Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | ISO 179-1/1eA |
Quadrant EPP Duratron® PEI U1000 PEI, unfilled, extruded (ISO Data) Duratron U1000 PEI is an amber translucent (non-optical quality) amorphous thermoplastic material, offering high strength and heat resistance. It performs continuously to 170 °C, making it ideal fo.. |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature 23.0 °C |
1.67 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB SCANMID 6 B11^ FX25 FR10 Nylon 6, Glass Fiber Reinforced, Flame Retardant Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.350 - 1.50 J/cm² | 1.67 - 7.14 ft-lb/in² | Average value: 0.700 J/cm² Grade Count:16 |
Overview of materials for Polysulfone (PSU) This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Charpy Impact, Notched | 0.350 - 1.50 J/cm² | 1.67 - 7.14 ft-lb/in² | Average value: 1.08 J/cm² Grade Count:19 |
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature -20.0 °C |
1.67 ft-lb/in² @Temperature -4.00 °F |
DIN 53453 |
Global PP-2300-LC Polypropylene Block Copolymer Description-opacity, medium to high stiffness, high impact strength at low temperatureApplications-furniture, crates, closures, electrical appliances, automotiveInformation provided by Global Polyme.. |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature -23.0 °C |
1.67 ft-lb/in² @Temperature -9.40 °F |
DIN 53453 |
Global PP-3375-RM Polypropylene Random Copolymer Description-medium stiffness, low melting temperatures, very good for seal Applications-fabricsInformation provided by Global Polymers Corporation. |
|||
Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | |
LATI Larton K/20 PPS, 20% Carbon Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | |
LATI Laticonther 83 CP/80 PA12, Impact Modified High thermal conductivity product based on Polyamide 12 (PA12), impact modified. Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro.. |
|||
Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | ISO 179/1eA |
Borealis Daploy™ WF420HMS High Melt Strength Polypropylene for Extrusion Coating Daploy WF420HMS resin is a propylene-based, structurally isomeric polymer, which combines significantly increased melt strength with largely drawability of the polymer melt. Thus, the material is g.. |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature 23.0 °C |
1.67 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Unipetrol PE HD LITEN® MB/ML 77 HDPE Made for injection molding applications.Information provided by Unipetrol RPA |
|||
Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Delrin® 570 NC000 Acetal (POM)
(Unverified Data**) 20% Glass Filled Medium Viscosity Acetal Homopolymer Delrin 570 NC000 is a medium viscosity acetal homopolymer containing 20% glass fiber filler for injection molding. Delrin 570 has very high stiff.. |
|||
Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® SC315 NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612 Developed for the Healthcare IndustryInformation provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Crastin® SO653 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 20% Glass Bead Filled Polybutylene Terephthalate with Low Warpage CharacteristicsCrastin SO653 NC010 is a 20% glass bead filled polybutylene terephthalate resin for injection molding. It has isotrop.. |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature -40.0 °C |
1.67 ft-lb/in² @Temperature -40.0 °F |
ISO R179 |
Arkema Group ORGASOL® 3502 D Nat 1 Copolyamide 6/12 Information provided by Arkema Group |
|||
Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | ISO 179 |
BASF Ultramid® 8200 HS PA 6 (Dry) Description: Ultramid 8200 HS is a heat stabilized, medium viscosity, PA6 injection molding homopolymer, exhibiting resistance to sink-mark formation in thick sections, and improved toughness over c.. |
|||
Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | ISO 179 |
BASF Ultramid® 8202C PA6 (Dry) Ultramid 8202C is a modified crystalline and low viscosity, nylon 6 injection molding homopolymer. It is also available in heat stabilized (Ultamid 8202C HS) and/or pigmented versions. Its unique .. |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature -30.0 °C |
1.67 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
BASF Ultramid® N-276 NF3001 40% Glass/Mineral Filled PA66 (Dry) Ultramid N-276 NF3001 is a 40% mineral/glass reinforced, heat stabilized injection molding nylon 6/6. |
|||
Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | ASTM D256 |
Chang Chun Plastic Longlite PM T355J Impact Phenolic Molding Compound ASTM Grade per ASTM D700 is 13.Information provided by Dowell Trading Company Ltd. |
|||
Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | ISO 179-1/1eA |
Murtfeldt Murpec® Polyetheretherketone In comparison with other thermoplastics, Murpec® has an exceptionally low thermal expansion coefficient. This property provides optimum dimensional stability and means that dimensions do not change.. |
|||
Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | Conditioned; ISO 179/IeA |
Addiplast Addilene PMD 50291 Flame Retardant Polypropylene Flame retardant, high rigidityInformation provided by Addiplast. |
|||
Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® FG151L NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612 with Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature 23.0 °C |
1.67 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Polyplastic Armlen® PP MF 40-2HS Polypropylene, 40% Mineral Filled Impact modified, injection moldingInformation provided by PolyPlastic Group. |
|||
Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | ISO 179-1/1eA |
Quadrant EPP Duratron® PAI T5530 PAI, 30% glass fibers, compression moulded (ISO Data) This 30 % glass fibre reinforced grade offers higher stiffness, strength and creep resistance than the Duratron PAI grades mentioned above. It is well suited for structural applications supporting s.. |
|||
Charpy Impact, Notched | 0.350 - 0.500 J/cm² | 1.67 - 2.38 ft-lb/in² | Injection; ISO 179/1eA |
Raschig Group 5567 DAP Diallyl Phthalate (DAP), Cast, Mineral Filler Glass-fiber reinforced diallyl phthalate molding compound free from halogens. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exc.. |
|||
Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | ISO 179/1eA |
CENTROPLAST CENTRO HPM Polyetherimide This material has high strength and rigidity at high temperatures, with good electrical properties. Applications include electrical insulators, and load-bearing components.Information provided by C.. |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature 23.0 °C |
1.67 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eA |
Hexion Bakelite™ PF 4260 Phenolic Formaldehyde Resin, Resistant to High Temperatures, Improved Electrical Properties, Low Shrinkage, High Mechanical Strength Phenolic molding compound, inorganically filled, glass fiber reinforced, high dimensional stability at raised temperature, good media resistance, heat-resistantApplication areas: Commutators (starte.. |