Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Zell-Metall Engineering Plastics Zellamid 1100 MO

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, MoS2 Filled
Manufacturer Zell-Metall Engineering Plastics
Trade Name Zellamid
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zell-Metall Engineering Plastics Zellamid 1100 MO.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Improved sliding and self lubricating properties are achieved by the addition of molybdenum disulphide. UV-radiation resistance is enhanced.Color: blackApplications: For conveyor screws
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
Moisture Absorption at Equilibrium 2.5 - 3.0 %
2.5 - 3.0 %
Saturation at 50% RH
Water Absorption at Saturation 6.0 - 7.0 %
6.0 - 7.0 %
23°C
Mechanical Properties Metric English Comments
Hardness, Shore D 83 - 85
83 - 85
DIN 53505
Ball Indentation Hardness 165 MPa
23900 psi
DIN 53456
Tensile Strength at Break 90.0 - 92.0 MPa
13100 - 13300 psi
DIN 53455
Elongation at Break 10 - 30 %
10 - 30 %
DIN 53455
Tensile Modulus 4.10 GPa
595 ksi
DIN 53457
0.900 GPa

@Temperature 100 °C
131 ksi

@Temperature 212 °F
DIN 53457
Charpy Impact Unnotched NB
NB
DIN 53453
Charpy Impact, Notched 2.20 - 2.80 J/cm²
10.5 - 13.3 ft-lb/in²
DIN 53453
Coefficient of Friction 0.050 - 0.10
0.050 - 0.10
to steel, added lubrication
0.30 - 0.35
0.30 - 0.35
to steel, no lubrication; ISO/DTR 7147
Abrasion 91
91
mm³; DIN 53516
Thermal Properties Metric English Comments
CTE, linear 80.0 µm/m-°C

@Temperature 20.0 °C
44.4 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 1.67 J/g-°C
0.399 BTU/lb-°F
Thermal Conductivity 0.280 W/m-K
1.94 BTU-in/hr-ft²-°F
DIN 52612
Melting Point 220 °C
428 °F
Maximum Service Temperature, Air 100 - 120 °C
212 - 248 °F
long time operation
120 - 140 °C
248 - 284 °F
medium time operation
160 °C
320 °F
a few hours operation
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Flammability, UL94 HB
HB
Descriptive Properties Value Comments
Time yield limit up to 5
s1/1000; DIN.53444
Users viewing this material also viewed the following: