Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.300 - 1.50 J/cm² | 1.43 - 7.14 ft-lb/in² | Average value: 0.892 J/cm² Grade Count:90 |
Overview of materials for Acetal Homopolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values .. |
|||
Charpy Impact, Notched | 1.00 - 1.50 J/cm² @Temperature -30.0 - -30.0 °C |
4.76 - 7.14 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 1.33 J/cm² Grade Count:2 |
Overview of materials for Polycarbonate, Gamma Radiation Resistant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Gamma Radiation Resistant". Each property range of values reported is minimum and maximum.. |
|||
Charpy Impact, Notched | 0.350 - 1.50 J/cm² | 1.67 - 7.14 ft-lb/in² | Average value: 0.700 J/cm² Grade Count:16 |
Overview of materials for Polysulfone (PSU) This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Charpy Impact, Notched | 0.600 - 1.50 J/cm² @Temperature -30.0 - 30.0 °C |
2.86 - 7.14 ft-lb/in² @Temperature -22.0 - 86.0 °F |
Average value: 1.27 J/cm² Grade Count:4 |
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an.. |
|||
Charpy Impact, Notched | 0.400 - 1.50 J/cm² @Temperature -30.0 - -20.0 °C |
1.90 - 7.14 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 0.800 J/cm² Grade Count:3 |
Overview of materials for Nylon 6, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a.. |
|||
Charpy Impact, Notched | 0.300 - 1.50 J/cm² @Temperature -40.0 - -20.0 °C |
1.43 - 7.14 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 1.01 J/cm² Grade Count:8 |
Overview of materials for Nylon 66/Nylon 6 Blend, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/Nylon 6 Blend, Glass Fiber Filled". Each property range of values reported is minimum and maxim.. |
|||
Charpy Impact, Notched | 0.350 - 1.50 J/cm² | 1.67 - 7.14 ft-lb/in² | Average value: 1.08 J/cm² Grade Count:19 |
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Charpy Impact, Notched | 0.400 - 1.50 J/cm² | 1.90 - 7.14 ft-lb/in² | Average value: 0.981 J/cm² Grade Count:24 |
Overview of materials for Nylon 66, 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc.. |
|||
Charpy Impact, Notched | 0.200 - 1.50 J/cm² | 0.952 - 7.14 ft-lb/in² | Average value: 0.533 J/cm² Grade Count:11 |
Overview of materials for Nylon 66, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Charpy Impact, Notched | 1.20 - 1.50 J/cm² @Temperature -30.0 - -30.0 °C |
5.71 - 7.14 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 1.38 J/cm² Grade Count:2 |
Overview of materials for Nylon 612, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Impact Modified". Each property range of values reported is minimum and maximum values of app.. |
|||
Charpy Impact, Notched | 0.400 - 1.50 J/cm² | 1.90 - 7.14 ft-lb/in² | Average value: 1.07 J/cm² Grade Count:11 |
Overview of materials for Nylon 46, Flame Retarded + Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Flame Retarded + Glass Fiber Reinforced". Each property range of values reported is minimum an.. |
|||
Charpy Impact, Notched | 0.700 - 1.50 J/cm² | 3.33 - 7.14 ft-lb/in² | Average value: 1.15 J/cm² Grade Count:4 |
Overview of materials for Nylon 46, Lubricated + Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Lubricated + Glass Fiber Reinforced". Each property range of values reported is minimum and ma.. |
|||
Charpy Impact, Notched | 0.500 - 1.50 J/cm² | 2.38 - 7.14 ft-lb/in² | Average value: 0.867 J/cm² Grade Count:6 |
Overview of materials for Nylon 66, Nucleated This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Nucleated". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Charpy Impact, Notched | 0.300 - 1.50 J/cm² | 1.43 - 7.14 ft-lb/in² | Average value: 0.923 J/cm² Grade Count:7 |
Overview of materials for Nylon 66, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu.. |
|||
Charpy Impact, Notched | 0.300 - 1.50 J/cm² | 1.43 - 7.14 ft-lb/in² | Average value: 0.879 J/cm² Grade Count:37 |
Overview of materials for Polyetheretherketone, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum.. |
|||
Charpy Impact, Notched | 0.500 - 1.50 J/cm² @Temperature -30.0 - -30.0 °C |
2.38 - 7.14 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 1.00 J/cm² Grade Count:2 |
Overview of materials for Polycarbonate, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, PTFE Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Charpy Impact, Notched | 0.700 - 1.50 J/cm² | 3.33 - 7.14 ft-lb/in² | Average value: 1.20 J/cm² Grade Count:5 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is .. |
|||
Charpy Impact, Notched | 1.50 - 1.50 J/cm² @Temperature -30.0 - -30.0 °C |
7.14 - 7.14 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 1.50 J/cm² Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is .. |
|||
Charpy Impact, Notched | 0.300 - 1.50 J/cm² @Temperature -30.0 - -30.0 °C |
1.43 - 7.14 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.614 J/cm² Grade Count:84 |
Overview of materials for Polyetherimide (PEI) This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat.. |
|||
Charpy Impact, Notched | 0.250 - 1.50 J/cm² | 1.19 - 7.14 ft-lb/in² | Average value: 0.882 J/cm² Grade Count:11 |
Overview of materials for Polypropylene with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are in.. |