ExxonMobil PP8255E1 Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Exxon Chemical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil PP8255E1 Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: A high crystallinity, medium impact copolymer resin designed for compounded and injection molded applications requiring high melt flow rate and excellent processing attributes.Availability: North America Features:Balanced Stiffness/ToughnessGood Heat Aging ResistanceGood Impact ResistanceGood ProcessabilityMedium Molecular Weight Nucleated Uses: Appliances Automotive ApplicationsCompoundingProcessing Method: Blow Molding, Compound and Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ExxonMobil Method
Melt Flow 30 g/10 min

@Load 2.16 kg,
Temperature 230 °C
30 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 21.0 MPa
3040 psi
2.0 in/min; ASTM D638
Elongation at Yield 3.9 %
3.9 %
2.0 in/min; ASTM D638
Flexural Modulus, 1% Secant 1190 MPa
173000 psi
0.05 in/min; ASTM D790A
1370 MPa
198000 psi
0.5 in/min; ASTM D790B
Izod Impact, Notched 1.92 J/cm
3.60 ft-lb/in
ASTM D256A
Gardner Impact 27.7 J

@Thickness 3.17 mm,
Temperature -28.9 °C
20.4 ft-lb

@Thickness 0.125 in,
Temperature -20.0 °F
Geometry GC; ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 96.1 °C
205 °F
ASTM D648