Material Notes:
Carbon fiber reinforced phenolic moldable composite with superior tribological properties. High tensile and flexural strength and modulus combined with low density.Information provided by Vyncolit, a Sumitomo Bak Group
Physical Properties Metric English Comments
Bulk Density 0.600 - 0.700 g/cc
0.0217 - 0.0253 lb/in³
Powder Density; ISO 60
Density 1.35 g/cc
0.0488 lb/in³
Relative Density; ISO 1183
Water Absorption 0.050 - 0.10 %
0.050 - 0.10 %
Linear Mold Shrinkage 0.00 - 0.0020 cm/cm
0.00 - 0.0020 in/in
Injection Molding; ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break 100 - 130 MPa
14500 - 18900 psi
ISO 527
Elongation at Break 0.40 - 0.70 %
0.40 - 0.70 %
Tensile; ISO 527
1.2 - 1.5 %
1.2 - 1.5 %
Flexure; ISO 178
Tensile Modulus 20.0 - 23.0 GPa
2900 - 3340 ksi
ISO 527
Flexural Strength 250 - 300 MPa
36300 - 43500 psi
At Rupture; ISO 178
Flexural Modulus 17.0 - 24.0 GPa
2470 - 3480 ksi
ISO 178
Compressive Strength 270 - 330 MPa
39200 - 47900 psi
ISO 604
Charpy Impact Unnotched 1.10 - 1.70 J/cm²
5.24 - 8.09 ft-lb/in²
ISO 179
Charpy Impact, Notched 0.200 - 0.300 J/cm²
0.952 - 1.43 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 1.00 - 5.00 µm/m-°C

@Temperature 20.0 °C
0.556 - 2.78 µin/in-°F

@Temperature 68.0 °F
TMA
CTE, linear, Transverse to Flow 25.0 - 40.0 µm/m-°C

@Temperature 20.0 °C
13.9 - 22.2 µin/in-°F

@Temperature 68.0 °F
TMA
Deflection Temperature at 1.8 MPa (264 psi) 230 - 250 °C
446 - 482 °F
ISO 75 A
Shrinkage 0.00 - 0.10 %
0.00 - 0.10 %
Post Shrinkage; ISO 2577
Electrical Properties Metric English Comments
Volume Resistivity 3.817e+7 ohm-cm
3.817e+7 ohm-cm
ASTM D257
Surface Resistance 3.669e+6 ohm
3.669e+6 ohm
ASTM D257
Descriptive Properties Value Comments
Color Black
Main Filler Carbon Fiber
Molding Method Compression, transfer, injection