Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.92 J/cm | 3.60 ft-lb/in | ASTM D-256 |
PlastiComp Complet® LCF30 - TPU Rigid Thermoplastic Polyurethane, 30% Long Carbon Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 30% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Izod Impact, Notched | 1.92 J/cm | 3.60 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DBL32 PC LNP* Lubricomp* DBL32 is a compound based on Polycarbonate resin containing 10% Glass Beads and 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 1.92 J/cm | 3.60 ft-lb/in | ASTM D256 |
I. Stern 913 High Impact Polystyrene Extrusion Grade Features:Good processing characteristicsExcellent toughness and environmental stress crackingApplicationsThermoformed containers and lids for food packagingCustom extruded sheetInformation provided .. |
|||
Izod Impact, Notched | 1.92 J/cm @Diameter 3.17 mm |
3.60 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
Ineos Nova FX530 Impact Polystyrene Features: Excellent environmental stress crack resistanceExcellent Izod impact strengthUL Classification 94 HBBalanced physical propertiesApplications: ExtrusionThermoformingSelected injection moldi.. |
|||
Izod Impact, Notched | 1.92 J/cm @Temperature -30.0 °C |
3.60 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® 365 PC+PET Unreinforced, opaque, provides chemical resistance and dimensional stability, UL94V-0 rated at 0.031"". |
|||
Izod Impact, Notched | 1.92 J/cm @Temperature -30.0 °C |
3.60 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® 365 PET (Asia Pacific) Unreinforced, opaque, provides chemical resistance and dimensional stability, UL94V-0 rated at 0.031"". |
|||
Izod Impact, Notched | 1.92 J/cm @Thickness 3.17 mm |
3.60 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA4/6 GF50 HS BK 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: BlackUL File Number: E1573.. |
|||
Izod Impact, Notched | 1.92 J/cm @Thickness 3.17 mm |
3.60 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA4/6 GF50 ML2 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Molybdenum Disulfide LubricantFeatures: LubricatedAppearance: BlackUL File Num.. |
|||
Izod Impact, Notched | 1.92 J/cm @Thickness 3.17 mm |
3.60 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 GF30 RM-1 L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: LubricantFeatures: Lubricated and Low Moisture AbsorptionInformation provided .. |
|||
Izod Impact, Notched | 1.92 J/cm | 3.60 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP DF006HL PC (Asia Pacific) LNP* THERMOCOMP* DF006HL is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Low Extractible. |
|||
Izod Impact, Notched | 1.92 J/cm @Thickness 3.17 mm |
3.60 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Plaslube® J-50/20/SI/2 Polycarbonate, 20% GFR, 2% Silicone |
|||
Izod Impact, Notched | 1.92 J/cm @Temperature 23.0 °C |
3.60 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp TH0450D LNP* Thermocomp* TH0450D is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by .. |
|||
Izod Impact, Notched | 1.92 J/cm @Temperature 23.0 °C |
3.60 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp TH0450D PUR (Asia Pacific) LNP* Thermocomp* TH0450D is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by .. |
|||
Izod Impact, Notched | 1.92 J/cm | 3.60 ft-lb/in | ASTM Data |
Styron Magnumâ„¢ PG914 ABS, High Impact MAGNUM ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ABS .. |
|||
Izod Impact, Notched | 1.92 J/cm | 3.60 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOTUF VF008 PA 66 (Asia Pacific) LNP THERMOTUF* VF008 is a compound based on Nylon resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Izod Impact, Notched | 1.92 J/cm | 3.60 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL HIPS3190 HIPS Complies with FDA Regulation 21 CFR 177.1640 for rubber modified polystyrene. HB rating from 0.062-0.125"" pending. Natural only. |
|||
Izod Impact, Notched | 1.92 J/cm | 3.60 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL HNA033 PPE+HIPS Noryl* HNA033 resin is an unfilled modified polyphenylene ether resin designed to withstand several cycles in an autoclave. This resin is suitable for multiple conversion routes and is available in.. |
|||
Izod Impact, Notched | 1.92 J/cm | 3.60 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL HNA033 PPE+HIPS (Asia Pacific) Noryl* HNA033 resin is an unfilled modified polyphenylene ether resin designed to withstand several cycles in an autoclave. This resin is suitable for multiple conversion routes and is available in.. |
|||
Izod Impact, Notched | 1.92 J/cm | 3.60 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL HNA033 PPE+HIPS (Europe-Africa-Middle East) Noryl* HNA033 resin is an unfilled modified polyphenylene ether resin designed to withstand several cycles in an autoclave. This resin is suitable for multiple conversion routes and is available in.. |
|||
Izod Impact, Notched | 1.92 J/cm @Thickness 3.17 mm |
3.60 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Electrablend® PA6/6 03001 Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber ReinforcementAdditive: Impact Modifier and Heat StabilizerFeatures: Electrically Conductive, Impact Modified and Heat Stab.. |
|||
Izod Impact, Notched | 1.92 J/cm | 3.60 ft-lb/in | ASTM D256A |
ExxonMobil PP8255E1 Polypropylene Homopolymer Product Description: A high crystallinity, medium impact copolymer resin designed for compounded and injection molded applications requiring high melt flow rate and excellent processing attributes... |
|||
Izod Impact, Notched | 1.92 J/cm | 3.60 ft-lb/in | Test Method A (0.125 in bar); ASTM D256 |
Diamond Polymers SE 3 HH Description: High Heat ABSInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 1.92 J/cm | 3.60 ft-lb/in | ASTM D256 |
Asahi Kasei Thermylene® P6-40FG-0700 40% Glass Fiber Reinforced, High Impact Information provided by Asahi Thermofil |
|||
Izod Impact, Notched | 1.92 J/cm | 3.60 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 526LD Nylon 66 Modified for toughness at low temperatures, injection molding grade.Data provided by the manufacturer |
|||
Izod Impact, Notched | 1.92 J/cm @Temperature 22.8 °C |
3.60 ft-lb/in @Temperature 73.0 °F |
Method A; ASTM D256 |
Amco PRIMATOP PP CO 350-40 Polypropylene Copolymer PP CO 350-40 features impact resistance and low temperature stiffness. Applications include injection molding and containers.Former A-Top Polymers product; part of Amco product line since 2013. |
|||
Izod Impact, Notched | 1.92 J/cm | 3.60 ft-lb/in | ASTM D-256 |
Axiall 3101 Rigid PVC, Extrusion Georgia Gulf 3101 is a powder blend designed for the extrusion of window, door and fence profiles where weatherability is of primary consideration.Information provided by Georgia GulfGeorgia Gulf be.. |
|||
Izod Impact, Notched | 1.92 J/cm | 3.60 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DBL32 PC (Asia Pacific) LNP* Lubricomp* DBL32 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Izod Impact, Notched | 1.92 J/cm | 3.60 ft-lb/in | @ 73°F; ASTM D256 |
Rochling Engineered Plastics Polystone® PVDF Extruded Sheet Information provided by Röchling Engineered Plastics. |