Material Notes:
Description-opacity, medium to high stiffness, high impact strength at low temperatureApplications-furniture, crates, closures, electrical appliances, automotiveInformation provided by Global Polymers Corporation.
Physical Properties Metric English Comments
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
L; ASTM D1238
Mechanical Properties Metric English Comments
Ball Indentation Hardness 63.0 MPa
9140 psi
DIN 53456
Tensile Strength, Yield 27.0 MPa
3920 psi
ASTM D638
Shear Modulus 0.580 GPa
84.1 ksi
DIN 53457
Charpy Impact, Notched 0.350 J/cm²

@Temperature -20.0 °C
1.67 ft-lb/in²

@Temperature -4.00 °F
DIN 53453
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 97.8 °C
208 °F
Unannealed; ASTM D648