Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CENTROPLAST CENTRO HPM Polyetherimide

Category Polymer , Thermoplastic , Polyetherimide (PEI)
Manufacturer CENTROPLAST Engineering Plastics GMBH
Trade Name CENTRO
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF CENTROPLAST CENTRO HPM Polyetherimide.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
This material has high strength and rigidity at high temperatures, with good electrical properties. Applications include electrical insulators, and load-bearing components.Information provided by CENTROPLAST Engineering Plastics GMBH
Physical Properties Metric English Comments
Density 1.27 g/cc
0.0459 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.75 %
0.75 %
in normal climate 23°C/50%RH; ISO 62
Water Absorption at Saturation 1.35 %
1.35 %
in water at 23°C; ISO 62
Mechanical Properties Metric English Comments
Hardness, Rockwell M 114
<br>@Thickness 10.0 mm
114
<br>@Thickness 0.394 in
ISO 2039-2
Ball Indentation Hardness 170 MPa
24700 psi
value at 30 sec.; ISO 2039-1
Tensile Strength, Yield 105 MPa
15200 psi
v = 50 mm/min; ISO 527-2
Elongation at Break 10 %
10 %
ISO 527-2
Tensile Modulus 3.40 GPa
493 ksi
ISO 527-2
Charpy Impact Unnotched NB
NB
ISO 179/1eU
Charpy Impact, Notched 0.350 J/cm²
1.67 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear 45.0 µm/m-°C
<br>@Temperature 20.0 °C
25.0 µin/in-°F
<br>@Temperature 68.0 °F
ISO 11359
Thermal Conductivity 0.220 W/m-K
1.53 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 170 °C
338 °F
Long Term
300 °C
572 °F
Short term
Deflection Temperature at 1.8 MPa (264 psi) 190 °C
374 °F
ISO 75-2
Flammability, UL94 V-0
<br>@Thickness 3.00 mm
V-0
<br>@Thickness 0.118 in
V-0
<br>@Thickness 6.00 mm
V-0
<br>@Thickness 0.236 in
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
IEC 60093
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IEC 60093
Dielectric Constant 3.0
<br>@Frequency 100 Hz
3.0
<br>@Frequency 100 Hz
IEC 60250
3.0
<br>@Frequency 1e+6 Hz
3.0
<br>@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 27.0 kV/mm
686 kV/in
in transformer oil; IEC 60243-1
Dissipation Factor 0.0020
<br>@Frequency 100 Hz
0.0020
<br>@Frequency 100 Hz
IEC 60250
0.0020
<br>@Frequency 1e+6 Hz
0.0020
<br>@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 175 V
175 V
IEC 60112
Copyright © lookpolymers.com All Rights Reserved