Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Quadrant EPP Duratron® PEI U1000 PEI, unfilled, extruded (ISO Data)

Category Polymer , Thermoplastic , Polyetherimide (PEI) , Polyetherimide (PEI), Extrusion Grade
Manufacturer Quadrant Engineering Plastics Products
Trade Name Duratron® PEI
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quadrant EPP Duratron® PEI U1000 PEI, unfilled, extruded (ISO Data).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Duratron U1000 PEI is an amber translucent (non-optical quality) amorphous thermoplastic material, offering high strength and heat resistance. It performs continuously to 170 °C, making it ideal for high strength / high heat applications, and also for applications requiring consistent dielectric properties over a wide frequency and temperature range. High maximum allowable service temperature in air (170°C continuously) Very good hydrolysis resistance (suitable for repeated steam sterilization) High strength and stiffness over a wide temperature range Inherent low flammability and low levels of smoke evolution during combustion Good dimensional stability Physiologically inert (suitable for food contact) Very good resistance against high energy radiation (gamma- and X-rays) Very good electrical insulating and dielectric properties
Physical Properties Metric English Comments
Density 1.27 g/cc
0.0459 lb/in³
ISO 1183-1
Moisture Absorption at Equilibrium 0.70 %
0.70 %
50% RH
Water Absorption at Saturation 1.3 %
1.3 %
Outgassing - Total Mass Loss 0.82 %
0.82 %
Mechanical Properties Metric English Comments
Hardness, Rockwell M 115
115
ISO 2039-2
Hardness, Shore D 85
85
Ball Indentation Hardness 165 MPa
23900 psi
ISO 2039-1
Tensile Strength 129 MPa
18700 psi
at Yield; ISO 527-1/-2
Elongation at Break 13 %
13 %
ISO 527-1/-2
Elongation at Yield 7.0 %
7.0 %
ISO 527-1/-2
Tensile Modulus 3.50 GPa
508 ksi
ISO 527-1/-2
Flexural Strength 167 MPa
24200 psi
Compressive Strength 31.0 MPa

@Strain 1 %
4500 psi

@Strain 1 %
ISO 604
61.0 MPa

@Strain 2 %
8850 psi

@Strain 2 %
ISO 604
137 MPa

@Strain 5 %
19900 psi

@Strain 5 %
ISO 604
K Factor (ISO) 1325 µm/km
1325 µm/km
Charpy Impact Unnotched NB
NB
ISO 179-1/1eU
Charpy Impact, Notched 0.350 J/cm²
1.67 ft-lb/in²
ISO 179-1/1eA
Coefficient of Friction, Dynamic 0.30 - 0.40
0.30 - 0.40
Thermal Properties Metric English Comments
CTE, linear 50.0 µm/m-°C

@Temperature 23.0 - 100 °C
27.8 µin/in-°F

@Temperature 73.4 - 212 °F
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 170 °C
338 °F
Continuous
Deflection Temperature at 1.8 MPa (264 psi) 195 °C
383 °F
ISO 75-1/-2
Glass Transition Temp, Tg 215 °C
419 °F
DSC, 20°C/min.; ISO 11357-1/-2
Flammability, UL94 V-0
V-0
Oxygen Index 47 %
47 %
ISO 4589-1/-2
Electrical Properties Metric English Comments
Volume Resistivity >= 1.0e+14 ohm-cm
>= 1.0e+14 ohm-cm
IEC 60093
Surface Resistivity per Square >= 1.0e+13 ohm
>= 1.0e+13 ohm
IEC 60093
Dielectric Constant 3.0

@Frequency >=100000 Hz
3.0

@Frequency >=100000 Hz
IEC 60250
Dielectric Strength 27.0 kV/mm
686 kV/in
Dissipation Factor 0.0020

@Frequency 100000 Hz
0.0020

@Frequency 100000 Hz
IEC 60250
Comparative Tracking Index 175 V
175 V
IEC 60112
Compliance Properties Metric English Comments
3A-Dairy Yes
Yes
Only natural
European Food 1935/2004 No
No
FDA Yes
Yes
only natural
USP Class VI No
No
Chemical Resistance Properties Metric English Comments
Acids, Strong (pH 1-3) Unacceptable
Unacceptable
Acids, Weak Acceptable
Acceptable
Alcohols Acceptable
Acceptable
Alkalies, Strong (pH 11-14) Unacceptable
Unacceptable
Alkalies, Weak Acceptable
Acceptable
Chlorinated Solvents Unacceptable
Unacceptable
Continuous Sunlight Acceptable
Acceptable
Hot Water / Steam Acceptable
Acceptable
Hydrocarbons - Aliphatic Limited
Limited
Hydrocarbons - Aromatic Unacceptable
Unacceptable
Inorganic Salt Solutions Acceptable
Acceptable
Ketones, Esters Unacceptable
Unacceptable
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved