Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BP Amoco Accpro® 9433 Enhanced Polypropylene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Suggested fabrication methods: Injection moldingFeatures: High stiffness, Surface hardness, Stain resistance, Antistatic, NucleatedComplies with FDA specification, Title 21, CFR 177.1520.Typical applications: Microwavable containersTypical property data below from injection molded samples.
Physical Properties Metric English Comments
Density 0.886 - 0.926 g/cc
0.0320 - 0.0335 lb/in³
ASTM D1505
Water Absorption <= 0.010 %
<= 0.010 %
24 hours; ASTM D570
Linear Mold Shrinkage 0.010 - 0.025 cm/cm
0.010 - 0.025 in/in
ASTM D955
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 109
109
ASTM D785
Tensile Strength, Yield 42.0 MPa
6090 psi
ASTM D638
Elongation at Break 10 %
10 %
ASTM D638
Flexural Modulus 2.41 GPa
350 ksi
ASTM D790A
Izod Impact, Notched 0.210 J/cm

@Diameter 3.17 mm
0.393 ft-lb/in

@Diameter 0.125 in
bar; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 132 °C
270 °F
ASTM D648