa
4210 - 5510 psi
ASTM D638-03
Elongation at Break 25 - 35 %
25 - 35 %
ASTM D638-05
Modulus of Elasticity 1.10 - 1.70 GPa
160 - 247 ksi
ASTM D638-04
Flexural Strength 35.0 - 45.0 MPa
5080 - 6530 psi
ASTM D790-03
Flexural Modulus 1.20 - 1.50 GPa
174 - 218 ksi
ASTM D790-04
Izod Impact, Notched 0.210 - 0.400 J/cm
0.393 - 0.749 ft-lb/in
ASTM D256-06
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 38.0 - 41.0 °C
100 - 106 °F
ASTM D648-06