Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.2mm and 5VB at 1... |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics EXTEM UH1016 TPI Blend (Europe-Africa-Middle East) High heat amorphous TPI Blend, Chemical Resistant, High Flow |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179/1eA |
Nilit FRIANYL A63 HS-GV40 Nylon 6.6 for injection molding, 40% glass fiber reinforced Nylon 6.6 for injection molding, high impact resistance.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179/1eU |
Lucite International Diakon® TD510 Toughened Acrylic Compound The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by.. |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO Data |
Styron Magnumâ„¢ FG960 ABS, High Impact MAGNUM ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ABS .. |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO Data |
Styron Magnumâ„¢ PG914 ABS, High Impact MAGNUM ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ABS .. |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO Data, Low Temp |
Styron Pulse® 930 ABS + Polycarbonate PULSE® 930 Engineering resin has been designed to provide excellent processability, high heat resistance, and high impact strength at room temperature. PULSE 930 Engineering resin has been used i.. |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL GTX GTX989 PPE+PA NORYL GTX989 is a conductive and high heat material, especially designed for in- and on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity.. |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL GTX GTX989 PPE+PA (Asia Pacific) NORYL GTX989 is a conductive and high heat material, especially designed for in- and on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity.. |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics LNP VERTON RX10409D PA 66 LNP* VERTON* RX10409D is a compound based on Nylon 66 containing proprietary fillers. Added feature of this grade is: Structural. |
|||
Charpy Impact, Notched | 2.20 - 2.80 J/cm² | 10.5 - 13.3 ft-lb/in² | DIN 53453 |
Zell-Metall Engineering Plastics Zellamid 1100 MO Improved sliding and self lubricating properties are achieved by the addition of molybdenum disulphide. UV-radiation resistance is enhanced.Color: blackApplications: For conveyor screws |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® 1SVX-65H nat PA1010-GF65 Product Description: Grilamid 1SVX-65H natural is a 65% glass fiber reinforced Polyamide 1010 injection molding grade with the following product profile: Raw materials based on renewable resources E.. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6000/58 GV 15 HWUVCP 15% Glass Fiber Nylon 6, Impact Modified Until -40°C, UV Stabilized, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | 50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® 80G33L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Toughened Polyamide 66 Zytel 80G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Inf.. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature -20.0 °C |
10.5 ft-lb/in² @Temperature -4.00 °F |
After conditioning at 23°C/50%RH; ISO 179/Af |
Arkema Group Orgalloy® LE 60 ES Polyamide Alloy Polyamide Alloy, Blow Molding of Technical PartsInformation provided by Arkema Group |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature -20.0 °C |
10.5 ft-lb/in² @Temperature -4.00 °F |
After conditioning at 23°C/50%RH; ISO 179/Af |
Arkema Group Orgalloy® LE 6000 Polyamide 6 Alloy Polyamide Alloy, Semi-Flexible grade, Nylon 6 basedTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature -20.0 °C |
10.5 ft-lb/in² @Temperature -4.00 °F |
After conditioning at 23°C/50%RH; ISO 179/Af |
Arkema Group Orgalloy® LE60 THM Polyamide Alloy Polyamide Alloy, Semi-Flexible gradeTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature -30.0 °C |
10.5 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Orgalloy® LT 4060 Flexible Nylon Alloy (Conditioned) Very flexible polyamide alloy: easy to process, low moisture absorption, good mechanical properties at low temperature. Demonstrates a good balance of properties eg, high flexibility (200 MPa), good.. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Akro-Plastic Akromid® A3 GF 60 (2424) PA 6.6 Conditioned, 60% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature -30.0 °C |
10.5 ft-lb/in² @Temperature -22.0 °F |
|
BASF Luranyl® KR 2404 Polyphenylene Ether + Styrene-Butadiene Blend Base grade with high heat deformation resistance and a balanced combination of stiffness and toughness. Uses include: steering-wheel covers and heater controls.Data was collected by ISO methods and.. |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179 |
BASF Ultramid® TG7S BK-102 35% Glass Filled PA6 (Dry) Ultramid TG7S is a 34% glass reinforced, heat stabilized, impact modified nylon 6 injection molding grade. It was developed to meet the demanding requirements of the first North American seat cushi.. |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179/1eA |
BASF Ultramid® A3EG6 30% Glass Filled PA66 (Conditioned) Ultramid A3EG6 is a 30% glass fiber reinforced injection molding PA66 grade for machinery components and housings of high stiffness and dimensional stability. |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179/1eA |
BASF Ultramid® A3EG7 35% Glass Filled PA66 (Conditioned) Ultramid A3EG6 is a 35% glass fiber reinforced injection molding PA66 grade for machinery components and housings of high stiffness and dimensional stability. |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179 |
Chi Mei Polylac® PA-763A ABS - Flame Retardant F.R. High Heat |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycolac® DL100LG ABS (Europe-Africa-Middle East) Cycolac DL100LG is a low gloss, high heat, high impact ABS/PC blend with low emission |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL FE8000S PPE+PS Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom.. |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL FE8000S PPE+PS (Asia Pacific) Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom.. |