| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.30 - 1.93 g/cc | 0.0470 - 0.0697 lb/in³ | Average value: 1.54 g/cc Grade Count:174 |
| Filler Content | 5.00 - 60.0 % | 5.00 - 60.0 % | Average value: 28.8 % Grade Count:70 |
| Water Absorption | 0.0110 - 0.180 % | 0.0110 - 0.180 % | Average value: 0.103 % Grade Count:85 |
| Water Absorption at Saturation | 0.250 - 0.500 % | 0.250 - 0.500 % | Average value: 0.355 % Grade Count:20 |
| 0.450 - 0.500 % <br>@Temperature 100 - 100 °C |
0.450 - 0.500 % <br>@Temperature 212 - 212 °F |
Average value: 0.459 % Grade Count:11 | |
| Additive Loading | 15.0 - 40.0 % | 15.0 - 40.0 % | Average value: 26.0 % Grade Count:5 |
| Viscosity | 200000 - 700000 cP <br>@Temperature 400 - 420 °C |
200000 - 700000 cP <br>@Temperature 752 - 788 °F |
Average value: 445000 cP Grade Count:13 |
| 350000 - 850000 cP <br>@Temperature 400 - 400 °C |
350000 - 850000 cP <br>@Temperature 752 - 752 °F |
Average value: 445000 cP Grade Count:3 | |
| 350000 - 850000 cP <br>@Shear Rate 1000 - 1000 1/s |
350000 - 850000 cP <br>@Shear Rate 1000 - 1000 1/s |
Average value: 445000 cP Grade Count:3 | |
| Linear Mold Shrinkage | 0.000500 - 0.0150 cm/cm | 0.000500 - 0.0150 in/in | Average value: 0.00421 cm/cm Grade Count:132 |
| Linear Mold Shrinkage, Transverse | 0.00250 - 0.0160 cm/cm | 0.00250 - 0.0160 in/in | Average value: 0.00810 cm/cm Grade Count:28 |
| Melt Flow | 0.700 - 110 g/10 min | 0.700 - 110 g/10 min | Average value: 32.7 g/10 min Grade Count:15 |
| Spiral Flow | 8.50 - 63.0 cm | 3.35 - 24.8 in | Average value: 21.7 cm Grade Count:14 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 85.0 - 108 | 85.0 - 108 | Average value: 103 Grade Count:18 |
| Hardness, Rockwell R | 115 - 126 | 115 - 126 | Average value: 123 Grade Count:9 |
| Hardness, Shore D | 85.0 - 96.0 | 85.0 - 96.0 | Average value: 88.9 Grade Count:22 |
| Tensile Strength, Ultimate | 51.0 - 240 MPa | 7400 - 34800 psi | Average value: 148 MPa Grade Count:161 |
| 25.0 - 215 MPa <br>@Temperature -55.0 - 275 °C |
3630 - 31200 psi <br>@Temperature -67.0 - 527 °F |
Average value: 109 MPa Grade Count:18 | |
| Tensile Strength, Yield | 98.0 - 220 MPa | 14200 - 31900 psi | Average value: 163 MPa Grade Count:15 |
| Elongation at Break | 0.700 - 30.0 % | 0.700 - 30.0 % | Average value: 2.98 % Grade Count:117 |
| 0.700 - 23.0 % <br>@Temperature 60.0 - 150 °C |
0.700 - 23.0 % <br>@Temperature 140 - 302 °F |
Average value: 2.67 % Grade Count:8 | |
| Elongation at Yield | 1.00 - 5.00 % | 1.00 - 5.00 % | Average value: 2.67 % Grade Count:57 |
| 3.00 - 3.50 % <br>@Temperature 90.0 - 150 °C |
3.00 - 3.50 % <br>@Temperature 194 - 302 °F |
Average value: 3.17 % Grade Count:1 | |
| Modulus of Elasticity | 3.86 - 39.7 GPa | 561 - 5760 ksi | Average value: 11.1 GPa Grade Count:156 |
| 5.10 - 37.0 GPa <br>@Temperature 60.0 - 150 °C |
740 - 5370 ksi <br>@Temperature 140 - 302 °F |
Average value: 15.9 GPa Grade Count:8 | |
| Flexural Yield Strength | 67.6 - 360 MPa | 9800 - 52200 psi | Average value: 219 MPa Grade Count:155 |
| 40.0 - 270 MPa <br>@Temperature -55.0 - 275 °C |
5800 - 39200 psi <br>@Temperature -67.0 - 527 °F |
Average value: 128 MPa Grade Count:8 | |
| Flexural Modulus | 3.80 - 24.1 GPa | 551 - 3500 ksi | Average value: 9.61 GPa Grade Count:155 |
