Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lucite International Elvakon® 4451 Super Low Gloss Acrylic Capstock

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic, Extruded
Manufacturer Lucite International
Trade Name Elvakon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucite International Elvakon® 4451 Super Low Gloss Acrylic Capstock.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable protective coating.Information provided by Lucite International
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
Water Absorption 0.40 %
0.40 %
ISO 62
Melt Flow 3.0 g/10 min
3.0 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell M 90
90
ISO 2039-2
Tensile Strength 37.0 MPa
5370 psi
ISO 527
Elongation at Break 10 %
10 %
ISO 527
Flexural Strength 51.0 MPa
7400 psi
ISO 178
Flexural Modulus 2.50 GPa
363 ksi
ISO 178
Izod Impact, Notched (ISO) 3.30 kJ/m²
1.57 ft-lb/in²
ISO 180/1A
Charpy Impact Unnotched 3.30 J/cm²
15.7 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.350 J/cm²
1.67 ft-lb/in²
ISO 179/1eA
Impact Test 1.20 J
0.885 ft-lb
Instrumented Falling Weight Impact; ISO 6603/2
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 82.0 °C
180 °F
ISO 75B
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C
160 °F
ISO 75A
Vicat Softening Point 76.0 °C
169 °F
ISO 306B
89.0 °C
192 °F
ISO 306A