| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
|
Nilit FRIANYL B63 W-GV35 Nylon 6 for injection molding, 35% glass fiber reinforced
Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Flexural Strength |
250
MPa @Temperature 23.0 °C |
36300
psi @Temperature 73.4 °F |
ISO 178 |
|
Solvay Specialty Polymers Primef® 4010 Polyphenylene Sulfide (PPS), 40% Glass Fiber Reinforcement
(discontinu
Primef 4010 is a 40% glass fiber reinforced polyphenylene sulfide (PPS) that offers enhanced mechanical properties. In general, PPS offers an excellent balance of properties including high temperatu..
|
|||
| Flexural Strength | 250 MPa | 36300 psi | ASTM D790 |
|
Gharda Chemicals G-PAEK™ 1200FCM Ultra High Performance PEK Polymer
(discontinued **)
Milled carbon fiber reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection molding, easy flow, Black in colorApplication Areas: Suitable for high temperature applica..
|
|||
| Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
|
Nilit FRIANYL C73 GV40 Nylon 6.6/6 for injection molding, 40% glass fiber reinforced
Nylon 6.6/6 for injection molding, medium viscosity.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Flexural Strength | 250 MPa | 36300 psi | |
|
Lehmann & Voss LUVOCOM® 1105-8169 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista..
|
|||
| Flexural Strength | 250 MPa | 36300 psi | |
|
Lehmann & Voss LUVOCOM® 1-7805 Polyamide 66, with glass fiber, aramid reinforcement and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Heat stabilised.High dimension..
|
|||
| Flexural Strength | 250 MPa | 36300 psi | |
|
Lehmann & Voss LUVOCOM® 19-7900 Polyamide 46, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
|
|||
| Flexural Strength | >= 250 MPa | >= 36300 psi | |
|
Hybrid Plastics Fireban® Mark VI Resorcinolinic (PRF)
The resin system produces a superiour fire resistant material.Information provided by Hybrid Plastics
|
|||
| Flexural Strength | >= 250 MPa | >= 36300 psi | |
|
Hybrid Plastics Fireban® Mark VII-IS Resorcinolinic (PRF)
The resin system produces a superiour fire resistant material.Information provided by Hybrid Plastics
|
|||
| Flexural Strength | >= 250 MPa | >= 36300 psi | |
|
MarkeTech AN 120 Aluminum Nitride Ceramic Substrate, 98% Purity
Data provided by the supplier, MarkeTech International.Substrate Specs: Maximum dimensions 5.5 x 3.6 in. Thickness 0.12-0.60 in. Surface roughness 0.3 µm as fired; 0.075 µm lapped; 0.025 µ..
|
|||
| Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
|
Kuraray Genestarâ„¢ G1301A-M61 Nylon, 30% Glass Filled
30% Glass reinforced and impact modified injection grade.Main Features:Higher elongation and impact strengthHeat resistanceChemical resistanceExample of applications:Quick connector
|
|||
| Flexural Strength | 250 MPa | 36300 psi | ASTM D790 |
|
Solvay TECHNYL® A 218 V25 Black 21 N PA66, 25% glass fiber, DRY
Description: TECHNYL® A 218 V25 is a polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The ..
|
|||
| Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
|
Solvay TECHNYL® A 718 V30 PA66, 30% glass fiber, DRY
Description: TECHNYL A 718 V30 is a polyamide 66 reinforced with glass fiber and thermal stabilized for injection moldingColors: it is sailed on natural and black colorAvailable in: Latin AmericaMai..
|
|||
| Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
|
SABIC Innovative Plastics LNP THERMOCOMP EC004XXC PEI
LNP* THERMOCOMP* EC004XXC is a compound based on Polyetherimide resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive.
|
|||
| Flexural Strength | 250 MPa | 36300 psi | ASTM D790 |
|
Polyram PlusTek PB300G6 Nylon 6, 30% Glass Fiber
30% Glass-fiber reinforced, heat stabilized polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Flexural Strength | 250 MPa | 36300 psi | ASTM D790 |
|
Polyram PlusTek PB306G6 Nylon 6, 30% Glass Fiber
30% glass-fiber reinforced, heat stabilized polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Flexural Strength | 250 MPa | 36300 psi | ASTM C1161 |
|
M Cubed Technologies TSC-15 Titanium-alloyed Reaction Bonded Silicon Carbide
Specialty reaction-bonded SiC for applications requiring high stiffness, high toughness, and also high thermal conductivity--mechanical seals, for example Flow-through complex channels can be forme..
|
|||
| Flexural Strength | 250 MPa | 36300 psi | MOR; ASTM-F417 |
|
CoorsTek Boron Carbide Reaction-Bonded Boron Carbide
Lowest density for ultra-lightweight designs
|
|||
| Flexural Strength | 250 MPa | 36300 psi | DAM; ISO 178 |
|
DuPont Performance Polymers Zytel® HTN FR52G30BL NC010 Polyphthalamide (PPA)
(Unverified Data**)
30% Glass Reinforced Flame Retardant PPA High Performance Polyamide Zytel HTNFR52G30BL NC010 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin that has been devel..
|
|||
| Flexural Strength | >= 250 MPa | >= 36300 psi | Perpendicular to laminations; IEC 1212-2 5.1 |
|
Hippe UP GM 204 Woven Glass Mat Reinforced Polyester (unsaturated) Resin - Sheet
Used in mechanical and electrical applications. Very high mechanical properties at ambient temperatures. Good mechanical properties at elevated temperatures.Information provided by Hippe.
|
|||
| Flexural Strength | >= 250 MPa | >= 36300 psi | Perpendicular to laminations; IEC 1212-2 5.1 |
|
Hippe UP GM 205 Woven Glass Mat Reinforced Polyester (unsaturated) Resin - Sheet
Used in mechanical and electrical applications. Very high mechanical properties at ambient temperatures. Good mechanical properties at elevated temperatures. Flame retardant.Information provided ..
|
|||
| Flexural Strength | <= 250 MPa | <= 36300 psi | 3.5% flexure; ISO 178 |
|
Azoty Tarnow™ Tarnamid® T-27 GF40 I Polyamide 6 - Glass Fiber Reinforced
40% Glass fiber reinforced, impact modified, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following mai..
|
|||
| Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
|
Ascend Performance Materials Vydyne® R540H Nylon 66, 40% Glass Reinforced, Conditioned
Vydyne® R540H is general-purpose, heat-stabilized, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic..
|
|||
| Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
|
Ascend Performance Materials VYDYNE® R543 Nylon, 43% Glass Reinforced, Conditioned
Vydyne® R543 is general purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fee, flow and mold release. Glass..
|
|||
| Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
|
Ascend Performance Materials Vydyne® R543H BK02 Nylon 66, 43% Glass Reinforced, Conditioned
Vydyne® R543H BK02 is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. ..
|
|||