Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Rochling Engineered Plastics Polystone® PVDF Extruded Sheet

Category Polymer , Thermoplastic , Fluoropolymer , PVDF , Polyvinylidinefluoride (PVDF), Molded/Extruded
Manufacturer Rochling Engineered Plastics
Trade Name Polystone®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Rochling Engineered Plastics Polystone® PVDF Extruded Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Röchling Engineered Plastics.
Physical Properties Metric English Comments
Density 1.78 g/cc
0.0643 lb/in³
ASTM D792
Water Absorption <= 0.10 %
<= 0.10 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Shore D 82
82
ASTM D785
Tensile Strength, Yield 51.7 MPa
7500 psi
ASTM D638
Flexural Modulus 2.00 GPa
290 ksi
ASTM D790
Izod Impact, Notched 1.92 J/cm
3.60 ft-lb/in
@ 73°F; ASTM D256
Thermal Properties Metric English Comments
CTE, linear 90.0 - 126 µm/m-°C

@Temperature 20.0 °C
50.0 - 70.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 127 °C
260 °F
ASTM D648
Users viewing this material also viewed the following: