Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
Nilit FRIANYL B63 W-GV35 Nylon 6 for injection molding, 35% glass fiber reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Strength | >= 250 MPa | >= 36300 psi | 10 mm/min; DIN 53452 |
Qualchem Danamid AFCF-30 Polyamide 66, 30% Carbon Fiber Reinforced with carbon fiber, antistatic and conductive.Information provided by Qualchem Zrt. |
|||
Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
Nilit FRIANYL B63 GV35 Nylon 6 for injection molding, 35% glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
Nilit FRIANYL C73 GV40 Nylon 6.6/6 for injection molding, 40% glass fiber reinforced Nylon 6.6/6 for injection molding, medium viscosity.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Strength | 250 MPa | 36300 psi | |
Lehmann & Voss LUVOCOM® 1105-7920/RD PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Flexural Strength | 250 MPa | 36300 psi | |
Lehmann & Voss LUVOCOM® 1105-8169 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista.. |
|||
Flexural Strength | 250 MPa @Temperature 22.0 °C |
36300 psi @Temperature 71.6 °F |
25 mm wide 100 mm long, flat samples; ISO 14125 |
Menzolit Menzolit® SMC 1400 Unsaturated Polyester UP SMC 1400 is a special SMC being used in the environment of a combustion engine. The glass level has been selected to combine good mouldability with good stiffness and strength properties. The produc.. |
|||
Flexural Strength | 250 MPa | 36300 psi | |
Lehmann & Voss LUVOCOM® 1105-0706 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch.. |
|||
Flexural Strength | 250 MPa | 36300 psi | |
Lehmann & Voss LUVOCOM® 1105-0858 PEEK, with glass fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High dimensionally stable precision parts, high continuous use tempera.. |
|||
Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
Solvay TECHNYL® A 218HP V35 PA66, 35% glass fiber, DRY Description: TECHNYL® A 218HP V35 is a polyamide 6.6, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits: The product of.. |
|||
Flexural Strength | 250 MPa | 36300 psi | ASTM D790 |
Solvay Specialty Polymers AvaSpire® AV-755 SL45 Polyaryletherketone (PAEK) AV-755 SL45 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates and high pressure-velocity (PV) tolerance in lubricated wear environments. Like th.. |
|||
Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp IF006S PA 6/12 (Asia Pacific) LNP* Thermocomp* IF006S is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia Paci.. |
|||
Flexural Strength | 250 MPa | 36300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RX99732C PA 66 LNP* Thermocomp* PDX-R-99732 is a Nylon 6/6 with proprietary fillers. |
|||
Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
Unitika A1030GFL PA6, 30% Glass Fiber Reinforced, Dry Information provided by Unitika Ltd. |
|||
Flexural Strength | 250 - 300 MPa | 36300 - 43500 psi | At Rupture; ISO 178 |
Vyncolit Vyntec® CF8030 Carbon Fiber Reinforced Novolac Phenolic Carbon fiber reinforced phenolic moldable composite with superior tribological properties. High tensile and flexural strength and modulus combined with low density.Information provided by Vyncolit,.. |
|||
Flexural Strength | 250 MPa | 36300 psi | ASTM D790 |
Polyram PlusTek PB300G6 Nylon 6, 30% Glass Fiber 30% Glass-fiber reinforced, heat stabilized polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Strength | 250 MPa | 36300 psi | At Rupture; ISO 178 |
Vyncolit X6952 Novolac Phenolic Glass fiber reinforced phenolic molding compound with superior mechanical properties: very high tensile and flexural strength combined with high elongation at break.USES: Information provided by Vyn.. |
|||
Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
Unitika A1025GO PA6, Flame Retardant, Dry Information provided by Unitika Ltd. |
|||
Flexural Strength | >= 250 MPa | >= 36300 psi | Perpendicular to laminations; IEC 1212-2 5.1 |
Hippe UP GM 205 Woven Glass Mat Reinforced Polyester (unsaturated) Resin - Sheet Used in mechanical and electrical applications. Very high mechanical properties at ambient temperatures. Good mechanical properties at elevated temperatures. Flame retardant.Information provided .. |
|||
Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
Eurotec® Tecomid® NA40 GR30 NL RM PA 6.6 30% glass fiber reinforced, low friction and wear Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
Eurotec® Tecomid® NA40 GR25 NL PA 6.6 25% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
Ascend Performance Materials Vydyne® R525H BK0201 Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525H BK0201 is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie.. |
|||
Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
Ascend Performance Materials Vydyne® R525H BLK Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525H BLK is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties.. |
|||
Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
Ascend Performance Materials Vydyne® R525H Nylon 66, 25% Glass Filled, Dry as Molded Vydyne® R525H is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties whe.. |
|||
Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
Ascend Performance Materials Vydyne® R540H Nylon 66, 40% Glass Reinforced, Conditioned Vydyne® R540H is general-purpose, heat-stabilized, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic.. |
|||
Flexural Strength | 250 MPa | 36300 psi | at max force; ISO 178 |
BASF Ultramid® B3ZG8 BK 20560 40% Glass Filled PA6-1 (Dry) Description: Impact-modified and 40% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness and toughness, for instance, for vehicle airbag housings and suitcas.. |