Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.350 J/cm² @Temperature -30.0 °C |
1.67 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Nilit Nilamon B3 H7 GK 35 15% Glass Fiber, 25% Mineral Reinforced PA6 Description: Nilamon B3 H7 GK 35 provides a combination between low warpage and high stiffness, while retaining a good impact strength. It has a high heat aging resistance, so that it is suitable fo.. |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature -30.0 °C |
1.67 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Nilit FRIANYL A63 HH-FK 1020 Nylon 6.6 for injection molding, 10% glass fiber and 20% glass ball reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | ISO 179-1/1eA |
Quadrant EPP Ketron® 1000 PEEK unfilled, extruded (ISO Data) Ketron PEEK-1000 stock shapes are produced from virgin polyetheretherketone resin and offer the highest toughness and impact strength of all Ketron PEEK grades. Both Ketron PEEK-1000 natural & black.. |
|||
Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | ISO 179-1/1eA |
Quadrant EPP Nylatron® NSM PA 6 + internal lubricant, cast (ISO Data) Nylatron NSM is a proprietary cast nylon 6 formulation containing solid lubricant additives which grant this materials self-lubricity, excellent frictional behaviour, superior wear resistance and ou.. |
|||
Charpy Impact, Notched | 0.350 - 0.450 J/cm² @Temperature 23.0 °C |
1.67 - 2.14 ft-lb/in² @Temperature 73.4 °F |
Injection; ISO 179/ 1eA |
Raschig Group 5562 DAP Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona.. |
|||
Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | ISO 179/1eA |
Nilit FRIANYL A63 AL40 Nylon 6.6 for injection molding, 40% aluminum filled Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.350 - 4.50 J/cm² @Temperature -40.0 - 30.0 °C |
1.67 - 21.4 ft-lb/in² @Temperature -40.0 - 86.0 °F |
Average value: 1.39 J/cm² Grade Count:39 |
Overview of materials for Nylon 66, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. .. |
|||
Charpy Impact, Notched | 0.350 - 1.90 J/cm² @Temperature -40.0 - -30.0 °C |
1.67 - 9.04 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 0.784 J/cm² Grade Count:15 |
Overview of materials for Nylon 612, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Unreinforced". Each property range of values reported is minimum and maximum values of approp.. |
|||
Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | ISO 179/1eA |
Lucite International Diakon® ST25G7 Toughened Acrylic Compound The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by.. |
|||
Charpy Impact, Notched | 0.350 - 0.550 J/cm² | 1.67 - 2.62 ft-lb/in² | ISO 179 |
Vyncolit G885 Novolac Phenolic Glass fiber and mineral filled phenolic molding compound with excellent mechanical and thermal properties. Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | ISO 179 |
Vyncolit X6151 Novolac Phenolic Glass fiber and mineral filled phenolic molding compound with excellent mechanical and thermal properties. Highest impact, high strain to failure, glycol resistant.USES: Water pumps and water pump .. |
|||
Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | ISO 179 |
Vyncolit X680 Novolac Phenolic Glass fiber and glass bead filled phenolic molding compound with excellent mechanical and thermal properties. Easily transformed into complex shapes. UL listed.USES: Complex precision parts with t.. |
|||
Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | ISO 179-1 |
Vyncolit BXE7665 Glass Filled Phenolic Molding Compound Novolac resin based, mainly glass fiber filled. Excellent electrical properties combined with very good mechanical properties. Grade especially suitable for electrical applications.Information pro.. |
|||
Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | ISO 179 |
Vyncolit G865 Novolac Phenolic Glass fiber filled phenolic molding compound with high mechanical, good thermal and electrical properties. USES: Asbestos-free replacement for die-cast automotive metal parts, e.g. reactors for aut.. |
|||
Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Crastin® CE2055 BK580 Polybutylene Terephthalate (PBT) Unreinforced Low Viscosity Polybutylene Terephthalate Crastin CE2055 is an unreinforced low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performanc.. |
|||
Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Crastin® SO653 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 20% Glass Bead Filled Polybutylene Terephthalate with Low Warpage CharacteristicsCrastin SO653 NC010 is a 20% glass bead filled polybutylene terephthalate resin for injection molding. It has isotrop.. |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature -30.0 °C |
1.67 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DuPont Performance Polymers Crastin® SO653 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 20% Glass Bead Filled Polybutylene Terephthalate with Low Warpage CharacteristicsCrastin SO653 NC010 is a 20% glass bead filled polybutylene terephthalate resin for injection molding. It has isotrop.. |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature -30.0 °C |
1.67 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® 151 NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature -30.0 °C |
1.67 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® BMN Y BZ TL Nylon 11, Bronze Bead Filled (Dry) Designation ISO 1874-PA11,MHLS,16-020,(Z+M)(B+D)(80BZ+05)Rigid grade with bronze beads (85%) and molybdenum fillers for injection molding. Available color: steel brown. Light and heat stabilized.No .. |
|||
Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | ISO 179/IeA |
Addiplast Addilene H 410 Polypropylene Homopolymer UnreinforcedInformation provided by Addiplast. |
|||
Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® FG151L NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612 with Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature 23.0 °C |
1.67 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Borealis HF136MO Polypropylene HF136MO is a polypropylene homopolymer intended for injection molding. This grade is characterized by a good combination of mechanical and flow properties. This polymer is a CR (controlled rheology.. |
|||
Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | ISO 179/1eA |
Lucite International Elvakon® 4451 Super Low Gloss Acrylic Capstock Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable prot.. |
|||
Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | ISO 179 |
Sumitomo Bakelite North America RX® 790 Fiberglass Reinforced Phenolic Novolac RX 790 is a fiberglass reinforced phenolic novolac compound, featuring a good balance of strength and toughness. Information supplied by Sumitomo Bak North America. |
|||
Charpy Impact, Notched | 0.350 - 0.750 J/cm² @Temperature -30.0 - -20.0 °C |
1.67 - 3.57 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 0.550 J/cm² Grade Count:2 |
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc.. |