| Compressive Yield Strength | 4.14 - 250 MPa | 600 - 36300 psi | Average value: 181 MPa Grade Count:21 |
| 35.0 - 160 MPa <br>@Temperature 120 - 250 °C |
5080 - 23200 psi <br>@Temperature 248 - 482 °F |
Average value: 101 MPa Grade Count:9 | |
| Compressive Modulus | 3.45 - 4.00 GPa | 500 - 580 ksi | Average value: 3.72 GPa Grade Count:6 |
| Shear Strength | 75.8 - 105 MPa | 11000 - 15300 psi | Average value: 92.4 MPa Grade Count:7 |
| Izod Impact, Notched | 0.112 - 2.40 J/cm | 0.210 - 4.50 ft-lb/in | Average value: 0.914 J/cm Grade Count:79 |
| Izod Impact, Unnotched | 3.74 - 13.3 J/cm | 7.00 - 25.0 ft-lb/in | Average value: 7.98 J/cm Grade Count:54 |
| Izod Impact, Notched (ISO) | 0.600 - 13.0 kJ/m² | 0.286 - 6.19 ft-lb/in² | Average value: 8.25 kJ/m² Grade Count:21 |
| Izod Impact, Unnotched (ISO) | 2.50 kJ/m² - NB | 1.19 ft-lb/in² - NB | Average value: 48.0 kJ/m² Grade Count:19 |
| Charpy Impact Unnotched | 1.80 - 8.50 J/cm² | 8.57 - 40.5 ft-lb/in² | Average value: 4.46 J/cm² Grade Count:77 |
| 2.00 - 5.50 J/cm² <br>@Temperature -30.0 - -20.0 °C |
9.52 - 26.2 ft-lb/in² <br>@Temperature -22.0 - -4.00 °F |
Average value: 4.12 J/cm² Grade Count:18 | |
| Charpy Impact, Notched | 0.300 - 1.50 J/cm² | 1.43 - 7.14 ft-lb/in² | Average value: 0.879 J/cm² Grade Count:37 |
| 0.300 - 4.00 J/cm² <br>@Temperature -30.0 - -20.0 °C |
1.43 - 19.0 ft-lb/in² <br>@Temperature -22.0 - -4.00 °F |
Average value: 1.34 J/cm² Grade Count:7 | |
| Coefficient of Friction | 0.240 - 0.450 | 0.240 - 0.450 | Average value: 0.308 Grade Count:30 |
| Coefficient of Friction, Static | 0.250 - 0.350 | 0.250 - 0.350 | Average value: 0.287 Grade Count:24 |
| K (wear) Factor | 6.80 - 353 x 10<sup>-8</sup> mm³/N-M | 3.38 - 175 x 10<sup>-10</sup> in³-min/ft-lb-hr | Average value: 184 x 10<sup>-8</sup> mm³/N-M Grade Count:4 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 13.0 - 55.0 µm/m-°C | 7.22 - 30.6 µin/in-°F | Average value: 26.6 µm/m-°C Grade Count:63 |
| 15.0 - 130 µm/m-°C <br>@Temperature >=143 °C |
8.33 - 72.2 µin/in-°F <br>@Temperature >=289 °F |
Average value: 66.2 µm/m-°C Grade Count:12 | |
| CTE, linear, Transverse to Flow | 36.0 - 110 µm/m-°C | 20.0 - 61.1 µin/in-°F | Average value: 59.8 µm/m-°C Grade Count:3 |
| Specific Heat Capacity | 1.28 - 1.73 J/g-°C <br>@Temperature 50.0 - 200 °C |
0.306 - 0.413 BTU/lb-°F <br>@Temperature 122 - 392 °F |
Average value: 1.50 J/g-°C Grade Count:2 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 10.0 - 3.80e+17 ohm-cm | 10.0 - 3.80e+17 ohm-cm | Average value: 2.29e+16 ohm-cm Grade Count:43 |
| Surface Resistance | 1000 - 1.90e+17 ohm | 1000 - 1.90e+17 ohm | Average value: 1.06e+16 ohm Grade Count:36 |
| Insulation Resistance | 1.00e+12 - 1.00e+16 ohm | 1.00e+12 - 1.00e+16 ohm | Average value: 3.89e+14 ohm Grade Count:52 |
| Static Decay | 2.00 sec | 2.00 sec | Average value: 2.00 sec Grade Count:3 |
| Dielectric Constant | 2.80 - 4.20 | 2.80 - 4.20 | Average value: 3.35 Grade Count:19 |
| Dielectric Strength | 15.0 - 175 kV/mm | 380 - 4450 kV/in | Average value: 26.4 kV/mm Grade Count:26 |
| Dissipation Factor | 0.00100 - 0.0100 | 0.00100 - 0.0100 | Average value: 0.00348 Grade Count:17 |
| Comparative Tracking Index | 150 - 200 V | 150 - 200 V | Average value: 155 V Grade Count:15 |