Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Vyncolit X6151 Novolac Phenolic

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Mineral/Glass Filled
Manufacturer Vyncolit N.V., Sumitomo Bakelite
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Vyncolit X6151 Novolac Phenolic.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Glass fiber and mineral filled phenolic molding compound with excellent mechanical and thermal properties. Highest impact, high strain to failure, glycol resistant.USES: Water pumps and water pump impellers without metal insert bushes. Intake manifolds.Information provided by Vyncolit, a Sumitomo Bak Group
Physical Properties Metric English Comments
Bulk Density 0.600 g/cc
0.0217 lb/in³
Powder Density; ISO 60
Density 1.55 g/cc
0.0560 lb/in³
Relative Density; ISO 1183
Linear Mold Shrinkage 0.0035 cm/cm
0.0035 in/in
Injection Molding; ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break 70.0 MPa
10200 psi
ISO 527
Elongation at Break 0.90 %
0.90 %
Tensile; ISO 527
1.65 %
1.65 %
Flexure; ISO 178
Tensile Modulus 11.0 GPa
1600 ksi
ISO 527
Flexural Strength 160 MPa
23200 psi
At Rupture; ISO 178
Flexural Modulus 10.0 GPa
1450 ksi
ISO 178
Compressive Strength 220 MPa
31900 psi
ISO 604
Charpy Impact Unnotched 1.20 J/cm²
5.71 ft-lb/in²
ISO 179
Charpy Impact, Notched 0.350 J/cm²
1.67 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature 20.0 °C
13.9 µin/in-°F

@Temperature 68.0 °F
TMA
CTE, linear, Transverse to Flow 45.0 µm/m-°C

@Temperature 20.0 °C
25.0 µin/in-°F

@Temperature 68.0 °F
TMA
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
ISO 75 Af
Flammability, UL94 V-1

@Thickness 1.60 mm
V-1

@Thickness 0.0630 in
V-0

@Thickness 4.00 mm
V-0

@Thickness 0.157 in
Shrinkage 0.10 %
0.10 %
Post Shrinkage; ISO 2577
Electrical Properties Metric English Comments
Dielectric Strength 30.0 kV/mm
762 kV/in
IEC 243
Comparative Tracking Index 175 V
175 V
IEC 112
Descriptive Properties Value Comments
Color Black
ISO type PF 2 C3
Main Filler Glass Fiber & Mineral
Molding Method Compression, transfer, injection
Users viewing this material also viewed the following: